A melting pot includes a pot body and a float salvaging apparatus. The pot body is provided with a melting chamber having an open upper end. The float salvaging apparatus includes a hanging bracket, a bearing plate, a rotating plate and a drive assembly configured to drive pivoting of the rotating plate. The hanging bracket is disposed above the melting chamber. The rotating plate is pivotably disposed on the bearing plate, and the bearing plate and the rotating plate are provided on the hanging bracket between an initial position and a first salvaging position in a manner of moving up and down. The drive assembly is connected to the rotating plate.

Cr-Mn-N austenitic heat-resistant steel and a method for manufacturing the same

A CrMnN austenitic heat-resistant steel is provided. The heat-resistant steel comprises, in weight percentage, carbon 0.20% to 0.50%, silicon 0.50% to 2.00%, manganese 2.00% to 5.00%, phosphorus less than 0.04%, sulphur less than 0.03%, chromium 20.00% to 27.00%, nickel 6.00% to 8.00%, molybdenum less than 0.50%, niobium less than 0.60%, tungsten less than 0.60%, vanadium less than 0.15%, nitrogen 0.30% to 0.60%, zirconium less than 0.10%, cobalt less than 0.10%, yttrium less than 0.10%, boron less than 0.20%, with the balance iron. The heat-resistant steel has high temperature strength, high thermal conductivity, low thermal expansion coefficient, good dimensional stability, good ductility, heat resistance, impact resistance, and low production costs, and meets the requirements for high performance engines.

DROSS REMOVAL DEVICE, DROSS REMOVAL METHOD, DROSS DETECTION DEVICE, AND DROSS DETECTION METHOD

What is provided is a novel and improved dross removal device capable of more efficiently collecting a bath surface dross using a dross robot, and a dross removal method.

In order to solve the problem, according to an aspect of the present invention, there is provided a dross removal device including: a dross robot that is configured to collect a bath surface dross present on a bath surface of a coating bath; a dross sensor that is configured to measure an intensity of infrared light from the bath surface of the coating bath; a dross sensor control device that is configured to specify a position of the bath surface dross according to a temporal change amount in the intensity of the infrared light; and a dross robot control device that is configured to cause the dross robot to collect the bath surface dross at the position specified by the dross sensor control device.

Melting pot, and float salvaging apparatus and method for melting pot

A melting pot includes a pot body and a float salvaging apparatus. The pot body is provided with a melting chamber having an open upper end. The float salvaging apparatus includes a hanging bracket, a bearing plate, a rotating plate and a drive assembly configured to drive pivoting of the rotating plate. The hanging bracket is disposed above the melting chamber. The rotating plate is pivotably disposed on the bearing plate, and the bearing plate and the rotating plate are provided on the hanging bracket between an initial position and a first salvaging position in a manner of moving up and down. The drive assembly is connected to the rotating plate.

Dross removal device, dross removal method, dross detection device, and dross detection method

A dross removal device including: a dross robot that is configured to collect a bath surface dross present on a bath surface of a coating bath; a dross sensor that is configured to measure an intensity of infrared light from the bath surface of the coating bath; a dross sensor control device that is configured to specify a position of the bath surface dross according to a temporal change amount in the intensity of the infrared light; and a dross robot control device that is configured to cause the dross robot to collect the bath surface dross at the position specified by the dross sensor control device.

Cr-Mn-N AUSTENITIC HEAT-RESISTANT STEEL AND A METHOD FOR MANUFACTURING THE SAME

A CrMnN austenitic heat-resistant steel is provided. The heat-resistant steel comprises, in weight percentage, carbon 0.20% to 0.50%, silicon 0.50% to 2.00%, manganese 2.00% to 5.00%, phosphorus less than 0.04%, sulphur less than 0.03%, chromium 20.00% to 27.00%, nickel 6.00% to 8.00%, molybdenum less than 0.50%, niobium less than 0.60%, tungsten less than 0.60%, vanadium less than 0.15%, nitrogen 0.30% to 0.60%, zirconium less than 0.10%, cobalt less than 0.10%, yttrium less than 0.10%, boron less than 0.20%, with the balance iron. The heat-resistant steel has high temperature strength, high thermal conductivity, low thermal expansion coefficient, good dimensional stability, good ductility, heat resistance, impact resistance, and low production costs, and meets the requirements for high performance engines.