C04B40/0633

Coated-fine-aggregate, concrete composition and method
09783457 · 2017-10-10 · ·

A concrete composition and method include a portion of fine aggregate bearing a coating of a polymer, which may be a continuous coating layer or a layer of powdered, discrete particles embedded in a binder. The polymeric coating may be a super absorbent polymer (insoluble in water, but absorbing water), or another polymer such as the acrylamides, co-polymers thereof, polyacrylamides, or the like (soluble in water). The coating absorbs water, but particles are too small to form significant voids. Water is absorbed into the concrete mix in far greater proportions (e.g. w/c ratio over 0.5) improving workability, doubling workability time, and improving ultimate compressive stress (strength).

Coated-fine-aggregate, concrete composition and method
09783457 · 2017-10-10 · ·

A concrete composition and method include a portion of fine aggregate bearing a coating of a polymer, which may be a continuous coating layer or a layer of powdered, discrete particles embedded in a binder. The polymeric coating may be a super absorbent polymer (insoluble in water, but absorbing water), or another polymer such as the acrylamides, co-polymers thereof, polyacrylamides, or the like (soluble in water). The coating absorbs water, but particles are too small to form significant voids. Water is absorbed into the concrete mix in far greater proportions (e.g. w/c ratio over 0.5) improving workability, doubling workability time, and improving ultimate compressive stress (strength).

Encapsulation of Silica Nanoparticle for Release

A method of producing a nanosilica-containing cement formulation, the method comprising the steps of mixing an amount of a determinant nanosilica particle and a functional coating; applying a dynamic initiator to trigger a reversible reaction of the functional coating to produce a reversible cage, where the reversible cage surrounds the determinant nanosilica particle to produce an encapsulated nanosilica; and mixing the encapsulated nanosilica and a cement formulation to produce the nanosilica-containing cement formulation

Encapsulation of Silica Nanoparticle for Release

A method of producing a nanosilica-containing cement formulation, the method comprising the steps of mixing an amount of a determinant nanosilica particle and a functional coating; applying a dynamic initiator to trigger a reversible reaction of the functional coating to produce a reversible cage, where the reversible cage surrounds the determinant nanosilica particle to produce an encapsulated nanosilica; and mixing the encapsulated nanosilica and a cement formulation to produce the nanosilica-containing cement formulation

Treatment of Subterranean Formations with Self-Healing Resins

Various embodiments disclosed relate to compositions including a plurality of capsules each independently comprising an outer wall and an inner compartment, the inner compartment independently comprising at least one of a first hardenable resin, a first hardener or activator, and a solvent, self-healing hardened resins formed from the same, and methods of using the same. In various embodiments, the present invention provides a method of treating a subterranean formation including placing the composition in a subterranean formation, and forming a selfhealing hardened resin in the subterranean formation from the composition.

Treatment of Subterranean Formations with Self-Healing Resins

Various embodiments disclosed relate to compositions including a plurality of capsules each independently comprising an outer wall and an inner compartment, the inner compartment independently comprising at least one of a first hardenable resin, a first hardener or activator, and a solvent, self-healing hardened resins formed from the same, and methods of using the same. In various embodiments, the present invention provides a method of treating a subterranean formation including placing the composition in a subterranean formation, and forming a selfhealing hardened resin in the subterranean formation from the composition.

Gas Migration Mitigation for Oil and Gas Well Cements

A method of using a nanosilica-containing cement in a well cementing operation in a well, the method comprising the steps of pumping a nanosilica-containing cement formulation into the well, wherein the nanosilica-containing cement formulation comprises maltodextrin-coated nanosilica and a cement formulation, where the maltodextrin-coated nanosilica comprises nanosilica particles encapsulated by maltodextrin coating, wherein the pH of the nanosilica-containing cement formulation is between 9 and 14, maintaining a temperature in the well due to a temperature of a formation surrounding the well, wherein the disintegration of the maltodextrin coating is initiated due to the temperature and pH of the nanosilica-containing cement, exposing the nanosilica particles due to the disintegration of the maltodextrin coating from the maltodextrin-coated nanosilica, and reacting the nanosilica particles with the cement formulation such that the transition time is reduced.

Gas Migration Mitigation for Oil and Gas Well Cements

A method of using a nanosilica-containing cement in a well cementing operation in a well, the method comprising the steps of pumping a nanosilica-containing cement formulation into the well, wherein the nanosilica-containing cement formulation comprises maltodextrin-coated nanosilica and a cement formulation, where the maltodextrin-coated nanosilica comprises nanosilica particles encapsulated by maltodextrin coating, wherein the pH of the nanosilica-containing cement formulation is between 9 and 14, maintaining a temperature in the well due to a temperature of a formation surrounding the well, wherein the disintegration of the maltodextrin coating is initiated due to the temperature and pH of the nanosilica-containing cement, exposing the nanosilica particles due to the disintegration of the maltodextrin coating from the maltodextrin-coated nanosilica, and reacting the nanosilica particles with the cement formulation such that the transition time is reduced.

Passivated Cement Accelerator

Embodiments relate to cementing operations and, in certain embodiments, to passivated cement accelerators and methods of using passivated cement accelerators in subterranean formations. An embodiment may comprise a method of cementing comprising: providing a cement composition comprising cement, water, and a passivated cement accelerator; and allowing the cement composition to set.

Passivated Cement Accelerator

Embodiments relate to cementing operations and, in certain embodiments, to passivated cement accelerators and methods of using passivated cement accelerators in subterranean formations. An embodiment may comprise a method of cementing comprising: providing a cement composition comprising cement, water, and a passivated cement accelerator; and allowing the cement composition to set.