Patent classifications
C04B40/0071
METHOD FOR MAKING CARBONATED PRECAST CONCRETE PRODUCTS WITH ENHANCED DURABILITY
A method for making a carbonated precast concrete product includes: obtaining a mixture including at least one binder material, an aggregate, and water; molding the mixture into a molded intermediate; demolding the molded intermediate to obtain a demolded intermediate, the demolded intermediate having a first water-to-binder ratio; conditioning the demolded intermediate to provide a conditioned article having a second water-to-binder ratio less than the first water-to-binder ratio of the demolded intermediate; moisturizing at least one surface of the conditioned article with an aqueous medium, thereby causing a weight gain of the conditioned article and providing a moisturized product, a first portion of the moisturized product having a third water-to-binder ratio greater than a fourth water-to-binder ratio of a remainder of the moisturized product; and curing the moisturized product with carbon dioxide to obtain the carbonated precast concrete product.
METHOD FOR MAKING CARBONATED PRECAST CONCRETE PRODUCTS WITH ENHANCED DURABILITY
A method for making a carbonated precast concrete product includes: obtaining a mixture including at least one binder material, an aggregate, and water; molding the mixture into a molded intermediate; demolding the molded intermediate to obtain a demolded intermediate, the demolded intermediate having a first water-to-binder ratio; conditioning the demolded intermediate to provide a conditioned article having a second water-to-binder ratio less than the first water-to-binder ratio of the demolded intermediate; moisturizing at least one surface of the conditioned article with an aqueous medium, thereby causing a weight gain of the conditioned article and providing a moisturized product, a first portion of the moisturized product having a third water-to-binder ratio greater than a fourth water-to-binder ratio of a remainder of the moisturized product; and curing the moisturized product with carbon dioxide to obtain the carbonated precast concrete product.
COMPOSITE MEMBER, AND HEAT GENERATION DEVICE, BUILDING MEMBER AND LIGHT EMITTING DEVICE, EACH OF WHICH USES SAME
A composite member includes a matrix part including an inorganic substance, and an organic infrared absorbing material present in a dispersed state inside the matrix part. The composite member has a porosity of 20% or less in a section of the matrix part. A heat generation device includes the composite member, and an infrared light source for irradiating the composite member with infrared rays. A building member and a light emitting device each include the composite member, or the heat generation device.
COMPOSITE MEMBER, AND HEAT GENERATION DEVICE, BUILDING MEMBER AND LIGHT EMITTING DEVICE, EACH OF WHICH USES SAME
A composite member includes a matrix part including an inorganic substance, and an organic infrared absorbing material present in a dispersed state inside the matrix part. The composite member has a porosity of 20% or less in a section of the matrix part. A heat generation device includes the composite member, and an infrared light source for irradiating the composite member with infrared rays. A building member and a light emitting device each include the composite member, or the heat generation device.
COMPOSITE MEMBER, AND CONSTRUCTION MEMBER AND DECORATION MEMBER USING SAME
A composite member includes a matrix part including an inorganic substance, and an organic dye present in a dispersed state inside the matrix part. The composite member has a porosity of 20% or less in a section of the matrix part. A construction member and a decoration member each include the composite member.
COMPOSITE MEMBER, AND CONSTRUCTION MEMBER AND DECORATION MEMBER USING SAME
A composite member includes a matrix part including an inorganic substance, and an organic dye present in a dispersed state inside the matrix part. The composite member has a porosity of 20% or less in a section of the matrix part. A construction member and a decoration member each include the composite member.
Composite blast furnace mineral powder and synthetic material made from same
A composite blast furnace mineral powder and a synthetic material made from same. The composite blast furnace mineral powder consists of the following materials in percentage by mass: 40-98.4% of blast furnace mineral powder, 7-20% of acrylic polymer emulsion or 1.5-3% of redispersible latex powder, 0.1-2% of fiber, 0-3% of pigment and the balance of filler. The composite blast furnace mineral powder can be pressed into a profile or a brick blank.
Composite blast furnace mineral powder and synthetic material made from same
A composite blast furnace mineral powder and a synthetic material made from same. The composite blast furnace mineral powder consists of the following materials in percentage by mass: 40-98.4% of blast furnace mineral powder, 7-20% of acrylic polymer emulsion or 1.5-3% of redispersible latex powder, 0.1-2% of fiber, 0-3% of pigment and the balance of filler. The composite blast furnace mineral powder can be pressed into a profile or a brick blank.
CONTROLLED AND EFFICIENT SYNTHESIS OF INORGANIC-ORGANIC COMPOSITE CEMENTATION AGENTS WITH ENHANCED STRAIN CAPACITY
Provided herein are manufacturing processes that include (1) subjecting precursor-containing solids to dissolution under acoustic perturbation to yield an initial slurry including dissolved precursors; (2) subjecting the initial slurry to hydrothermal synthesis to yield a subsequent slurry including siliceous solids formed from the dissolved precursors; and (3) subjecting the subsequent slurry to cementation to yield a cemented siliceous solid. Also provided herein are cemented siliceous solids formed by the manufacturing processes.
WATER-REPELLENT MEMBER, AND BUILDING MEMBER AND WET ROOM MEMBER USING SAME
A water-repellent member includes a matrix part including an inorganic substance including at least one of a metal oxide or a metal hydroxide, and a water-repellent resin present in a dispersed state inside the matrix part. The water-repellent member has a porosity of 20% or less in a section of the matrix part. A building member and a wet room member each include the water-repellent member.