C04B35/78

Temperature and thermal gradient sensor for ceramic matrix composites and methods of preparation thereof

The subject of the present invention relates to a device that can be applied to the surface of a ceramic matrix composites (CMC) in such a way that the CMC itself will contribute to the extraordinarily large thermoelectric power. The present invention obtains greater resolution of temperature measurements, which can be obtained at exceedingly high temperatures.

Temperature and thermal gradient sensor for ceramic matrix composites and methods of preparation thereof

The subject of the present invention relates to a device that can be applied to the surface of a ceramic matrix composites (CMC) in such a way that the CMC itself will contribute to the extraordinarily large thermoelectric power. The present invention obtains greater resolution of temperature measurements, which can be obtained at exceedingly high temperatures.

REGENERATIVE BURNER MEDIA
20200115290 · 2020-04-16 ·

A high strength ceramic body for use in a regenerative burner media bed, comprising a generally spherical refractory portion and a plurality of irregular aggregate portions distributed randomly throughout the generally spherical portion. The aggregate portions are selected from the group comprising tabular alumina, white fused alumina, mullite, chamotte, and combinations thereof. The generally spherical portion has a porosity of less than 1 percent and is more than 99.5 weight percent alumina.

REGENERATIVE BURNER MEDIA
20200115290 · 2020-04-16 ·

A high strength ceramic body for use in a regenerative burner media bed, comprising a generally spherical refractory portion and a plurality of irregular aggregate portions distributed randomly throughout the generally spherical portion. The aggregate portions are selected from the group comprising tabular alumina, white fused alumina, mullite, chamotte, and combinations thereof. The generally spherical portion has a porosity of less than 1 percent and is more than 99.5 weight percent alumina.

HIGH TEMPERATURE OXIDATION PROTECTION FOR COMPOSITES
20200062662 · 2020-02-27 · ·

The present disclosure provides a method for coating a composite structure, comprising forming a first slurry by combining a first pre-slurry composition comprising a first phosphate glass composition, with a primary flow modifier and a first carrier fluid, wherein the primary flow modifier comprises at least one of cellulose or calcium silicate; applying the first slurry on a surface of the composite structure to form a base layer; and heating the composite structure to a temperature sufficient to adhere the base layer to the composite structure.

HIGH TEMPERATURE OXIDATION PROTECTION FOR COMPOSITES
20200062662 · 2020-02-27 · ·

The present disclosure provides a method for coating a composite structure, comprising forming a first slurry by combining a first pre-slurry composition comprising a first phosphate glass composition, with a primary flow modifier and a first carrier fluid, wherein the primary flow modifier comprises at least one of cellulose or calcium silicate; applying the first slurry on a surface of the composite structure to form a base layer; and heating the composite structure to a temperature sufficient to adhere the base layer to the composite structure.

High permittivity nanocomposites for electronic devices

The invention pertains to the field of electronic devices and the preparation thereof. In an aspect is an electronic device comprising a nanocomposite of carbon nanodomains homogeneously embedded in an insulating ceramic matrix, wherein the size and distribution of carbon nanodomains is such that the nanocomposite has a permittivity of greater than or equal to 200.

High permittivity nanocomposites for electronic devices

The invention pertains to the field of electronic devices and the preparation thereof. In an aspect is an electronic device comprising a nanocomposite of carbon nanodomains homogeneously embedded in an insulating ceramic matrix, wherein the size and distribution of carbon nanodomains is such that the nanocomposite has a permittivity of greater than or equal to 200.

High temperature oxidation protection for composites
10526253 · 2020-01-07 · ·

The present disclosure provides a method for coating a composite structure, comprising forming a first slurry by combining a first pre-slurry composition comprising a first phosphate glass composition, with a primary flow modifier and a first carrier fluid, wherein the primary flow modifier comprises at least one of cellulose or calcium silicate; applying the first slurry on a surface of the composite structure to form a base layer; and heating the composite structure to a temperature sufficient to adhere the base layer to the composite structure.

High temperature oxidation protection for composites
10526253 · 2020-01-07 · ·

The present disclosure provides a method for coating a composite structure, comprising forming a first slurry by combining a first pre-slurry composition comprising a first phosphate glass composition, with a primary flow modifier and a first carrier fluid, wherein the primary flow modifier comprises at least one of cellulose or calcium silicate; applying the first slurry on a surface of the composite structure to form a base layer; and heating the composite structure to a temperature sufficient to adhere the base layer to the composite structure.