C03C2218/17

METHOD AND DEVICE FOR PROVIDING FLAT GLASS ELEMENTS WITH AN ANTI-CORROSION AGENT AND SEPARATION AGENT APPLICATION
20210246068 · 2021-08-12 ·

When on flat glass elements an anti-corrosion agent and a separation agent, containing a powdery anti-corrosion agent and a powdery separation agent, is applied with the anti-corrosion agent and the separation agent being jointly applied on at least one side of the flat glass elements, the partial quantities of the powdery separation agent and the powdery anti-corrosion agent can be dosed according to requirement without causing an excess of separation agent or a shortage of anti-corrosion agent by holding ready and dosing the said anti-corrosion agent and separation agent independently from each other and by blending them together only after dosing.

ENAMEL COMPOSITION, METHOD FOR PREPARING ENAMEL COMPOSITION, AND COOKING APPLIANCE
20230399254 · 2023-12-14 ·

An enamel composition, a method for preparing an enamel composition, and a cooking appliance are provided. The enamel composition may include 15 to 50 wt % of phosphorus pentoxide (P.sub.2O.sub.5); 5 to 20 wt % of one or more of lithium oxide (Li.sub.2O), sodium oxide (Na.sub.2O), or potassium oxide (K.sub.2O); 1 to 5 wt % of one or more of sodium fluoride (NaF), calcium fluoride (CaF.sub.2), or aluminum fluoride (AlF.sub.3); 1 to 35 wt % of one or more of magnesium oxide (MgO), barium oxide (BaO), or calcium oxide (CaO); and 5 to 30 wt % of one or more of manganese dioxide (MnO.sub.2), molybdenum trioxide (MoO.sub.3), bismuth oxide (Bi.sub.2O.sub.3), or nickel oxide (NiO). The enamel composition may be cleaned without being putting it into water.

METHOD FOR TREATING A GLASS-WALLED CONTAINER AND CORRESPONDING APPARATUS
20210114921 · 2021-04-22 ·

The invention relates to a method, and to an associated apparatus, for treating a container (1) comprising a glass wall (2) defining a receiving cavity (3) for receiving a product, said glass wall (2) having an inner face (4) and an opposite outer face (5), said glass wall (2) being provided with a first coating that includes a solid residual compound resulting from a step of dealkalization of the glass in the vicinity of the surface of said inner face (4) of said glass wall (2) to which said container (1) had previously been subjected, said method comprising a step of spraying the surface of said glass wall (2) with droplets of a liquid, in order to form on said glass wall (2), starting from said first coating, a second coating which includes said residual compound and which is more transparent and/or more uniform than said first coating. -Treatment of glass-walled containers.

ENAMEL COMPOSITION, METHOD FOR PREPARING ENAMEL COMPOSITION, AND COOKING APPLIANCE
20230406756 · 2023-12-21 ·

An enamel composition, a method for preparing an enamel composition, and a cooking appliance are provided. The enamel composition may include 15 to 50 wt % of phosphorus pentoxide (P.sub.2O.sub.5); 5 to 20 wt % of one or more of lithium oxide (Li.sub.2O), sodium oxide (Na.sub.2O), or potassium oxide (K.sub.2O); 1 to 5 wt % of one or more of sodium fluoride (NaF), calcium fluoride (CaF.sub.2), or aluminum fluoride (AlF.sub.3); 1 to 35 wt % of one or more of magnesium oxide (MgO), barium oxide (BaO), or calcium oxide (CaO); and 5 to 30 wt % of one or more of manganese dioxide (MnO.sub.2), molybdenum trioxide (MoO.sub.3), bismuth oxide (Bi.sub.2O.sub.3), or nickel oxide (NiO). The enamel composition may be cleaned without being putting it into water.

ENAMEL COMPOSITION, METHOD FOR PREPARING ENAMEL COMPOSITION, AND COOKING APPLIANCE
20240002279 · 2024-01-04 ·

An enamel composition, a method for preparing an enamel composition, and a cooking appliance are provided. The enamel composition may include phosphorus pentoxide (P.sub.2O.sub.5) at 15 to 50 wt %; silicon dioxide (SiO.sub.2) at 10 to 20 wt %; boron oxide (B.sub.2O.sub.3) at 1 to 15 wt %; one or more of lithium oxide (Li.sub.2O), sodium oxide (Na.sub.2O), or potassium oxide (K.sub.2O) at 5 to 20 wt %; one or more of sodium fluoride (NaF), calcium fluoride (CaF.sub.2), or aluminum fluoride (AlF.sub.3) at 1 to 5 wt %; one or more of magnesium oxide (MgO), barium oxide (BaO), or calcium oxide (CaO) at 1 to 35 wt %; and one or more of titanium dioxide (TiO.sub.2), cerium dioxide (CeO.sub.2), molybdenum trioxide (MoO.sub.3), bismuth oxide (Bi.sub.2O.sub.3), or copper oxide (CuO) at 10 to 25 wt %, such that a heating time required for cleaning may be shortened and oil contaminants may be completely removed.

