Patent classifications
H10P14/3216
Preparation method of aluminum nitride composite structure based on two-dimensional (2D) crystal transition layer
A preparation method of an aluminum nitride (AlN) composite structure based on a two-dimensional (2D) crystal transition layer is provided. The preparation method includes: transferring the 2D crystal transition layer on a first periodic groove of an epitaxial substrate; forming a second periodic groove staggered with the first periodic groove on the 2D crystal transition layer; depositing a supporting protective layer; depositing a functional layer of a required AlN-based material; and removing the 2D crystal transition layer through thermal oxidation to obtain a semi-suspended AlN composite structure. The preparation method has low difficulty and is suitable for large-scale industrial production. Design windows of the periodic grooves and the AlN functional layer are large and can meet the material requirements of deep ultraviolet light-emitting diodes (DUV-LEDs) and radio frequency (RF) electronic devices for different purposes, resulting in a wide application range.
Substrate processing for GaN growth
Exemplary semiconductor structures may include a silicon-containing substrate. The structures may include a layer of a metal nitride overlying the silicon-containing substrate. The structures may include a gallium nitride structure overlying the layer of the metal nitride. The structures may include an oxygen-containing layer disposed between the layer of the metal nitride and the gallium nitride structure.
Low-temperature deposition of high-quality aluminum nitride films for heat spreading applications
Provided are high quality metal-nitride, such as aluminum nitride (AlN), films for heat dissipation and heat spreading applications, methods of preparing the same, and deposition of high thermal conductivity heat spreading layers for use in RF devices such as power amplifiers, high electron mobility transistors, etc. Aspects of the inventive concept can be used to enable heterogeneously integrated compound semiconductor on silicon devices or can be used in in non-RF applications as the power densities of these highly scaled microelectronic devices continues to increase.
Manufacturing method of gallium nitride film
A method for manufacturing a gallium nitride film includes the steps of placing a substrate so as to face a target containing nitrogen and gallium in a vacuum chamber, supplying a sputtering gas into the vacuum chamber, supplying a nitrogen radical into the vacuum chamber, generating a plasma of the sputtering gas by application of a voltage to the target, generating a gallium ion by a collision of an ion of the sputtering gas with the target, and stopping the application of the voltage to the target and depositing gallium nitride on the substrate. The gallium nitride is generated by a reaction of the gallium ion with a nitrogen anion which is generated by a reaction of an electron in the vacuum chamber with the nitrogen radical.
MANUFACTURABLE GALLIUM AND NITROGEN CONTAINING SINGLE FREQUENCY LASER DIODE
A method for manufacturing an optical device includes providing a carrier waver, provide a first substrate having a first surface region, and forming a first gallium and nitrogen containing epitaxial material overlying the first surface region. The first epitaxial material includes a first release material overlying the first substrate. The method also includes patterning the first epitaxial material to form a plurality of first dice arranged in an array; forming a first interface region overlying the first epitaxial material; bonding the first interface region of at least a fraction of the plurality of first dice to the carrier wafer to form bonded structures; releasing the bonded structures to transfer a first plurality of dice to the carrier wafer, the first plurality of dice transferred to the carrier wafer forming mesa regions on the carrier wafer; and forming an optical waveguide in each of the mesa regions, the optical waveguide configured as a cavity to form a laser diode of the electromagnetic radiation.
Semiconductor device
According to one embodiment, a semiconductor device includes a first electrode, a second electrode, a third electrode, a first nitride region, a second nitride region, and a third nitride region. The first nitride region includes Al.sub.x1Ga.sub.1-x1N (0x1<1). The first nitride region includes a first partial region, a second partial region, a third partial region, a fourth partial region, and a fifth partial region. The second nitride region includes Al.sub.x2Ga.sub.1-x2N (x1<x21) or In.sub.yAl.sub.zGa.sub.(1-y-z)N (0<y1, 0z<1, y+z1). The second nitride region includes a sixth partial region. The third nitride region includes Al.sub.x3Ga.sub.1-x3N (x1<x3<x2). The third nitride region includes a seventh partial region.
Method to improve performances of tunnel junctions grown by metal organic chemical vapor deposition
A device including an activated p-type layer comprising a III-Nitride based Mg-doped layer grown by vapor phase deposition or a growth method different from MBE. The p-type layer is activated through a sidewall of the p-type layer after the removal of defects from the sidewall thereby increasing a hole concentration in the p-type layer. In one or more examples, the device includes an active region between a first n-type layer and the p-type layer; a second n-type layer on the p-type layer; and a tunnel junction between the second n-type layer and the p-type layer, and the activated p-type layer has a hole concentration characterized by a current density of at least 100 Amps per centimeter square flowing between the first n-type layer and the second n-type layer in response to a voltage of 4 volts or less applied across the first n-type layer and the second n-type layer.
VARIABLE COMPOSITION TERNARY COMPOUND SEMICONDUCTOR ALLOYS, STRUCTURES, AND DEVICES
In.sub.xAl.sub.yGa.sub.1-x-yN semiconductor structures having optoelectronic elements characterized by epitaxial layers having different in-plane a-lattice parameters and different InN mole fractions are disclosed. The active regions are configured to emit radiation in different wavelength ranges and are characterized by strain states within about 1% to 2% of compressive strain. The epitaxial layers are grown on patterned In.sub.xAl.sub.yGa.sub.1-x-yN seed regions on a single substrate, where the relaxed InGaN growth layers provide (0001) In.sub.xAl.sub.yGa.sub.1-x-yN growth surfaces characterized by different in-plane a-lattice parameters and different InN mole fractions. In.sub.xAl.sub.yGa.sub.1-x-yN semiconductor structures can be used in optoelectronic devices such as in light sources for illumination and in display applications.
Growth-anneal cycling of a semiconductor layer
A method of fabricating a semiconductor device includes providing a substrate, implementing a growth procedure to form a semiconductor layer supported by the substrate, performing an anneal of the semiconductor layer, the anneal being conducted at a higher temperature than the growth procedure, and repeating the growth procedure and the anneal. The anneal is conducted at or above a decomposition temperature for the semiconductor layer.
Method for manufacturing a semiconductor substrate and method for suppressing occurrence of cracks in a growth layer
An object of the present invention is to provide a novel technique capable of suppressing the occurrence of cracks in the growth layer. The present invention is a method for manufacturing a semiconductor substrate, which includes: an embrittlement processing step S10 of reducing strength of an underlying substrate 10; and a crystal growth step S20 of forming the growth layer 20 on the underlying substrate 10. In addition, the present invention is a method for suppressing the occurrence of cracks in the growth layer 20, and this method includes an embrittlement processing step S10 of reducing the strength of the underlying substrate 10 before forming the growth layer 20 on the underlying substrate 10.