C04B2/04

Process and apparatus for manufacture of hydroxide slurry
10358364 · 2019-07-23 · ·

A method of manufacture of high-solids hydroxide slurries from caustic calcined carbonate powder is described, whereby the properties of the slurry are its low resistance to shear thinning to facilitate transport, a high stability for transport and storage, ease of reconstitution after long periods of storage, and, as required, a high concentration of chemically reactive species at the particle surface. The method achieves these specifications by mixing caustic calcined carbonate or hydroxide powder with water in an insulated reactor vessel, and agitating the slurry sufficiently such that the hydration reaction causes the water to spontaneously boil, such that the remaining hydration proceeds spontaneously under the fixed conditions of boiling through the water loss. The mixing process is preferably carried out by a shear pump. A viscosity modifier, such as acetic acid, is used to thin the slurry to enable the mixing system to maintain uniform mixing. The reaction is terminated when the boiling has spontaneously ceased and the temperature has spontaneously dropped to a set point though the reactor heat losses, where the processing time is sufficiently long that the slurry meets the desired specifications.

Process and apparatus for manufacture of hydroxide slurry
10358364 · 2019-07-23 · ·

A method of manufacture of high-solids hydroxide slurries from caustic calcined carbonate powder is described, whereby the properties of the slurry are its low resistance to shear thinning to facilitate transport, a high stability for transport and storage, ease of reconstitution after long periods of storage, and, as required, a high concentration of chemically reactive species at the particle surface. The method achieves these specifications by mixing caustic calcined carbonate or hydroxide powder with water in an insulated reactor vessel, and agitating the slurry sufficiently such that the hydration reaction causes the water to spontaneously boil, such that the remaining hydration proceeds spontaneously under the fixed conditions of boiling through the water loss. The mixing process is preferably carried out by a shear pump. A viscosity modifier, such as acetic acid, is used to thin the slurry to enable the mixing system to maintain uniform mixing. The reaction is terminated when the boiling has spontaneously ceased and the temperature has spontaneously dropped to a set point though the reactor heat losses, where the processing time is sufficiently long that the slurry meets the desired specifications.

Highly Porous Powdered Slaked Lime Composition

The present invention concerns a powdery slaked lime composition an Alpine fluidity greater than 50% and including a first fraction of particles having a size less than 32 m and a second fraction of particles with the size greater than 32 m, the second fraction being less than 10% by weight, compared to the total weight of the composition. The invention also relates to a method for producing same.

PROCESS FOR MANUFACTURE OF HYDROXIDE SLURRY
20190177194 · 2019-06-13 ·

A method of manufacture of high-solids hydroxide slurries from caustic calcined carbonate powder is described, whereby the properties of the slurry are its low resistance to shear thinning to facilitate transport, a high stability for transport and storage, ease of reconstitution after long periods of storage, and, as required, a high concentration of chemically reactive species at the particle surface. The method achieves these specifications by mixing caustic calcined carbonate or hydroxide powder with water in an insulated reactor vessel, and agitating the slurry sufficiently such that the hydration reaction causes the water to spontaneously boil, such that the remaining hydration proceeds spontaneously under the fixed conditions of boiling through the water loss. The mixing process is preferably carried out by a shear pump. A viscosity modifier, such as acetic acid, is used to thin the slurry to enable the mixing system to maintain uniform mixing. The reaction is terminated when the boiling has spontaneously ceased and the temperature has spontaneously dropped to a set point though the reactor heat losses, where the processing time is sufficiently long that the slurry meets the desired specifications.

PROCESS FOR MANUFACTURE OF HYDROXIDE SLURRY
20190177194 · 2019-06-13 ·

A method of manufacture of high-solids hydroxide slurries from caustic calcined carbonate powder is described, whereby the properties of the slurry are its low resistance to shear thinning to facilitate transport, a high stability for transport and storage, ease of reconstitution after long periods of storage, and, as required, a high concentration of chemically reactive species at the particle surface. The method achieves these specifications by mixing caustic calcined carbonate or hydroxide powder with water in an insulated reactor vessel, and agitating the slurry sufficiently such that the hydration reaction causes the water to spontaneously boil, such that the remaining hydration proceeds spontaneously under the fixed conditions of boiling through the water loss. The mixing process is preferably carried out by a shear pump. A viscosity modifier, such as acetic acid, is used to thin the slurry to enable the mixing system to maintain uniform mixing. The reaction is terminated when the boiling has spontaneously ceased and the temperature has spontaneously dropped to a set point though the reactor heat losses, where the processing time is sufficiently long that the slurry meets the desired specifications.

