C08G2261/60

RUBBER COMPOSITION FOR TIRE

Provided is a rubber composition for a tire containing a rubber component including 15 to 55 wt % of an end modified group-containing cycloolefin ring-opening polymer having a glass transition temperature of −120 to −90° C. and 45 to 85 wt % of an end modified group-containing solution polymerized conjugated diene polymer having a glass transition temperature of −60 to −10° C. and having an aromatic vinyl monomer unit content ratio of more than 30 wt % and 50 wt % or less, a silica, and a silane coupling agent including a monosulfide group and/or a thiol group, wherein the content of the silica with respect to 100 parts by weight of the rubber component is 30 to 200 parts by weight, and the content of the silane coupling agent including a monosulfide group and/or a thiol group with respect to 100 parts by weight of the silica is 0.3 to 20 parts by weight.

Process for making urethane-isocyanates

Polyisocyanurate or polyurethane-isocyanurate polymers are made by curing an aromatic polyisocyanate or a mixture of at least one aromatic polyisocyanate and at least one polyol having a hydroxyl equivalent weight of up to 200 in which the isocyanate index is at least 2.00, in the presence of at least one isocyanate trimerization catalyst, to form a polyisocyanurate or polyurethane-isocyanurate polymer having a glass transition temperature of at least 100° C., and then exposing the polyisocyanurate or polyurethane-isocyanurate polymer formed step a) to water under superatmospheric pressure at a temperature of at least 70° C.

POLYMER COMPOSITION AND MOLDED BODY
20170321030 · 2017-11-09 · ·

The present invention is a polymer composition comprising a hydrogenated crystalline cycloolefin ring-opening polymer (A) that comprises a repeating unit derived from a polycyclic norbornene-based monomer that includes three or more rings, 5 to 100 parts by weight of a glass filler (B) based on 100 parts by weight of the hydrogenated crystalline cycloolefin ring-opening polymer (A), and 5 to 20 parts of a metal oxide (C) based on 100 parts by weight of the hydrogenated crystalline cycloolefin ring-opening polymer (A), and a formed article.

The polymer composition according to the present invention exhibits excellent electrical properties (low dielectric loss tangent), excellent adhesion to plating, and excellent reflow heat resistance, and can maintain strength even when subjected to high-temperature/high-humidity conditions.

POLYARYLETHER KETONE IMIDE SULFONE ADHESIVES

Aspects of the present disclosure generally describe polyarylether ketones and methods of use. In some aspects, a composition includes one or more polymers of formulae (I), (II), or (III):

##STR00001##

POLYARYLETHER KETONE IMIDE ADHESIVES

Aspects of the present disclosure generally describe polyarylether ketones and methods of use. In some aspects, a composition includes one or more polymers of formula (IV):

##STR00001##

FRONTALLY POLYMERIZED POLYMERIC BODY AND METHOD OF PRODUCING A POLYMERIC BODY HAVING SPATIALLY VARYING PROPERTIES

A frontally polymerized polymeric body includes, according to a first embodiment, a deformable polymer comprising polydicyclopentadiene (pDCPD) and/or poly(5-ethylidene-2-norbornene) (pENB), where the deformable polymer has a fracture strain of at least about 0.5 mm mm.sup.−1. According to a second embodiment, the frontally polymerized polymeric body includes a first polymer comprising pDCPD and/or pENB, and a second polymer adjacent to the first polymer also comprising the pDCPD and/or the pENB. The second polymer is more or less deformable than the first polymer. Thus, the frontally polymerized polymeric body exhibits spatially varying mechanical and/or other properties.

Copolymer, polymer, molding material and resin molded body

The present invention provides: a copolymer (A) which is a copolymer obtained by copolymerizing one or plural cycloolefin monomers and one or plural acyclic olefin monomers, or a copolymer obtained by copolymerizing two or more cycloolefin monomers, wherein the glass transition temperature (Tg) of the copolymer is 100° C. or higher, the refractive index of the copolymer is 1.545 or higher, and the Abbe's number of the copolymer is 50 or larger, and at least one of the cycloolefin monomers is a deltacyclene.

COPOLYMER, ELECTROLUMINESCENCE DEVICE MATERIAL INCLUDING COPOLYMER, AND ELECTROLUMINESCENCE DEVICE

A copolymer including a structural unit represented by Chemical Formula 1

##STR00001##

wherein the copolymer is capable of improving luminous efficiency and durability, particularly, an improvement in luminescence life-span, of an electroluminescence device, particularly a quantum dot electroluminescence device.

Olefin metathesis photopolymers

Described herein are compositions and methods for processing photopolymers based on olefin metathesis. The compositions and methods comprise latent ruthenium complexes and photoacids and/or photoacid generators.

Ring-opening copolymer composition
11718709 · 2023-08-08 · ·

A ring-opened copolymer composition has a ring-opened copolymer containing structural unit derived from a norbornene compound represented by general formula (1) below and structural unit derived from a monocyclic olefin, wherein a content of a norbornene compound represented by general formula (1) is 1 ppm by weight or more and 1000 ppm by weight or less based on the ring-opened copolymer, ##STR00001## wherein R.sup.1 to R.sup.4 are each a hydrogen atom, a hydrocarbon group having 1 to 20 carbon atoms, or a substituent containing a halogen atom, a silicon atom, an oxygen atom or a nitrogen atom, and R.sup.2 and R.sup.3 may be bonded to each other to form a ring, and “m” is 0 or 1.