Patent classifications
B21B2045/0227
Annular cooling device for large-scale cylindrical shell
The present invention discloses an annular cooling device for large-scale cylindrical shell, which comprises a plurality of inner jet devices and outer jet devices; the inner jet devices are arranged inside the cylindrical shell along the inner periphery; the outer jet devices are arranged outside the cylindrical shell along the outer periphery; each inner jet device and each outer jet device are oppositely arranged; the inner jet devices are used for spraying cooling medium to the inner wall of the cylindrical shell; the outer jet devices are used for spraying the cooling medium to the outer wall of the cylindrical shell; and the spray ranges of each inner jet device and each outer jet device in the axial direction of the cylindrical shell are both greater than the length of the cylindrical shell.
Piercing machine, and method for producing seamless metal pipe using the same
A piercing machine includes a plurality of skewed rolls, a plug, a mandrel bar and an outer surface cooling mechanism. The outer surface cooling mechanism is disposed around the mandrel bar at a position that is rearward of the plug, and with respect to an outer surface of a hollow shell advancing through a cooling zone which has a specific length in an axial direction of the mandrel bar and which is located rearward of the plug, as seen from an advancing direction of the hollow shell, the outer surface cooling mechanism ejects a cooling fluid toward an upper part of the outer surface, a lower part of the outer surface, a left part of the outer surface and a right part of the outer surface of the hollow shell to cool the hollow shell inside the cooling zone.
Production method of seamless steel pipe
The production method of a seamless steel pipe includes a heating step of heating an Nb-containing steel material to 800 to 1030° C., a pipe-making step of producing a hollow shell by performing piercing-rolling or elongation-rolling on the Nb-containing steel material, by using a piercing mill including a plurality of skewed rolls, a plug disposed between the plurality of skewed rolls, and a mandrel bar, and a cooling step immediately after rolling, of carrying out cooling using a cooling liquid on a hollow shell portion that passes between rear ends of the plurality of skewed rolls, in the hollow shell, so as to reduce an outer surface temperature of the hollow shell portion to 700 to 1000° C. within 15.0 seconds after the hollow shell portion passes between the rear ends of the plurality of skewed rolls.
Hot and cold composite formed square and rectangular steel tube with thickened corners and production method
A hot and cold composite formed square and rectangular steel tube and a production method for the same are provided. The radius of an outer corner of the square and rectangular steel tube meets the following conditions: when t is less than or equal to 6 mm, R is greater than 0 and less than 2.0 t; when t is greater than 6 mm and less than or equal to 10 mm, R is greater than 0 and less than 2.5 t; when t is greater than 10 mm, R is greater than 0 and less than 3.0 t, wherein t is the wall thickness of a straight tube part of the square and rectangular steel tube; R is the radius of each of the outer corners of the four corners of the square and rectangular steel tube; and the wall thickness of each corner of the square and rectangular steel tube is between 1.0 t and 1.8 t.
APPARATUS LINE FOR MANUFACTURING SEAMLESS STEEL PIPE AND TUBE AND METHOD OF MANUFACTURING DUPLEX SEAMLESS STAINLESS STEEL PIPE
An apparatus line for manufacturing seamless steel pipes and tubes includes: a heating apparatus for heating a steel raw material; a piercing apparatus for piercing the heated steel raw material thus forming a hollow material; and a rolling apparatus for applying working to the hollow material to form a seamless steel pipe having a predetermined shape. A cooling apparatus is arranged on an exit side of the rolling apparatus. A heated steel raw material is worked by the rolling apparatus after being pierced by the piercing apparatus, and thereafter, using a surface temperature of a hollow piece before being cooled by the cooling apparatus as a cooling start temperature, the hollow piece is cooled to a cooling stop temperature differing by 50° C. or more from the cooling start temperature and being equal to or above 600° C. at an average cooling speed of 1.0° C./s or more in terms of an outer surface temperature.
