Patent classifications
C30B1/10
Process for forming graphene layers on silicon carbide
A process for forming graphene, includes: depositing at least a first and a second metal onto a surface of silicon carbide (SiC), and heating the SiC and the first and second metals under conditions that cause the first metal to react with silicon of the silicon carbide to form carbon and at least one stable silicide. The corresponding solubilities of the carbon in the stable silicide and in the second metal are sufficiently low that the carbon produced by the silicide reaction forms a graphene layer on the SiC.
METHOD FOR PREPARING GRAPHITE-TITANIUM OXIDE COMPOSITE
According to an embodiment of the present invention, a method for preparing a graphite-titanium oxide composite comprises (S1) a surface-modifying graphite with benzyl alcohol or a cellulose-based material using a sol-gel method, (S2) distributing the surface-modified graphite in a solvent, adding a titanium precursor to the solvent, and mixing the titanium precursor with the surface-modified graphite to obtain a graphite-titanium mixture, and (S3) thermally treating the graphite-titanium mixture to grow a titanium oxide on a surface of the graphite.
METHOD FOR PREPARING GRAPHITE-TITANIUM OXIDE COMPOSITE
According to an embodiment of the present invention, a method for preparing a graphite-titanium oxide composite comprises (S1) a surface-modifying graphite with benzyl alcohol or a cellulose-based material using a sol-gel method, (S2) distributing the surface-modified graphite in a solvent, adding a titanium precursor to the solvent, and mixing the titanium precursor with the surface-modified graphite to obtain a graphite-titanium mixture, and (S3) thermally treating the graphite-titanium mixture to grow a titanium oxide on a surface of the graphite.
NONLINEAR OPTICAL CRYSTAL MATERIAL, METHOD FOR PREPARATION THEREOF, AND APPLICATION THEREOF
The present application discloses a nonlinear optical crystal material, preparation method and application of the nonlinear optical crystal material. The nonlinear optical crystal material has an excellent infrared nonlinear optical performance, whose frequency-doubling intensity can reach 9.3 times of AgGaS.sub.2 with the same particle size, and it meets type-I phase matching; and its laser damage threshold can reach 7.5 times of AgGaS.sub.2 with the same particle size. The nonlinear optical crystal material has important application value in the frequency-converters which can be used for frequency doubling, sum frequency, difference frequency, optical parametric oscillation of laser in mid and far infrared waveband, and the like.
NONLINEAR OPTICAL CRYSTAL MATERIAL, METHOD FOR PREPARATION THEREOF, AND APPLICATION THEREOF
The present application discloses a nonlinear optical crystal material, preparation method and application of the nonlinear optical crystal material. The nonlinear optical crystal material has an excellent infrared nonlinear optical performance, whose frequency-doubling intensity can reach 9.3 times of AgGaS.sub.2 with the same particle size, and it meets type-I phase matching; and its laser damage threshold can reach 7.5 times of AgGaS.sub.2 with the same particle size. The nonlinear optical crystal material has important application value in the frequency-converters which can be used for frequency doubling, sum frequency, difference frequency, optical parametric oscillation of laser in mid and far infrared waveband, and the like.
Methods for low energy inorganic material synthesis
The present invention relates to solvothermal vapor synthesis methods for the crystallization of a phase from a mixture of selected inorganic or organic precursors in an unsaturated vapor-phase reaction medium.
Methods for low energy inorganic material synthesis
The present invention relates to solvothermal vapor synthesis methods for the crystallization of a phase from a mixture of selected inorganic or organic precursors in an unsaturated vapor-phase reaction medium.
LOW TEMPERATURE SYNTHESIS, GROWTH AND DOPING METHODS AND RESULTING MATERIALS
Low temperature synthesis, growth and doping methods and resulting materials are disclosed. According to an aspect, a method for material transformation includes providing a target material comprising carbon and/or hydrocarbon. The method also includes placing the target material within a fluid comprising a hydrogen source. Further, the method includes applying energy to the target material such that at least some of the target material is transformed to the same material with new beneficial bonding configuration.
LOW TEMPERATURE SYNTHESIS, GROWTH AND DOPING METHODS AND RESULTING MATERIALS
Low temperature synthesis, growth and doping methods and resulting materials are disclosed. According to an aspect, a method for material transformation includes providing a target material comprising carbon and/or hydrocarbon. The method also includes placing the target material within a fluid comprising a hydrogen source. Further, the method includes applying energy to the target material such that at least some of the target material is transformed to the same material with new beneficial bonding configuration.
Nickel cobalt complex hydroxide particles and method for producing the same, positive electrode active material for non-aqueous electrolyte secondary battery and method for producing the same, and non-aqueous electrolyte secondary battery
A method for producing a nickel cobalt complex hydroxide includes first crystallization of supplying a solution containing Ni, Co and Mn, a complex ion forming agent and a basic solution separately and simultaneously to one reaction vessel to obtain nickel cobalt complex hydroxide particles, and a second crystallization of, after the first crystallization, further supplying a solution containing nickel, cobalt, and manganese, a solution of a complex ion forming agent, a basic solution, and a solution containing said element M separately and simultaneously to the reaction vessel to crystallize a complex hydroxide particles containing nickel, cobalt, manganese and said element M on the nickel cobalt complex hydroxide particles crystallizing a complex hydroxide particles comprising Ni, Co, Mn and the element M on the nickel cobalt complex hydroxide particles.