B03D1/012

Mining Collectors
20220388013 · 2022-12-08 ·

A family of mining collectors and surfactants that uses alkoxylates allows for the easy adjustment of solubility and molecular weight useful because anionic and cationic mineral collectors require such varying degrees of solubility and molecular weight. The family of the present invention allows for the optimization of both parameters and an increase in collector efficiency.

Mining Collectors
20220388013 · 2022-12-08 ·

A family of mining collectors and surfactants that uses alkoxylates allows for the easy adjustment of solubility and molecular weight useful because anionic and cationic mineral collectors require such varying degrees of solubility and molecular weight. The family of the present invention allows for the optimization of both parameters and an increase in collector efficiency.

Process to treat phosphate ores

The present invention relates to a process for treating non-sulfidic ores with a collector composition containing a primary and a secondary collector, wherein the primary collector is selected from the group of amphoteric and anionic surface active compounds and the secondary collector is an ethoxylated fatty acid wherein the average degree of ethoxylation is higher than 0 and less than 2, to collector compositions suitable for use in the above process, and to pulp comprising such collector compositions.

Method for removing heavy metals from an aqueous solution

The invention provides a method for removing a dissolved heavy metal from an aqueous solution. The method comprises dissolving in the aqueous solution a foaming agent of formula (I) or a salt thereof. The method further comprises passing a gas through the aqueous solution to form a foam and separating the foam from the aqueous solution. ##STR00001##

Method for removing heavy metals from an aqueous solution

The invention provides a method for removing a dissolved heavy metal from an aqueous solution. The method comprises dissolving in the aqueous solution a foaming agent of formula (I) or a salt thereof. The method further comprises passing a gas through the aqueous solution to form a foam and separating the foam from the aqueous solution. ##STR00001##

Mineral processing

According to the invention there is provided a method of processing a mixture of minerals including the steps of: (a) providing a mixture of minerals which includes a metal containing mineral and one or more unwanted gangue minerals; (b) achieving a contact between the mixture of minerals and polymeric material that includes a mineral binding moiety which selectively binds to the metal containing mineral; and (c) separating the gangue minerals and the polymeric material which has the metal containing mineral bound thereto.

Mineral processing

According to the invention there is provided a method of processing a mixture of minerals including the steps of: (a) providing a mixture of minerals which includes a metal containing mineral and one or more unwanted gangue minerals; (b) achieving a contact between the mixture of minerals and polymeric material that includes a mineral binding moiety which selectively binds to the metal containing mineral; and (c) separating the gangue minerals and the polymeric material which has the metal containing mineral bound thereto.

Preparation of copper(II)-ammonia complex ion sulfidization activator and sulfidization flotation method for copper oxide ore

The disclosure relates to mineral processing, and more particularly to a copper(II)-ammonia complex ion sulfidization activator, and its preparation and application. A molar ratio of NH.sub.3 to Cu.sup.2+ in the active ingredient of the copper(II)-ammonia complex ion sulfidization activator is 2:1-4:1. The preparation method includes: dropwise adding an ammonia solution to a copper salt solution; and adjusting the mixture to pH 6-7.2 with dilute sulfuric acid to obtain the copper(II)-ammonia complex ion sulfidization activator. During the sulfidization flotation for the copper oxide ore, the copper(II)-ammonia complex ion sulfidization activator is added and mixed uniformly with the ore slurry prior to the introduction of the sulfidizing agent.

SODIUM PETROLEUM SULFONATE COLLECTOR FOR FLUORITE FLOTATION AND ITS PREPARATION AND APPLICATION METHOD
20230143136 · 2023-05-11 ·

Disclosed is a sodium petroleum sulfonate collector for fluorite flotation, comprising sodium petroleum sulfonate and non-polar oil, wherein the molar ratio of the non-polar oil to the sodium petroleum sulfonate is 3.33-5.67, the sodium petroleum sulfonate comprises raw material oil and active substance, the molecular weight of the raw material oil is 350-450, the molecular weight of the sodium petroleum sulfonate is 500-750, the aromatic hydrocarbon comprises benzene ring hydrocarbon and naphthalene ring hydrocarbon, the content of the benzene ring hydrocarbon is 5% to 11%, and the content of the naphthalene ring hydrocarbon is 5% to 5.2%, the raw material oil needs to be sulfonated by sulfur trioxide, and the molar ratio of the aromatic hydrocarbon to the sulfur trioxide in the raw material oil is 2.4 to 5. The sodium petroleum sulfonate collector proposed by this disclosure is both efficient and low temperature resistant.

SODIUM PETROLEUM SULFONATE COLLECTOR FOR FLUORITE FLOTATION AND ITS PREPARATION AND APPLICATION METHOD
20230143136 · 2023-05-11 ·

Disclosed is a sodium petroleum sulfonate collector for fluorite flotation, comprising sodium petroleum sulfonate and non-polar oil, wherein the molar ratio of the non-polar oil to the sodium petroleum sulfonate is 3.33-5.67, the sodium petroleum sulfonate comprises raw material oil and active substance, the molecular weight of the raw material oil is 350-450, the molecular weight of the sodium petroleum sulfonate is 500-750, the aromatic hydrocarbon comprises benzene ring hydrocarbon and naphthalene ring hydrocarbon, the content of the benzene ring hydrocarbon is 5% to 11%, and the content of the naphthalene ring hydrocarbon is 5% to 5.2%, the raw material oil needs to be sulfonated by sulfur trioxide, and the molar ratio of the aromatic hydrocarbon to the sulfur trioxide in the raw material oil is 2.4 to 5. The sodium petroleum sulfonate collector proposed by this disclosure is both efficient and low temperature resistant.