C09D201/06
PAINT COMPOSITION
A paint composition contains (A) a binder component, (B) a first rheology control agent, and (C) a second rheology control agent, wherein the first rheology control agent (B) is a non-aqueous dispersion resin (b); the second rheology control agent (C) contains a reaction product of (c1) a polyisocyanate compound, (c2) a primary monoamine having a number average molecular weight of 300 or less, and (c3) a polyether amine having two or more amino groups and having a number average molecular weight of 1000 or more and less than 6000; and the proportion of the polyether amine having two or more amino groups and having a number average molecular weight of 1000 or more and less than 6000 (c3) is within the range of 10 to 30 mass % based on the total amount of the components (c1) to (c3).
PAINT COMPOSITION
A paint composition contains (A) a binder component, (B) a first rheology control agent, and (C) a second rheology control agent, wherein the first rheology control agent (B) is a non-aqueous dispersion resin (b); the second rheology control agent (C) contains a reaction product of (c1) a polyisocyanate compound, (c2) a primary monoamine having a number average molecular weight of 300 or less, and (c3) a polyether amine having two or more amino groups and having a number average molecular weight of 1000 or more and less than 6000; and the proportion of the polyether amine having two or more amino groups and having a number average molecular weight of 1000 or more and less than 6000 (c3) is within the range of 10 to 30 mass % based on the total amount of the components (c1) to (c3).
DEVICE AND PRODUCTION METHOD FOR THE SAME
A device includes a substrate and a hydrophilic polymer layer made of a hydrophilic polymer having a hydroxyl group. The hydrophilic polymer layer having a hydroxyl group is fixed to at least a part of a surface of the substrate and the hydrophilic polymer further has an amide group. A liquid film retention time of the device is 15 seconds or more. The device has a surface of a substrate which is hydrophilized. A method for producing the device by a simple method is also disclosed.
THERMOSETTING COATING COMPOSITION AND COATED ARTICLE
A thermosetting coating composition includes a hydroxyl group-containing resin, a curing agent, a phosphazene compound, and a solvent. The curing agent is a polyisocyanate curing agent and/or a blocked polyisocyanate curing agent.
PAINT COMPOSITION
A paint composition contains (A) a binder component, (B) a first rheology control agent, and (C) a second rheology control agent, wherein the first rheology control agent (B) contains a reaction product of (b1) a polyisocyanate compound, (b2) a primary monoamine having a number average molecular weight of 300 or less, and (b3) a polyether amine having a number average molecular weight of more than 300 and less than 6000; the proportion of the polyether amine having a number average molecular weight of more than 300 and less than 6000 (b3) is 0.5 mass % or more and less than 10 mass % based on the total amount of the components (b1) to (b3); the second rheology control agent (C) contains a reaction product of (c1) a polyisocyanate compound, (c2) a primary monoamine having a number average molecular weight of 300 or less, and (c3) a polyether amine having two or more amino groups and having a number average molecular weight of 1000 or more and less than 6000; and the proportion of the polyether amine having two or more amino groups and having a number average molecular weight of 1000 or more and less than 6000 (c3) is within a range of 10 to 30 mass % based on the total amount of the components (c1) to (c3).
PAINT COMPOSITION
A paint composition contains (A) a binder component, (B) a first rheology control agent, and (C) a second rheology control agent, wherein the first rheology control agent (B) contains a reaction product of (b1) a polyisocyanate compound, (b2) a primary monoamine having a number average molecular weight of 300 or less, and (b3) a polyether amine having a number average molecular weight of more than 300 and less than 6000; the proportion of the polyether amine having a number average molecular weight of more than 300 and less than 6000 (b3) is 0.5 mass % or more and less than 10 mass % based on the total amount of the components (b1) to (b3); the second rheology control agent (C) contains a reaction product of (c1) a polyisocyanate compound, (c2) a primary monoamine having a number average molecular weight of 300 or less, and (c3) a polyether amine having two or more amino groups and having a number average molecular weight of 1000 or more and less than 6000; and the proportion of the polyether amine having two or more amino groups and having a number average molecular weight of 1000 or more and less than 6000 (c3) is within a range of 10 to 30 mass % based on the total amount of the components (c1) to (c3).
Coating liquid composition and process for producing article provided with film using it
To provide a coating liquid composition containing a fluororesin, whereby a film excellent in the surface flatness can be formed by a plate printing method. A coating liquid composition comprising a fluororesin having an aliphatic ring in the main chain and a fluorinated solvent, wherein the fluorinated solvent has a boiling point of at least 185° C., and the composition has a viscosity of at most 1,000 mP.Math.s at 25° C.
Coating liquid composition and process for producing article provided with film using it
To provide a coating liquid composition containing a fluororesin, whereby a film excellent in the surface flatness can be formed by a plate printing method. A coating liquid composition comprising a fluororesin having an aliphatic ring in the main chain and a fluorinated solvent, wherein the fluorinated solvent has a boiling point of at least 185° C., and the composition has a viscosity of at most 1,000 mP.Math.s at 25° C.
RHEOLOGY CONTROL AGENT AND PAINT COMPOSITION
A rheology control agent contains a reaction product of a polyisocyanate compound (a1), a primary monoamine having a number average molecular weight of 300 or less (a2), and a polyether amine having two or more amino groups and having a number average molecular weight of 1000 or more and less than 6000 (a3), wherein the proportion of the polyether amine having a number average molecular weight of 1000 or more and less than 6000 (a3) is within the range of 10 to 30 mass % based on the total amount of the components (a1) to (a3).
RHEOLOGY CONTROL AGENT AND PAINT COMPOSITION
A rheology control agent contains a reaction product of a polyisocyanate compound (a1), a primary monoamine having a number average molecular weight of 300 or less (a2), and a polyether amine having two or more amino groups and having a number average molecular weight of 1000 or more and less than 6000 (a3), wherein the proportion of the polyether amine having a number average molecular weight of 1000 or more and less than 6000 (a3) is within the range of 10 to 30 mass % based on the total amount of the components (a1) to (a3).