Patent classifications
C21C7/0025
Clean and rapid smelting method in an electric arc furnace with full scrap steel
A clean and rapid smelting method in an electric arc furnace with full scrap steel, is suitable for smelting process of 30-300 t electric arc furnace with full scrap steel. In the smelting process of the electric arc furnace with full scrap steel, different kinds of mediums are injected by an injection lance which is installed inside refractory material of sidewall at the bottom of the electric arc furnace in different stages of smelting. Carburization is utilized in molten pool to accelerate melting down and improve carbon content of the molten pool at the stage of recarburizing and fluxing. A reaction in the molten pool is intensified at the stage of high efficiency dephosphorization and deep denitrogenation, to enhance efficient dephosphorization and deep denitrification of the reaction in the molten pool, thereby accelerating the smelting speed of the electric arc furnace with full scrap steel, improving effect of dephosphorization and denitrification.
Production method for smelting clean steel from full-scrap steel using duplex electric arc furnaces
A production method for smelting clean steel from full-scrap steel using duplex electric arc furnaces. Electric arc furnaces located in two positions are connected in series, wherein the electric arc furnace in a first position is dephosphorization electric arc furnace, and the electric arc furnace in a second position is a decarbonization electric arc furnace. The production method includes: performing smelting by combining a decarbonization electric arc furnace and 1-3 dephosphorization electric arc furnaces; a specific process of performing the smelting includes: in a charging period of the 1-3 dephosphorization electric arc furnaces, adding the full-scrap steel for the smelting, lime, slag in the decarbonization electric arc furnace, auxiliary materials and carbon powder or a carbon block into the dephosphorization electric arc furnace.
PRODUCTS COMPRISING CHAR AND CARBON, AND ASSOCIATED SYSTEMS, DEVICES, AND METHODS
Mixture products containing charred products and coal or coke, and associated systems, devices and methods are disclosed herein. The charred product components of the mixture products can be made by receiving an input material in an oven, and heating the oven containing the input material to a predetermined temperature of at least 900? F. for a predetermined time of no more than 48 hours to produce a charred product. Advantageously, embodiments of the present technology can enable a more efficient mixture product production process. The resulting mixture products can also have higher quality in terms of desired Coke Strength After Reaction (CSR), Coke Reactivity Index (CRI), volatile matter content, ash content, sulfur content, grain size, etc.
Methods for utilizing olefin coke in a steel making process and products made therefrom
Methods and compositions for producing reduced carbon footprint steel compositions by providing a molten steel having a carbon content; and introducing a carbon containing agent into the molten steel. At least a portion of the carbon containing agent is a reclaimed olefin coke.
Pyrometallurgical Method for Recycling Shredded Material of Waste from the Production of New and Defective or End-of-Life Batteries for Electric Vehicles or Portable Li-Ion Batteries
A pyrometallurgical process for recycling shredded spent electric vehicle batteries of Li-ion type and/or waste from the production of these new batteries and battery rejects, and/or portable batteries of Li-ion type. The process entails the addition of iron, smelting via the supply of energy, separation of a slag, oxidizing treatment and separation of a second slag.
SYSTEMS AND METHODS FOR SELF-REDUCTION OF IRON ORE
Disclosed herein, in some aspects, are systems and methods for producing a material comprising iron through self-reduction of iron ore using bio-oil and/or other reducing agents (e.g., bio-based reducing agents), such as biocrude, ethanol, or other bio-based liquids or biologically sourced liquids. The bio-oil and/or other reducing agents can be mixed with the iron ore to form a furnace mixture, which can be heated, such that the components of the bio-oil and/or other reducing agents in the furnace mixture reduce the iron ore to form an iron product (e.g., a material that includes metallic iron). In some cases, the pre-formed furnace mixture allows for the reducing agents to interact with the iron more readily, thereby providing for quicker reaction rates, and thereby quicker reduction of iron ore, as compared to direct reduction iron production.
CLEAN AND RAPID SMELTING METHOD IN AN ELECTRIC ARC FURNACE WITH FULL SCRAP STEEL
A clean and rapid smelting method in an electric arc furnace with full scrap steel, is suitable for smelting process of 30300 t electric arc furnace with full scrap steel. In the smelting process of the electric arc furnace with full scrap steel, different kinds of medium is injected by an injection lance which is installed inside refractory material of sidewall at the bottom of the electric arc furnace in different stages of smelting; carburization is utilized in molten pool to accelerate melting down and improve carbon content of the molten pool at the stage of recarburizing and fluxing; reaction in the molten pool is intensified at the stage of high efficiency dephosphorization and deep denitrogenation, to enhance efficient dephosphorization and deep denitrification of the reaction in the molten pool, thereby accelerating the smelting speed of the electric arc furnace with full scrap steel, improving effect of dephosphorization and denitrification.
METHOD FOR PRODUCTION OF IRON-SILICON-ALUMINUM ALLOYS AND THEIR USE
Method of producing FeSiAI alloys wherein a carbonaceous rock with an ash content >50% to <65%, is being mixed with quartzite, iron-bearing material, and wood chips, if required, high volatile coal, in a preset ratio of the charge components and the homogenized charge material is being loaded into a melting furnace for melting of FeSiAI alloy, the charged carbonaceous rock can contain i.a. the following chemical composition in the mineral part (ash): Fe.sub.2O.sub.3 1.5-4.5% SiO.sub.2 55-65% Al.sub.2O.sub.3 25-35%, especially 32-34% CaO 0.3-3% MgO 0.3-2% TiO.sub.2 up to 1.5 S>0-0.4%, especially 0.01-0.06% P 0.01-0.05%
METHOD AND SYSTEM FOR PRODUCING HIGH-CARBON DRI USING SYNGAS
Producing direct reduced iron (DRI) having chemically-combined carbon includes providing DRI at a temperature above 400 C., providing a first gas stream including hydrogen and carbon monoxide, passing the first gas stream through a methane forming process to yield a second gas stream containing a higher concentration of methane than the first gas stream; and contacting the second gas stream with the DRI. A system for producing the DRI includes a vessel for containing DRI at a temperature above 400 C., a methane forming reactor containing a catalyst bed for producing methane from a first gas stream containing hydrogen and carbon monoxide, a first conduit to feed a gas stream including hydrogen and carbon monoxide to the methane forming reactor, and a second conduit to feed the second gas stream to the vessel containing the DRI.
PRODUCTION METHOD FOR SMELTING CLEAN STEEL FROM FULL-SCRAP STEEL USING DUPLEX ELECTRIC ARC FURNACES
A production method for smelting clean steel from full-scrap steel using duplex electric arc furnaces, which belongs to the field of electric arc furnace steelmaking. This method makes electric arc furnaces located in two positions be connected in series, wherein the electric arc furnace in a first position is dephosphorization electric arc furnace, and the electric arc furnace in a second position is decarbonization electric arc furnace.