High reactivity lime hydrate and methods of manufacturing and uses thereof

A sorbent composition with improved acid gas reactivity comprising calcium hydroxide particles is provided. In the calcium hydroxide composition, about 90% percent of the calcium hydroxide particles are less than or equal to about 10 microns; the ratio of 90% of the calcium hydroxide particles below a specified size to the ratio of 10% of the calcium hydroxide particles above a specified size is less than about 8; and the calcium hydroxide particles have a BET surface area of about 18 m.sup.2/g or greater.

HIGH TEMPERATURE HYDRATOR
20190144333 · 2019-05-16 ·

An apparatus includes a fluidized bed vessel with inlet ports arranged to receive at least one feed stream comprising calcium oxide, calcium carbonate, water, and a fluidizing gas into a fluidized bed vessel. The calcium oxide contacts the water to initiate a hydrating reaction to produce calcium hydroxide and heat. The fluidized bed vessel is configured to operate with a fluidization velocity that fluidizes and separates at least a portion of the calcium carbonate and at least a portion of the calcium oxide into a first fluidization regime, and at least a portion of the calcium hydroxide and at least another portion of the calcium oxide into a second fluidization regime. The apparatus further includes a heat transfer assembly configured to transfer heat of the hydrating reaction to the calcium carbonate, and a cyclone configured to separate a portion of the fluidization gas from a portion of at least one of the calcium hydroxide, calcium carbonate or calcium oxide.

HIGH TEMPERATURE HYDRATOR
20190144333 · 2019-05-16 ·

An apparatus includes a fluidized bed vessel with inlet ports arranged to receive at least one feed stream comprising calcium oxide, calcium carbonate, water, and a fluidizing gas into a fluidized bed vessel. The calcium oxide contacts the water to initiate a hydrating reaction to produce calcium hydroxide and heat. The fluidized bed vessel is configured to operate with a fluidization velocity that fluidizes and separates at least a portion of the calcium carbonate and at least a portion of the calcium oxide into a first fluidization regime, and at least a portion of the calcium hydroxide and at least another portion of the calcium oxide into a second fluidization regime. The apparatus further includes a heat transfer assembly configured to transfer heat of the hydrating reaction to the calcium carbonate, and a cyclone configured to separate a portion of the fluidization gas from a portion of at least one of the calcium hydroxide, calcium carbonate or calcium oxide.

Method for Producing a Highly Porous Fine Powdered Slaked Lime Composition, and Product Obtained Therefrom

The present invention relates to a method for producing a highly porous fine powdery slaked lime composition, comprising a fluidification step for forming said highly porous fine powdery slaked lime composition having an Alpine fluidity greater than 50% and which is carried out in a dryer/grinder chosen from the group consisting of a pin-type dryer/grinder, a cage-type dryer/grinder, an instantaneous dryer/disagglomerator and a combination of these until the powdery slaked lime composition has a non-solid residual-phase content of less than or equal to 3.5% by weight and greater than or equal to 0.3% by weight, as well as the product obtained therefrom.

Method for Producing a Highly Porous Fine Powdered Slaked Lime Composition, and Product Obtained Therefrom

The present invention relates to a method for producing a highly porous fine powdery slaked lime composition, comprising a fluidification step for forming said highly porous fine powdery slaked lime composition having an Alpine fluidity greater than 50% and which is carried out in a dryer/grinder chosen from the group consisting of a pin-type dryer/grinder, a cage-type dryer/grinder, an instantaneous dryer/disagglomerator and a combination of these until the powdery slaked lime composition has a non-solid residual-phase content of less than or equal to 3.5% by weight and greater than or equal to 0.3% by weight, as well as the product obtained therefrom.