ENVIRONMENT-FRIENDLY HOT-MELT COMPOSITION FOR VEHICLE INTERIOR MATERIAL
Disclosed is an environment-friendly hot-melt composition for a vehicle interior material, the hot-melt composition including: 65 wt % to 85 wt % of an aromatic polyamide; 10 wt % to 30 wt % of an aliphatic polyamide; 1 wt % to 5 wt % of an olefinic elastomer graft-polymerized with maleic anhydride; and 0.1 wt % to 2 wt % of an antioxidant.
ENVIRONMENT-FRIENDLY HOT-MELT COMPOSITION FOR VEHICLE INTERIOR MATERIAL
Disclosed is an environment-friendly hot-melt composition for a vehicle interior material, the hot-melt composition including: 65 wt % to 85 wt % of an aromatic polyamide; 10 wt % to 30 wt % of an aliphatic polyamide; 1 wt % to 5 wt % of an olefinic elastomer graft-polymerized with maleic anhydride; and 0.1 wt % to 2 wt % of an antioxidant.
ENVIRONMENT-FRIENDLY HOT-MELT COMPOSITION FOR VEHICLE INTERIOR MATERIAL
Disclosed is an environment-friendly hot-melt composition for a vehicle interior material, the hot-melt composition including: 65 wt % to 85 wt % of an aromatic polyamide; 10 wt % to 30 wt % of an aliphatic polyamide; 1 wt % to 5 wt % of an olefinic elastomer graft-polymerized with maleic anhydride; and 0.1 wt % to 2 wt % of an antioxidant.
Environment-friendly hot-melt composition for vehicle interior material
Disclosed is an environment-friendly hot-melt composition for a vehicle interior material, the hot-melt composition including: 65 wt % to 85 wt % of an aromatic polyamide; 10 wt % to 30 wt % of an aliphatic polyamide; 1 wt % to 5 wt % of an olefinic elastomer graft-polymerized with maleic anhydride; and 0.1 wt % to 2 wt % of an antioxidant.
Environment-friendly hot-melt composition for vehicle interior material
Disclosed is an environment-friendly hot-melt composition for a vehicle interior material, the hot-melt composition including: 65 wt % to 85 wt % of an aromatic polyamide; 10 wt % to 30 wt % of an aliphatic polyamide; 1 wt % to 5 wt % of an olefinic elastomer graft-polymerized with maleic anhydride; and 0.1 wt % to 2 wt % of an antioxidant.
Soft hand copolyamide composition
Composition comprising, on a weight basis, the total being equal to 100%: from 98% to 100% of at least one copolyamide bearing amide units and polyether units, having a melting point (T.sub.m) from about 90 to about 150 C., in particular from about 100 C. to about 125 C., and having a flexural modulus of less than 100 MPa, as determined according to standard ISO 178 (2010); from 0 to 2% of at least one additive chosen from stabilizers and dyes, or a mixture thereof,
for the manufacture of a heat-sensitive adhesive, in particular a veil, a film, granules, a filament, a grate, a powder or a suspension.
ENVIRONMENT-FRIENDLY HOT-MELT COMPOSITION FOR VEHICLE INTERIOR MATERIAL
Disclosed is an environment-friendly hot-melt composition for a vehicle interior material, the hot-melt composition including: 65 wt % to 85 wt % of an aromatic polyamide; 10 wt % to 30 wt % of an aliphatic polyamide; 1 wt % to 5 wt % of an olefinic elastomer graft-polymerized with maleic anhydride; and 0.1 wt % to 2 wt % of an antioxidant.
ENVIRONMENT-FRIENDLY HOT-MELT COMPOSITION FOR VEHICLE INTERIOR MATERIAL
Disclosed is an environment-friendly hot-melt composition for a vehicle interior material, the hot-melt composition including: 65 wt % to 85 wt % of an aromatic polyamide; 10 wt % to 30 wt % of an aliphatic polyamide; 1 wt % to 5 wt % of an olefinic elastomer graft-polymerized with maleic anhydride; and 0.1 wt % to 2 wt % of an antioxidant.
ENVIRONMENT-FRIENDLY HOT-MELT COMPOSITION FOR VEHICLE INTERIOR MATERIAL
Disclosed is an environment-friendly hot-melt composition for a vehicle interior material, the hot-melt composition including: 65 wt % to 85 wt % of an aromatic polyamide; 10 wt % to 30 wt % of an aliphatic polyamide; 1 wt % to 5 wt % of an olefinic elastomer graft-polymerized with maleic anhydride; and 0.1 wt % to 2 wt % of an antioxidant.
HOT-MELT ADHESIVE COMPOSITION
The invention relates to a hot-melt adhesive composition comprising: i) at least one specific semicrystalline aliphatic copolyamide containing a unit Y exhibiting a Tg of less than 30 C., ii) from 3% to 35% by weight, with respect to the total weight of the composition, of at least one thermally conductive filler, the content of carbon atoms of which is of between 80% and 100%, with respect to the number of atoms constituting the filler, the composition comprising less than 20% of its components having a density of greater than 3. The invention also relates to its process of preparation and to its use.