C10B53/08
METHOD FOR PRODUCING FERROCOKE
A method for producing ferrocoke in which it is possible to use a cheap and poor-quality coal having a high ash content while suppressing the decrease of the strength in ferrocoke or formed coke and a special coal mixing is not performed with respect to the fusion frequently causing problems in the carbonization with the shaft furnace. In a method for producing ferrocoke by molding and carbonizing a mixture of coal and iron ore, the coal is a single coal or a mixture of plural coals and a non-caking or slight caking coal having a load average value of ash content of not less than 10.7% and a load average value of mean maximum reflectance of not less than 0.81% is used.
METHOD FOR PRODUCING FERROCOKE
A method for producing ferrocoke in which it is possible to use a cheap and poor-quality coal having a high ash content while suppressing the decrease of the strength in ferrocoke or formed coke and a special coal mixing is not performed with respect to the fusion frequently causing problems in the carbonization with the shaft furnace. In a method for producing ferrocoke by molding and carbonizing a mixture of coal and iron ore, the coal is a single coal or a mixture of plural coals and a non-caking or slight caking coal having a load average value of ash content of not less than 10.7% and a load average value of mean maximum reflectance of not less than 0.81% is used.
METHOD FOR PRODUCING MOLDED PRODUCT FOR FERROCOKE
A method for producing a molded product for ferrocoke, wherein a high-strength molded product for ferrocoke can be produced advantageously without making particular investment in facilities and inviting the operating troubles. In a method for producing a molded product for ferrocoke by molding a mixed starting material of coal, an iron-source material, a high-softening point binder having a softening point of not lower than 150 C., and a low-softening point binder having a softening point of lower than 150 C., at least one of the iron-source material and the high-softening point binder is previously heated to not less than a temperature lower by 20 C. than a softening point of the high-softening point binder to perform molding of the mixture.
METHOD FOR PRODUCING MOLDED PRODUCT FOR FERROCOKE
A method for producing a molded product for ferrocoke, wherein a high-strength molded product for ferrocoke can be produced advantageously without making particular investment in facilities and inviting the operating troubles. In a method for producing a molded product for ferrocoke by molding a mixed starting material of coal, an iron-source material, a high-softening point binder having a softening point of not lower than 150 C., and a low-softening point binder having a softening point of lower than 150 C., at least one of the iron-source material and the high-softening point binder is previously heated to not less than a temperature lower by 20 C. than a softening point of the high-softening point binder to perform molding of the mixture.
BIOMASS TREATMENT PROCESS AND APPARATUS
A process and apparatus are provided in the present invention for treatment of particulate biomass. The present process comprises a densification stage, a first treatment stage, a second treatment stage, a cooling stage; the present apparatus comprises a thermo-chemical treatment chamber which is a two-stage compact moving bed type including two compartments for pre-torrefaction and torrefaction and having a star or spider or ring formic hot gas distribution system equipped with at least one hot gas input and at least one hot gas output for each compartment, and at least one particulate biomass inlet and at least one particulate biomass outlet.
BIOMASS TREATMENT PROCESS AND APPARATUS
A process and apparatus are provided in the present invention for treatment of particulate biomass. The present process comprises a densification stage, a first treatment stage, a second treatment stage, a cooling stage; the present apparatus comprises a thermo-chemical treatment chamber which is a two-stage compact moving bed type including two compartments for pre-torrefaction and torrefaction and having a star or spider or ring formic hot gas distribution system equipped with at least one hot gas input and at least one hot gas output for each compartment, and at least one particulate biomass inlet and at least one particulate biomass outlet.
FERROCOKE MANUFACTURING METHOD
In a ferrocoke manufacturing method by shaping and carbonizing a mixture of coal and iron ore, a hardly softening coal having a button index (CSN) of not more than 2.0 is used as the coal. The coal can be a blend of hardly softening coal and easily softening coal, and the hardly softening coal can be a coal having a button index (CSN) of 1.0 and a volatile matter of not less than 17%, and the easily softening coal can be a coal satisfying that a value obtained by multiplying CSN of easily softening coal by a blending ratio of easily softening coal in all coals is a range of 0.3-5.2. The coal can also be a blend of hardly softening coal and easily softening coal, and the hardly softening coal can be a coal having a button index (CSN) of 1.5-2.0, and the easily softening coal can be a coal satisfying that a value obtained by multiplying CSN of easily softening coal by a blending ratio of easily softening coal in all coals is nit more than 5.0.
FERROCOKE MANUFACTURING METHOD
In a ferrocoke manufacturing method by shaping and carbonizing a mixture of coal and iron ore, a hardly softening coal having a button index (CSN) of not more than 2.0 is used as the coal. The coal can be a blend of hardly softening coal and easily softening coal, and the hardly softening coal can be a coal having a button index (CSN) of 1.0 and a volatile matter of not less than 17%, and the easily softening coal can be a coal satisfying that a value obtained by multiplying CSN of easily softening coal by a blending ratio of easily softening coal in all coals is a range of 0.3-5.2. The coal can also be a blend of hardly softening coal and easily softening coal, and the hardly softening coal can be a coal having a button index (CSN) of 1.5-2.0, and the easily softening coal can be a coal satisfying that a value obtained by multiplying CSN of easily softening coal by a blending ratio of easily softening coal in all coals is nit more than 5.0.
Magnetic Metal Oxide Biochar Composite Particles, and Their Use in Recovering Pollutants From Aqueous Solution
Composite particles are disclosed comprising magnesium oxide, iron oxide, and biochar; and methods of making and using the composite particles. The composite particles may be used to recover solutes including phosphate, nitrate, ammonium, and organic compounds from aqueous solution, and the resulting solute-loaded particles may be used as a fertilizer to enhance plant growth. The composites be used to remove pollutants from agricultural runoff, wastewater, and surface water. The particles possess magnetic properties that enhance their recovery following solute adsorption.
TORREFIED BIOMASS BRIQUETTES AND RELATED METHODS
The presently disclosed subject matter relates to torrefied biomass briquettes and methods for producing the same that make use of a mixture of lightly torrefied material (LTM) and highly torrefied material (HTM) and/or make use of torrefied materials that are subjected to a hydrolysis pretreatment prior to being torrefied.