Apparatus line for manufacturing seamless steel pipe and tube and method of manufacturing duplex seamless stainless steel pipe
An apparatus line for manufacturing seamless steel pipes and tubes includes: a heating apparatus for heating a steel raw material; a piercing apparatus for piercing the heated steel raw material thus forming a hollow material; and a rolling apparatus for applying working to the hollow material to form a seamless steel pipe having a predetermined shape. A cooling apparatus is arranged on an exit side of the rolling apparatus. A heated steel raw material is worked by the rolling apparatus after being pierced by the piercing apparatus, and thereafter, using a surface temperature of a hollow piece before being cooled by the cooling apparatus as a cooling start temperature, the hollow piece is cooled to a cooling stop temperature differing by 50° C. or more from the cooling start temperature and being equal to or above 600° C. at an average cooling speed of 1.0° C./s or more in terms of an outer surface temperature.
HOT AND COLD COMPOSITE FORMED SQUARE AND RECTANGULAR STEEL TUBE WITH THICKENED CORNERS AND PRODUCTION METHOD
A hot and cold composite formed square and rectangular steel tube and a production method for the same are provided. The radius of an outer corner of the square and rectangular steel tube meets the following conditions: when t is less than or equal to 6 mm, R is greater than 0 and less than 2.0 t; when t is greater than 6 mm and less than or equal to 10 mm, R is greater than 0 and less than 2.5 t; when t is greater than 10 mm, R is greater than 0 and less than 3.0 t, wherein t is the wall thickness of a straight tube part of the square and rectangular steel tube; R is the radius of each of the outer corners of the four corners of the square and rectangular steel tube; and the wall thickness of each corner of the square and rectangular steel tube is between 1.0 t and 1.8 t.
Annular Cooling Device for Large-Scale Cylindrical Shell
The present invention discloses an annular cooling device for large-scale cylindrical shell, which comprises a plurality of inner jet devices and outer jet devices; the inner jet devices are arranged inside the cylindrical shell along the inner periphery; the outer jet devices are arranged outside the cylindrical shell along the outer periphery; each inner jet device and each outer jet device are oppositely arranged; the inner jet devices are used for spraying cooling medium to the inner wall of the cylindrical shell; the outer jet devices are used for spraying the cooling medium to the outer wall of the cylindrical shell; and the spray ranges of each inner jet device and each outer jet device in the axial direction of the cylindrical shell are both greater than the length of the cylindrical shell.
PRODUCTION METHOD OF SEAMLESS STEEL PIPE
The production method of a seamless steel pipe includes a heating step of heating an Nb-containing steel material to 800 to 1030 C., a pipe-making step of producing a hollow shell by performing piercing-rolling or elongation-rolling on the Nb-containing steel material, by using a piercing mill including a plurality of skewed rolls, a plug disposed between the plurality of skewed rolls, and a mandrel bar, and a cooling step immediately after rolling, of carrying out cooling using a cooling liquid on a hollow shell portion that passes between rear ends of the plurality of skewed rolls, in the hollow shell, so as to reduce an outer surface temperature of the hollow shell portion to 700 to 1000 C. within 15.0 seconds after the hollow shell portion passes between the rear ends of the plurality of skewed rolls.
PIERCING MACHINE, AND METHOD FOR PRODUCING SEAMLESS METAL PIPE USING THE SAME
A piercing machine includes a plurality of skewed rolls, a plug, a mandrel bar and an outer surface cooling mechanism. The outer surface cooling mechanism is disposed around the mandrel bar at a position that is rearward of the plug, and with respect to an outer surface of a hollow shell advancing through a cooling zone which has a specific length in an axial direction of the mandrel bar and which is located rearward of the plug, as seen from an advancing direction of the hollow shell, the outer surface cooling mechanism ejects a cooling fluid toward an upper part of the outer surface, a lower part of the outer surface, a left part of the outer surface and a right part of the outer surface of the hollow shell to cool the hollow shell inside the cooling zone.