C08K5/01
Damping thermoplastic elastomer blends exhibiting clarity
A thermoplastic elastomer compound includes polyester-type thermoplastic polyurethane and no greater than about 30 weight percent of styrene-isobutylene-styrene block copolymer. The compound has good clarity, as exhibited by a haze of no greater than about 60%, or 50%, or 30%, according to ASTM D 1003. Additionally, the compound has good damping properties, as exhibited by a resilience or vertical rebound of less than about 25% according to ASTM D2632.
Damping thermoplastic elastomer blends exhibiting clarity
A thermoplastic elastomer compound includes polyester-type thermoplastic polyurethane and no greater than about 30 weight percent of styrene-isobutylene-styrene block copolymer. The compound has good clarity, as exhibited by a haze of no greater than about 60%, or 50%, or 30%, according to ASTM D 1003. Additionally, the compound has good damping properties, as exhibited by a resilience or vertical rebound of less than about 25% according to ASTM D2632.
STYRENE RESIN, STYRENE RESIN COMPOSITION, MOLDED ARTICLE THEREOF, AND STYRENE RESIN PRODUCTION METHOD
A styrene resin having a syndiotactic structure, with an endothermic amount in a range of 175 to 260° C. of less than 30% based on the total endothermic amount, and a styrene resin composition containing 50 to 95% by mass of a thermoplastic resin composition and 5 to 50% by mass of a glass filler, the thermoplastic resin composition containing 100 parts by mass containing 80 to 100% by mass of a styrene resin having a syndiotactic structure and 0 to 20% by mass of a rubbery elastic material, 0.2 to 2.0 parts by mass of at least one kind of an antioxidant selected from a phenol-based antioxidant and a sulfur antioxidant, 1.5 to 5.0 parts by mass of at least one kind of a compound selected from a polyphenylene ether or a modified polyphenylene ether, and at least one kind selected from a nucleating agent or a release agent.
STYRENE RESIN, STYRENE RESIN COMPOSITION, MOLDED ARTICLE THEREOF, AND STYRENE RESIN PRODUCTION METHOD
A styrene resin having a syndiotactic structure, with an endothermic amount in a range of 175 to 260° C. of less than 30% based on the total endothermic amount, and a styrene resin composition containing 50 to 95% by mass of a thermoplastic resin composition and 5 to 50% by mass of a glass filler, the thermoplastic resin composition containing 100 parts by mass containing 80 to 100% by mass of a styrene resin having a syndiotactic structure and 0 to 20% by mass of a rubbery elastic material, 0.2 to 2.0 parts by mass of at least one kind of an antioxidant selected from a phenol-based antioxidant and a sulfur antioxidant, 1.5 to 5.0 parts by mass of at least one kind of a compound selected from a polyphenylene ether or a modified polyphenylene ether, and at least one kind selected from a nucleating agent or a release agent.
CHLOROPRENE-BASED BLOCK COPOLYMER, LATEX, LATEX COMPOSITION, AND RUBBER COMPOSITION
A chloroprene-based block copolymer, a latex, a latex composition, and a rubber composition that can produce a product with excellent flexibility and tensile properties without the use of a vulcanizing agent or a vulcanizing accelerator. A chloroprene-based block copolymer, includes 5 to 30% by mass of a polymer block (A) and 70 to 95% by mass of a chloroprene-based polymer block (B), wherein: the polymer block (A) is derived from a monomer; when the monomer is polymerized alone, a polymer with a glass transition temperature of 80° C. or higher can be obtained; the chloroprene-based polymer block (B) includes a chloroprene monomer; and the chloroprene-based block copolymer has a toluene insoluble content of 20 to 100% by mass with respect to 100% by mass of the chloroprene-based block copolymer.
CHLOROPRENE-BASED BLOCK COPOLYMER, LATEX, LATEX COMPOSITION, AND RUBBER COMPOSITION
A chloroprene-based block copolymer, a latex, a latex composition, and a rubber composition that can produce a product with excellent flexibility and tensile properties without the use of a vulcanizing agent or a vulcanizing accelerator. A chloroprene-based block copolymer, includes 5 to 30% by mass of a polymer block (A) and 70 to 95% by mass of a chloroprene-based polymer block (B), wherein: the polymer block (A) is derived from a monomer; when the monomer is polymerized alone, a polymer with a glass transition temperature of 80° C. or higher can be obtained; the chloroprene-based polymer block (B) includes a chloroprene monomer; and the chloroprene-based block copolymer has a toluene insoluble content of 20 to 100% by mass with respect to 100% by mass of the chloroprene-based block copolymer.
CURABLE CASTING COMPOUND FOR THE MANUFACTURE OF MOLDED PLASTICS
This invention relates to a curable casting compound for the manufacture of molded plastics, comprising a casting compound having a binder composition and a filler composition, wherein the filler composition has at least a first portion of an inorganic filler and a second portion of an organic filler, wherein the second portion of organic filler comprises comminuted nutshells—as a nutshell portion, in particular granular nutshells, having a percentage by weight of 1% by wt. to 100% by wt. of the filler composition.
CURABLE CASTING COMPOUND FOR THE MANUFACTURE OF MOLDED PLASTICS
This invention relates to a curable casting compound for the manufacture of molded plastics, comprising a casting compound having a binder composition and a filler composition, wherein the filler composition has at least a first portion of an inorganic filler and a second portion of an organic filler, wherein the second portion of organic filler comprises comminuted nutshells—as a nutshell portion, in particular granular nutshells, having a percentage by weight of 1% by wt. to 100% by wt. of the filler composition.
HEAT AGING-RESISTANT AND FLEXIBLE POLYOLEFIN FORMULATION
A polyolefin formulation comprising constituents (A) to (E) in the following amounts: from 15.0 to 55.0 weight percent (wt %) of (A) a polypropylene homopolymer; from 77.9 to 30.0 wt % of (B) a poly(ethylene-co-1-alkene) copolymer; from 3.0 to 6.5 wt % of (C) an ethylene/propylene diblock copolymer; from 4.0 to 8.0 wt % of (D) a saturated-and-aromatic (C.sub.14-C.sub.60)hydrocarbon; and from 0.1 to 1.5 wt % of (E) an antioxidant; wherein the wt % of (B) divided by the wt % (A) is a mass ratio of from 5.0:1.0 to 0.50:1.0; and wherein the amounts of constituents (A), (B), and (C) total from 88.0 to 95.9 wt % of the polyolefin formulation; and wherein the amounts of constituents (A) to (E) total from 92.1 to 100.0 wt % of the polyolefin formulation.
HEAT AGING-RESISTANT AND FLEXIBLE POLYOLEFIN FORMULATION
A polyolefin formulation comprising constituents (A) to (E) in the following amounts: from 15.0 to 55.0 weight percent (wt %) of (A) a polypropylene homopolymer; from 77.9 to 30.0 wt % of (B) a poly(ethylene-co-1-alkene) copolymer; from 3.0 to 6.5 wt % of (C) an ethylene/propylene diblock copolymer; from 4.0 to 8.0 wt % of (D) a saturated-and-aromatic (C.sub.14-C.sub.60)hydrocarbon; and from 0.1 to 1.5 wt % of (E) an antioxidant; wherein the wt % of (B) divided by the wt % (A) is a mass ratio of from 5.0:1.0 to 0.50:1.0; and wherein the amounts of constituents (A), (B), and (C) total from 88.0 to 95.9 wt % of the polyolefin formulation; and wherein the amounts of constituents (A) to (E) total from 92.1 to 100.0 wt % of the polyolefin formulation.