20170368420 · 2017-12-28 · ·

In a golf ball having a core and a cover of at least one layer, the core and/or at least one layer of the cover are formed of a resin composition that includes (A) 100 parts by weight of a thermoplastic resin, and (B) 1 to 30 parts by weight of a compound having a fluorene skeleton, or a derivative thereof. This resin composition for golf balls has an improved injection-moldability and thus enables the ball to achieve both a reduced spin rate and a good durability (scuff resistance).

Method of golf ball manufacture employing ultrasonic welding, and resulting golf ball and golf ball components and/or layers

A golf ball a core, one or more intermediate layers, and one or more cover layers. The core may comprise an inner portion and an outer portion. One or more layers of the golf ball may be formed by the application of ultrasonic welding on two half shells to form. One or more of the layers may be formed by a number of different chemical compositions, and may have varying thicknesses, hardnesses, coefficients of restitution, and PGA compression. The golf ball itself may have varying coefficient of restitution and PGA compression, depending on the layers.

METHOD OF GOLF BALL MANUFACTURE EMPLOYING ULTRASONIC WELDING, AND RESULTING GOLF BALL AND GOLF BALL COMPONENTS AND/OR LAYERS
20230256302 · 2023-08-17 ·

A golf ball a core, one or more intermediate layers, and one or more cover layers. The core may comprise an inner portion and an outer portion. One or more layers of the golf ball may be formed by the application of ultrasonic welding on two half shells to form. One or more of the layers may be formed by a number of different chemical compositions, and may have varying thicknesses, hardnesses, coefficients of restitution, and PGA compression. The golf ball itself may have varying coefficient of restitution and PGA compression, depending on the layers.

GOLF BALL

An object of the present disclosure is to provide a golf ball having good shot feeling and excellent durability while having non-lowered resilience. The present disclosure provides a golf ball comprising a spherical core and one or more cover layers disposed outside the spherical core, wherein at least one layer of the cover layers contains (A) a base resin and (B) a polyethylene oxide.

METHOD OF GOLF BALL MANUFACTURE EMPLOYING ULTRASONIC WELDING, AND RESULTING GOLF BALL AND GOLF BALL COMPONENTS AND/OR LAYERS
20210252343 · 2021-08-19 ·

A golf ball a core, one or more intermediate layers, and one or more cover layers. The core may comprise an inner portion and an outer portion. One or more layers of the golf ball may be formed by the application of ultrasonic welding on two half shells to form. One or more of the layers may be formed by a number of different chemical compositions, and may have varying thicknesses, hardnesses, coefficients of restitution, and PGA compression. The golf ball itself may have varying coefficient of restitution and PGA compression, depending on the layers.

Golf ball incorporating at least one layer of neutralized acid polymer composition containing low molecular weight acid wax(es) as sole acid polymer component and low molecular weight non-acid wax(es) in the non-acid polymer component

Golf ball comprising layer(s) comprised of a mixture of: (a) low molecular weight acid-containing wax(es); (b) non-acid-polymer(s) including at least one low molecular weight non-acid wax such as high density oxidized polyethylene homopolymers; ethylene maleic anhydride copolymers; polypropylene maleic anhydride copolymers; polypropylene homopolymers; ethylene-vinyl acetate copolymers; high density oxidized homopolymers; oxidized copolymers; polyethylene micronized waxes; polytetrafluoroethylene micronized waxes; emulsifiable low molecular weight non-acid waxes; non-emulsifiable low molecular weight non-acid waxes; and/or chemically modified low molecular weight non-acid waxes; and (c) organic acid(s) or salt thereof. Molecular weight of each low molecular weight acid-containing wax is about 500 to 7000, or up to 30,000. Interactions between components (a), (b), and (c) advantageously produce layer of ionomeric material having heat stability, processability, and well-retained durability, adhesion, CoR, compression and targeted feel without need for blending high and low molecular weight acid-containing polymer(s).

Golf ball

In a golf ball having a core and a cover of at least one layer, the outermost layer of the cover is formed of a resin composition that includes (A) 100 parts by weight of a thermoplastic resin, and (B) 1 to 30 parts by weight of a compound having a fluorene skeleton, or a derivative thereof, and the resin composition has a melt flow rate of at least 3.0 g/10 min. This resin composition for golf balls has an improved injection-moldability and thus enables the ball to achieve both a reduced spin rate and a good durability (scuff resistance).