ENAMEL COMPOSITION, METHOD FOR PREPARING ENAMEL COMPOSITION, AND COOKING APPLIANCE
20240002280 · 2024-01-04 ·

An enamel composition, a method for preparing an enamel composition, and a cooking appliance are provided. The enamel composition may include phosphorus pentoxide (P.sub.2O.sub.5) at 15 to 50 wt %; silicon dioxide (SiO.sub.2) at 10 to 20 wt %; boron oxide (B.sub.2O.sub.3) at 1 to 15 wt %; one or more of lithium oxide (Li.sub.2O), sodium oxide (Na.sub.2O), or potassium oxide (K.sub.2O) at 5 to 20 wt %; one or more of sodium fluoride (NaF), calcium fluoride (CaF.sub.2), or aluminum fluoride (AlF.sub.3) at 1 to 5 wt %; one or more of magnesium oxide (MgO), barium oxide (BaO), or calcium oxide (CaO) at 1 to 35 wt %; and one or more of titanium dioxide (TiO.sub.2), cerium dioxide (CeO.sub.2), molybdenum trioxide (MoO.sub.3), bismuth oxide (Bi.sub.2O.sub.3), or copper oxide (CuO) at 10 to 25 wt %, such that a heating time required for cleaning may be shortened and oil contaminants may be completely removed.

Carbide, nitride and silicide enhancers for laser absorption

A compounded polymer material that can be laser marked is provided. The compounded polymer material includes an enhancer of nitrides, carbides, silicides, or combinations thereof. Upon forming the compounded polymer material into an article and exposing it to laser radiation, the irradiated portion of the compounded polymer material absorbs the laser radiation, increases in temperature, and forms a mark in the article. A lightness value difference (L) between the mark and the non-irradiated portion of the article has an absolute value of at least 5, and the lightness value difference between the mark and the non-irradiated portion is greater than if the polymer material did not include the enhancer.

SURFACE COATING MATERIAL AND FILM AND STACKED STRUCTURE AND DISPLAY DEVICE AND ARTICLE

Disclosed are a surface coating material including a first material and a second material having a different structure, wherein the first material has a greater weight average molecular weight than the second material, a film, a stacked structure, a display device, and an article including a glass substrate coated with the surface coating material.

ENAMEL COMPOSITION, METHOD FOR PREPARING ENAMEL COMPOSITION, AND COOKING APPLIANCE
20200270168 · 2020-08-27 ·

An enamel composition, a method for preparing an enamel composition, and a cooking appliance are provided. The enamel composition may include 15 to 50 wt % of silicon dioxide (SiO.sub.2); 1 to 10 wt % of boron oxide (B.sub.2O.sub.3); 10 to 20 wt % of at least one of lithium superoxide (Li.sub.2O), sodium oxide (Na.sub.2O), or potassium oxide (K.sub.2O); 1 to 5 wt % of sodium fluoride (NaF); 1 to 10 wt % of zinc oxide (ZnO); and 20 to 50 wt % of at least one of titanium dioxide (TiO.sub.2), molybdenum oxide (MoO.sub.3), bismuth oxide (Bi.sub.2O.sub.3), cerium dioxide (CeO.sub.2), manganese dioxide (MnO.sub.2), or Iron oxide (Fe.sub.2O.sub.3), which provides an enamel composition with a reduced cleaning time, and facilitates cleaning without soaking in water.

ENAMEL COMPOSITION, METHOD FOR PREPARING ENAMEL COMPOSITION, AND COOKING APPLIANCE
20200270171 · 2020-08-27 ·

An enamel composition, a method for preparing an enamel composition, and a cooking appliance are provided. The enamel composition may include phosphorus pentoxide (P.sub.2O.sub.5) at 15 to 50 wt %; silicon dioxide (SiO.sub.2) at 10 to 20 wt %; boron oxide (B.sub.2O.sub.3) at 1 to 15 wt %; one or more of lithium superoxide (Li.sub.2O), sodium oxide (Na.sub.2O), or potassium oxide (K.sub.2O) at 5 to 20 wt %; one or more of sodium fluoride (NaF), calcium fluoride (CaF.sub.2), or aluminum fluoride (AlF.sub.3) at 1 to 5 wt %; one or more of magnesium oxide (MgO), barium oxide (BaO), or calcium oxide (CaO) at 1 to 35 wt %; and one or more of titanium dioxide (TiO.sub.2), cerium dioxide (CeO.sub.2), molybdenum trioxide (MoO.sub.3), bismuth oxide (Bi.sub.2O.sub.3), or copper oxide (CuO) at 10 to 25 wt %, such that a heating time required for cleaning may be shortened and oil contaminants may be completely removed.