C08K5/10
Film for laminating glass, method for manufacturing film for laminating glass, and vehicle comprising film for laminating glass
A film for laminating glass includes a polyvinyl acetal, a plasticizer, inorganic particles, and a trioxane-based compound.
Adhesive Composition
The present disclosure provides an adhesive composition. The adhesive composition contains (A) multi-stage latex polymer particles, (B) a linear diamine base, and (C) an ethoxylated surfactant. The (A) multi-stage latex polymer particles include (i) a first-stage polymer containing acrylic acid monomer and a first vinyl monomer, and (ii) a second-stage polymer containing a meth acrylic acid monomer and a second vinyl monomer, with the proviso that the second vinyl monomer is different than the meth acrylic acid monomer. The first-stage polymer is bound to the second-stage polymer.
LOW VISCOSITY DUAL CURE ADDITIVE MANUFACTURING RESINS
Provided herein according to some embodiments is a dual cure additive manufacturing resin, comprising: (i) a light polymerizable component, (ii) a photoinitiator, (iii) a heat polymerizable component, and (iv) a non-reactive diluent, which resin is useful for the production of three-dimensional objects by additive manufacturing. Methods of using the same are also provided.
LOW VISCOSITY DUAL CURE ADDITIVE MANUFACTURING RESINS
Provided herein according to some embodiments is a dual cure additive manufacturing resin, comprising: (i) a light polymerizable component, (ii) a photoinitiator, (iii) a heat polymerizable component, and (iv) a non-reactive diluent, which resin is useful for the production of three-dimensional objects by additive manufacturing. Methods of using the same are also provided.
Ink, method of manufacturing ink, printing method, and printing device
An ink contains water, an organic solvent, a polyurethane resin, and a cyclic ester including a structure represented by Chemical formula I, wherein the proportion of the cyclic ester having a crystal having a particle diameter of 1 μm or greater is less than 4 ppm of the total of the ink after the ink is allowed to stand at a temperature range of from 20 to 30 degrees C. for 30 days. ##STR00001##
Ink, method of manufacturing ink, printing method, and printing device
An ink contains water, an organic solvent, a polyurethane resin, and a cyclic ester including a structure represented by Chemical formula I, wherein the proportion of the cyclic ester having a crystal having a particle diameter of 1 μm or greater is less than 4 ppm of the total of the ink after the ink is allowed to stand at a temperature range of from 20 to 30 degrees C. for 30 days. ##STR00001##
SULPHUR ADDITIVE AND SULPHUR MODIFIED BITUMEN
The present disclosure discloses an additive for preparing modified bitumen comprising a) sulphur with a weight percentage in the range of 90-95% with respect to the additive; b) at least two H2S suppressants with a combined weight percentage in the range of 4-7% with respect to the additive; c) bitumen with a weight percentage in the range of 0.5-3% with respect to the additive; and d) at least one smell masking agent in the range of 0.05-1.0% with respect to the additive. The present disclosure provides a convenient process for the preparation of the additive. The present disclosure also reveals a sulphur modified bitumen and a process for preparing the sulphur modified bitumen.
SULPHUR ADDITIVE AND SULPHUR MODIFIED BITUMEN
The present disclosure discloses an additive for preparing modified bitumen comprising a) sulphur with a weight percentage in the range of 90-95% with respect to the additive; b) at least two H2S suppressants with a combined weight percentage in the range of 4-7% with respect to the additive; c) bitumen with a weight percentage in the range of 0.5-3% with respect to the additive; and d) at least one smell masking agent in the range of 0.05-1.0% with respect to the additive. The present disclosure provides a convenient process for the preparation of the additive. The present disclosure also reveals a sulphur modified bitumen and a process for preparing the sulphur modified bitumen.
CELLULOSE ACETATE AND CELLULOSE ACETATE COMPOSITION
This cellulose acetate has a total degree of acetyl substitution of 1.75 or more and 2.55 or less, and a degree of acetyl substitution at 2-position or a degree of acetyl substitution at 3-position is 0.7 or less. This cellulose acetate composition includes the cellulose acetate and an additive. The additive is one or more selected from the group consisting of (a) substances of which a pH of a 1 wt. % aqueous solution at 20° C. is 8 or more, (b) substances that dissolve in water at 20° C. in an amount of 2 wt. % or more, and (c) substances that exhibit biodegradability in seawater.
CELLULOSE ACETATE AND CELLULOSE ACETATE COMPOSITION
This cellulose acetate has a total degree of acetyl substitution of 1.75 or more and 2.55 or less, and a degree of acetyl substitution at 2-position or a degree of acetyl substitution at 3-position is 0.7 or less. This cellulose acetate composition includes the cellulose acetate and an additive. The additive is one or more selected from the group consisting of (a) substances of which a pH of a 1 wt. % aqueous solution at 20° C. is 8 or more, (b) substances that dissolve in water at 20° C. in an amount of 2 wt. % or more, and (c) substances that exhibit biodegradability in seawater.