Patent classifications
B22F9/082
COMPOSITE MATERIAL
According to an aspect of the present disclosure, a composite material includes: a primary phase which is an alloy including a metallic element M and a nonmetallic element X and of which at least a portion is an amorphous phase; and a secondary phase which is dispersed in the primary phase and includes a ceramic compound including the metallic element M and the nonmetallic element X and represented by M.sub.aX.sub.b (wherein a and b are each greater than 0).
Metal refinement
A method, and systems in which such method may be practiced, allow for the separation of elemental metals from metal alloy. A metal alloy is atomized to form metal alloy particulates. The metal alloy particulates are exposed to an oxidizing agent, such as chlorine gas in the presence of a salt, such as NaCl, an acid, such as HCl, and water. The resulting solution may be filtered to remove particulates, reduced, filtered, reduced, filtered, and so on. In aspects, the method is used to refine gold alloy by oxidation of elemental sponge gold to gold chloride followed by reduction to pure elemental gold.
Metal refinement
A method, and systems in which such method may be practiced, allow for the separation of elemental metals from metal alloy. A metal alloy is atomized to form metal alloy particulates. The metal alloy particulates are exposed to an oxidizing agent, such as chlorine gas in the presence of a salt, such as NaCl, an acid, such as HCl, and water. The resulting solution may be filtered to remove particulates, reduced, filtered, reduced, filtered, and so on. In aspects, the method is used to refine gold alloy by oxidation of elemental sponge gold to gold chloride followed by reduction to pure elemental gold.
HARD PARTICLE POWDER FOR SINTERED BODY
The present invention relates to a hard particle powder for a sintered body, the powder including, in terms of mass %, 0.01≤C≤1.0, 2.5≤Si≤3.3, 0.1≤Ni≤20.0, 5.0≤Cr≤15.0, and 35.0≤Mo≤45.0, with the balance being Fe and inevitable impurities, in which the powder before performing sintering comprises an alloy phase comprising a hexagonal crystal structure of C14 type Laves phase.
Article for producing ultra-fine powders and method of manufacture thereof
A multistage centrifugal atomizer comprises an outer shell that contains an inlet port and an outlet port and that encloses a tundish, a first inclined rotating surface and a second inclined rotating surface. The first inclined rotating surface is opposedly disposed to the second inclined rotating surface. The inlet is used to introduce a molten material into the multistage atomizer and the outlet is used to remove ultrafine particles having a D50 of less than 20 micrometers.
Metal powder for additive manufacturing
A metal powder having a composition including the following elements, expressed in content by weight: 6.5%≤Si≤10%, 4.5%≤Nb≤10%, 0.2%≤B≤2.0%, 0.2%≤Cu≤2.0%, C≤2% and optionally containing Ni≤10 wt % and/or Co≤10 wt % and/or Cr≤7 wt % and/or Zr as a substitute for any part of Nb on a one-to-one basis and/or Mo as a substitute for any part of Nb on a one-to-one basis and/or P as a substitute for any part of Si on a one-to-one basis, the balance being Fe and unavoidable impurities resulting from the elaboration, the metal powder having a microstructure including at least 5% in area fraction of an amorphous phase, the balance being made of crystalline ferritic phases with a grain size below 20 μm and possible precipitates, the metal powder having a mean sphericity SPHT of at least 0.80.
APPARATUS FOR MANUFACTURING METAL POWDER
An apparatus for manufacturing metal powder according to the present invention is a metal powder manufacturing apparatus, in which molten metal is broken up, and liquid droplets of the atomized molten metal are cooled by spraying cooling water using a cooling water spraying nozzle provided inside a chamber. The cooling water spraying nozzle is provided such that cooling water is sprayed in a fan shape, and cooling water spraying nozzles provided at different heights have increasing angles of inclination with respect to the inner wall of the chamber as the heights thereof are reduced, thereby decreasing a deviation between flying distances of the molten metal liquid droplets to efficiently manufacture metal powder having uniform properties.
APPARATUS FOR MANUFACTURING METAL POWDER
An apparatus for manufacturing metal powder according to the present invention is a metal powder manufacturing apparatus, in which molten metal is broken up, and liquid droplets of the atomized molten metal are cooled by spraying cooling water using a cooling water spraying nozzle provided inside a chamber. The cooling water spraying nozzle is provided such that cooling water is sprayed in a fan shape, and cooling water spraying nozzles provided at different heights have increasing angles of inclination with respect to the inner wall of the chamber as the heights thereof are reduced, thereby decreasing a deviation between flying distances of the molten metal liquid droplets to efficiently manufacture metal powder having uniform properties.
APPARATUS, COMPOSITIONS, AND METHODS FOR STAINLESS-COATED STEEL REINFORCEMENT BAR
In some embodiments, a coating applied to steel reinforcement bar (e.g., steel rebar) that could considerably extend the lifetime of concrete structures by reducing steel rebar corrosion is disclosed. The coating includes a thin, passivating steel (e.g., stainless steel) layer that is applied to the outside of conventional steel rebar. The coating can be applied in-line through metal cold spray manufacturing, which is a high throughput coating technique that can be integrated into existing steel manufacturing plants. Furthermore, a novel, high performance ferritic steel with tailored resistance to corrosion from chlorides is described. The new ferritic steel is distinct from other commercial and experimental steels, and is better suited for coating low-cost steel structures like rebar. Multiple alloying elements including Cr, Al, and Si will each form protective oxides independently, increasing the total amount of protection and extending it over much wider ranges of pH and electrical potential.
APPARATUS, COMPOSITIONS, AND METHODS FOR STAINLESS-COATED STEEL REINFORCEMENT BAR
In some embodiments, a coating applied to steel reinforcement bar (e.g., steel rebar) that could considerably extend the lifetime of concrete structures by reducing steel rebar corrosion is disclosed. The coating includes a thin, passivating steel (e.g., stainless steel) layer that is applied to the outside of conventional steel rebar. The coating can be applied in-line through metal cold spray manufacturing, which is a high throughput coating technique that can be integrated into existing steel manufacturing plants. Furthermore, a novel, high performance ferritic steel with tailored resistance to corrosion from chlorides is described. The new ferritic steel is distinct from other commercial and experimental steels, and is better suited for coating low-cost steel structures like rebar. Multiple alloying elements including Cr, Al, and Si will each form protective oxides independently, increasing the total amount of protection and extending it over much wider ranges of pH and electrical potential.