Patent classifications
B22F2009/045
IRON NITRIDE POWDER WITH ANISOTROPIC SHAPE
Techniques are disclosed for milling an iron-containing raw material in the presence of a nitrogen source to generate anisotropically shaped particles that include iron nitride and have an aspect ratio of at least 1.4. Techniques for nitridizing an anisotropic particle including iron, and annealing an anisotropic particle including iron nitride to form at least one a″-Fe16N2 phase domain within the anisotropic particle including iron nitride also are disclosed. In addition, techniques for aligning and joining anisotropic particles to form a bulk material including iron nitride, such as a bulk permanent magnet including at least one a″-Fe16N2 phase domain, are described. Milling apparatuses utilizing elongated bars, an electric field, and a magnetic field also are disclosed.
METHOD FOR PRODUCING NANOPARTICLES AND THE NANOPARTICLES PRODUCED THEREFROM
Disclosed herein is a method comprising disposing a container containing a metal and/or ferromagnetic solid and abrasive particles in a static magnetic field; where the container is surrounded by an induction coil; activating the induction coil with an electrical current, to heat up the metallic or ferromagnetic solid to form a fluid; generating sonic energy to produce acoustic cavitation and abrasion between the abrasive particles and the container; and producing nanoparticles that comprise elements from the container, the metal and/or the ferromagnetic solid and the abrasive particles. Disclosed herein too is a composition comprising first metal or a first ceramic; and particles comprising carbides and/or nitrides dispersed therein. Disclosed herein too is a composition comprising nanoparticles comprising chromium carbide, iron carbide, nickel carbide, γ-Fe and magnesium nitride.
METHOD FOR PRODUCING NANOPARTICLES AND THE NANOPARTICLES PRODUCED THEREFROM
Disclosed herein is a method comprising disposing a container containing a metal and/or ferromagnetic solid and abrasive particles in a static magnetic field; where the container is surrounded by an induction coil; activating the induction coil with an electrical current, to heat up the metallic or ferromagnetic solid to form a fluid; generating sonic energy to produce acoustic cavitation and abrasion between the abrasive particles and the container; and producing nanoparticles that comprise elements from the container, the metal and/or the ferromagnetic solid and the abrasive particles. Disclosed herein too is a composition comprising first metal or a first ceramic; and particles comprising carbides and/or nitrides dispersed therein. Disclosed herein too is a composition comprising nanoparticles comprising chromium carbide, iron carbide, nickel carbide, γ-Fe and magnesium nitride.
High frequency low loss magnetic core and method of manufacture
A high saturation, low loss magnetic material suitable for high frequency electrical devices, including power converters, transformers, solenoids, motors, and other such devices.
High frequency low loss magnetic core and method of manufacture
A high saturation, low loss magnetic material suitable for high frequency electrical devices, including power converters, transformers, solenoids, motors, and other such devices.
METHOD FOR PREPARING FUNCTIONAL COMPOSITE POWDER AND FUNCTIONAL COMPOSITE POWDER
The present disclosure relates to a method for preparing a functional composite powder and a functional composite powder, and more particularly, to a method for preparing a functional composite powder, the method including the steps of: preparing a metal material powder and an implantation material; adding the metal material powder and the implantation material into a mixer; and forming a functional composite powder by applying kinetic energy to the metal material powder and the implantation material in the mixer, and a functional composite powder prepared by the method.
Alloy Powders and Methods for Producing the Same
The present invention relates to an alloy with formula of RE-M-B—Fe as defined herein and oxygen content less than 0.9 wt %, wherein said RE is in the range of 29.0 weight % to 33.0 weight %; M is in the range of 0.25 weight % to 1.0 weight %; B is in the range of 0.8 weight % to 1.1 weight %; and Fe makes up the balance. The present invention also relates to a method for preparing a RE-M-Fe—B magnetic powder, as defined herein comprising the steps of: (a) melt spinning a RE-M-Fe—B alloy composition to obtain a melt-spun powder; (b) pressing the melt-spun powder of step (a) to obtain a compact body; (c) hot deforming the compact body of step (b) to obtain a die-upset magnet; (d) crushing the die-upset magnet of step (c) to obtain a powder; (e) milling and sieving the powder of step (d); and (f) passivating the powder of step (e) to obtain a magnetic powder; wherein: each of steps (d) to (f) is performed under a low oxygen environment and transfer between each of steps (d) to (f) is a sealed transfer; and wherein the oxygen content of the low oxygen environment and during each sealed transfer is below 0.5 weight %.
Iron nitride powder with anisotropic shape
Techniques are disclosed for milling an iron-containing raw material in the presence of a nitrogen source to generate anisotropically shaped particles that include iron nitride and have an aspect ratio of at least 1.4. Techniques for nitridizing an anisotropic particle including iron, and annealing an anisotropic particle including iron nitride to form at least one α″-Fe.sub.16N.sub.2 phase domain within the anisotropic particle including iron nitride also are disclosed. In addition, techniques for aligning and joining anisotropic particles to form a bulk material including iron nitride, such as a bulk permanent magnet including at least one α″-Fe.sub.16N.sub.2 phase domain, are described. Milling apparatuses utilizing elongated bars, an electric field, and a magnetic field also are disclosed.
Apparatus and method for forming nanoparticles
Certain aspects of the technology disclosed herein include an apparatus and method for forming nanoparticles. The method includes a mechanical milling process induced by aerodynamic, centrifugal, and centripetal forces and further augmented by ultrasound, magnetic pulse, and high voltage impact. A nanoparticle mill having an atmospheric and luminance controlled environment can form precisely calibrated nanoparticles. A nanoparticle mill can include first aerodynamic vane configured to rotate around a central axis of the nanoparticle mill in a first direction, and a second aerodynamic vane configured to rotate around the central axis in a second direction. An aerodynamic shape of an aerodynamic vane can be configured to cause particles within the nanoparticle mill to flow around the aerodynamic vane. The nanoparticle mill can include a primary product line, a nanoparticle sampling line, a particle programming array, a solidifying chamber, or any combination thereof.
Apparatus and method for forming nanoparticles
Certain aspects of the technology disclosed herein include an apparatus and method for forming nanoparticles. The method includes a mechanical milling process induced by aerodynamic, centrifugal, and centripetal forces and further augmented by ultrasound, magnetic pulse, and high voltage impact. A nanoparticle mill having an atmospheric and luminance controlled environment can form precisely calibrated nanoparticles. A nanoparticle mill can include first aerodynamic vane configured to rotate around a central axis of the nanoparticle mill in a first direction, and a second aerodynamic vane configured to rotate around the central axis in a second direction. An aerodynamic shape of an aerodynamic vane can be configured to cause particles within the nanoparticle mill to flow around the aerodynamic vane. The nanoparticle mill can include a primary product line, a nanoparticle sampling line, a particle programming array, a solidifying chamber, or any combination thereof.