GOLF BALL INCORPORATING AT LEAST ONE LAYER OF NEUTRALIZED ACID POLYMER COMPOSITION CONTAINING LOW MOLECULAR WEIGHT ACID WAX(ES) AS SOLE ACID POLYMER COMPONENT AND LOW MOLECULAR WEIGHT NON-ACID WAX(ES) IN THE NON-ACID POLYMER COMPONENT

Golf ball comprising layer(s) comprised of a mixture of: (a) low molecular weight acid-containing wax(es); (b) non-acid-polymer(s) including at least one low molecular weight non-acid wax such as high density oxidized polyethylene homopolymers; ethylene maleic anhydride copolymers; polypropylene maleic anhydride copolymers; polypropylene homopolymers; ethylene-vinyl acetate copolymers; high density oxidized homopolymers; oxidized copolymers; polyethylene micronized waxes; polytetrafluoroethylene micronized waxes; emulsifiable low molecular weight non-acid waxes; non-emulsifiable low molecular weight non-acid waxes; and/or chemically modified low molecular weight non-acid waxes; and (c) organic acid(s) or salt thereof. Molecular weight of each low molecular weight acid-containing wax is about 500 to 7000, or up to 30,000. Interactions between components (a), (b), and (c) advantageously produce layer of ionomeric material having heat stability, processability, and well-retained durability, adhesion, CoR, compression and targeted feel without need for blending high and low molecular weight acid-containing polymer(s).

Golf ball incorporating at least one layer of neutralized acid polymer composition containing low molecular weight acid wax(es) as sole acid polymer component and low molecular weight non-acid wax(es) in the non-acid polymer component

Golf ball comprising layer(s) comprised of neutralized acid polymer composition consisting of mixture of: (a) low molecular weight acid-containing wax(es); (b) non-acid polymer(s) including at least one low molecular weight non-acid wax such as high density oxidized polyethylene homopolymers; ethylene maleic anhydride copolymers; polypropylene maleic anhydride copolymers; polypropylene homopolymers; ethylene-vinyl acetate copolymers; high density oxidized homopolymers; oxidized copolymers; polyethylene micronized waxes; polytetrafluoroethylene micronized waxes; emulsifiable low molecular weight non-acid waxes; non-emulsifiable low molecular weight non-acid waxes; and/or chemically modified low molecular weight non-acid waxes; and (c) organic acid(s) or salt thereof. Molecular weight of each low molecular weight acid-containing wax is about 500 to 7000, or up to 30,000. Interactions between components (a), (b), and (c) advantageously produce layer of ionomeric material having heat stability, processability, and well-retained durability, adhesion, CoR, compression and targeted feel without need for blending high and low molecular weight acid-containing polymer(s).

Golf ball incorporating at least one layer of plasticized neutralized acid polymer composition containing low molecular weight acid wax(es) as sole acid polymer component and low molecular weight non-acid wax(es) in the non-acid polymer component

Golf ball comprising layer(s) comprised of plasticized neutralized acid polymer composition consisting of mixture of: (a) low molecular weight acid-containing wax(es); (b) non-acid-polymer(s) including at least one low molecular weight non-acid wax such as high density oxidized polyethylene homopolymers; ethylene maleic anhydride copolymers; polypropylene maleic anhydride copolymers; polypropylene homopolymers; ethylene-vinyl acetate copolymers; high density oxidized homopolymers; oxidized copolymers; polyethylene micronized waxes; polytetrafluoroethylene micronized waxes; emulsifiable low molecular weight non-acid waxes; non-emulsifiable low molecular weight non-acid waxes; and/or chemically modified low molecular weight non-acid waxes; (c) organic acid(s) or salt thereof; and (d) plasticizer(s). Molecular weight of each low molecular weight acid-containing wax is about 500 to 7000, or up to 30,000. Interactions between components (a), (b), (c) and (d) advantageously produce layer of ionomeric material having heat stability, processability, and well-retained durability, adhesion, CoR, compression and softer feel without need for blending high and low molecular weight acid-containing polymer(s).