C04B41/4572

Cool side coating for ceramic or ceramic matrix composite article

An article may include a substrate including a ceramic or a ceramic matrix composite. The substrate defines a hot side surface configured to face a heated gas environment and a cool side surface opposite the hot side surface. The article also includes a cool side coating on the cool side surface. The cool side coating comprises at least one material having a flow temperature equal to or slightly less than a temperature of the heated gas environment.

Cool side coating for ceramic or ceramic matrix composite article

An article may include a substrate including a ceramic or a ceramic matrix composite. The substrate defines a hot side surface configured to face a heated gas environment and a cool side surface opposite the hot side surface. The article also includes a cool side coating on the cool side surface. The cool side coating comprises at least one material having a flow temperature equal to or slightly less than a temperature of the heated gas environment.

HIGH-WEAR-RESISTANCE FAR-INFRARED CERAMIC POLISHED GLAZED TILE AND PREPARATION METHOD THEREFOR

The present application provides a high-wear-resistance far-infrared ceramic polished glazed tile and preparation method therefor. The preparation method includes application of far-infrared overglaze, ink-jet printing, application of transparent far-infrared polished glaze and application of abrasion-resistant far-infrared polished glaze in sequence on a body, firing, and polishing. By adopting the far-infrared overglaze, the transparent far-infrared polished glaze and the abrasion-resistant far-infrared polished glaze in combination, the polished glaze tile can have a far-infrared function, high transparency, and high abrasion resistance.

HIGH-WEAR-RESISTANCE FAR-INFRARED CERAMIC POLISHED GLAZED TILE AND PREPARATION METHOD THEREFOR

The present application provides a high-wear-resistance far-infrared ceramic polished glazed tile and preparation method therefor. The preparation method includes application of far-infrared overglaze, ink-jet printing, application of transparent far-infrared polished glaze and application of abrasion-resistant far-infrared polished glaze in sequence on a body, firing, and polishing. By adopting the far-infrared overglaze, the transparent far-infrared polished glaze and the abrasion-resistant far-infrared polished glaze in combination, the polished glaze tile can have a far-infrared function, high transparency, and high abrasion resistance.

METHOD FOR APPLYING METALS TO CLAY WITH COLORED SLIP AND UNCOLORED CLAY
20170355174 · 2017-12-14 ·

Disclosed herein is a method for applying metals to clay. More particularly, the present invention relates to applying malleable metals, such as silver, to clay, such that the metal attaches to the clay and as an added feature forms beads on the surface of the clay.

METHOD FOR APPLYING METALS TO CLAY WITH COLORED SLIP AND UNCOLORED CLAY
20170355174 · 2017-12-14 ·

Disclosed herein is a method for applying metals to clay. More particularly, the present invention relates to applying malleable metals, such as silver, to clay, such that the metal attaches to the clay and as an added feature forms beads on the surface of the clay.

INTEGRATED POLYMER-DERIVED CERAMIC THIN-FILM SENSOR PRODUCED BY LAYSER PYROLYSIS AND ADDITIVE MANUFACTURING AND FABRICATION METHOD THEREOF

An integrated polymer-derived ceramic (PDC) thin-film sensor produced by laser pyrolysis and additive manufacturing and a fabrication method thereof are provided. Using a metal component or an insulating material as a substrate, a PDC-doped composite insulating film layer with high density, high insulation, and high temperature resistance is formed by a layer-by-layer laser pyrolysis and additive manufacturing on the surface of the metal component, and a strain sensitive layer with excellent electrical conductivity is obtained by Weissenberg direct writing process PDC-doped filler sensitive grid on the composite insulating film layer and laser pyrolysis enhancing graphitization of PDC. In this way, the in situ integrated laser fabrication of highly insulating film layer, sensitive grid with excellent electrical conductivity, and metal substrate based on PDC materials is developed, which achieves the laser processing of “liquid-solid-function” transformation of PDC composites and allows the successful use thereof in strain sensing of metallic materials.

Method for enhancing optical properties in ceramics having applications in dental restorations

A method for enhancing optical properties of sintered, zirconia ceramic bodies and zirconia ceramic dental restorations is provided. The porous or pre-sintered stage of a ceramic body is treated with an yttrium-containing composition and sintered, resulting in sintered ceramic bodies having enhanced optical properties. The enhanced optical properties may be substantially permanent, remaining for the useful life of the sintered ceramic body.

Method for enhancing optical properties in ceramics having applications in dental restorations

A method for enhancing optical properties of sintered, zirconia ceramic bodies and zirconia ceramic dental restorations is provided. The porous or pre-sintered stage of a ceramic body is treated with an yttrium-containing composition and sintered, resulting in sintered ceramic bodies having enhanced optical properties. The enhanced optical properties may be substantially permanent, remaining for the useful life of the sintered ceramic body.

Pressureless sintering-based method for making a two-phase ceramic composite body

Inventive manufacture of CrB.sub.2—Al.sub.2O.sub.3 composites is based on pressureless sintering. According to typical inventive practice, CrB.sub.2 powder and Al.sub.2O.sub.3 powder are mixed together in selected volumetric proportions so that the volume of the CrB.sub.2 does not exceed 50% of the overall volume of the CrB.sub.2—Al.sub.2O.sub.3 mixture. The CrB.sub.2—Al.sub.2O.sub.3 mixture is shaped into a green body. The green body is pressureless sintered in a non-oxidizing atmosphere at a firing temperature in the approximate range between 1600° C. and 2050° C. The present invention succeeds in preparing, via pressureless sintering, a proportionality-associated range of compositions in the CrB.sub.2—Al.sub.2O.sub.3 system, which is a potentially “advanced” ceramic system. A typical inventively fabricated CrB.sub.2—Al.sub.2O.sub.3 composite is inventively configured in a complex shape, and has “advanced” material (e.g., mechanical) properties that are favorable for a contemplated application. Inventive manufacture of ceramic-ceramic composites is thus dually attributed, and uncommonly so, with complex shape-ability and advanced capability.