B27K2240/50

Method for the modification of wood

Disclosed is a method for the continuous impregnation of wood elements, such as wood chips. The method comprises the subsequent steps of subjecting the wood elements to vacuum, to contact with acetylation fluid, and to impregnation pressure. Preferably, the process is conducted in a plant having conveyors, such as transportation screws, in suitable positions between the zones in which the subsequent process steps are conducted. The impregnation method is used in connection with the acetylation of the wood elements, and preferably is followed by a continuous acetylation process conducted in an acetylation reaction zone downstream of the zone where the impregnation is conducted.

A WOOD PRESERVATIVE COMPOSITION COMPRISING 4,5-DICHLORO-2-OCTYLISOTHIAZOL-3(2H)-ONE, A METHOD TREATING A WOOD SUBSTRATE THEREWITH, AND A WOOD PRODUCT PRODUCED THEREFROM
20240342946 · 2024-10-17 ·

A wood preservative composition comprising 4,5-dichloro-2-octylisothiazol-3(2H)-one, a method of treating a wood substrate therewith, and a wood product produced therefrom are provided. The wood preservative composition comprises at least 0.5% by weight of DCOI based on the total weight of the composition and a retaining additive comprising a solvent-borne polymeric resin, a wax, or a combination thereof. A weight ratio of the DCOI to the retaining additive in the composition is in a range of 1:5 to 5:1.

A WOOD PRESERVATIVE COMPOSITION COMPRISING 4,5-DICHLORO-2-OCTYLISOTHIAZOL-3(2H)-ONE, A METHOD TREATING A WOOD SUBSTRATE THEREWITH, AND A WOOD PRODUCT PRODUCED THEREFROM
20240342947 · 2024-10-17 ·

A wood preservative composition comprising 4.5-dichloro-2-octylisothiazol-3 (2H)-one, a method of treating a wood substrate therewith, and a wood product produced therefrom are provided. The wood preservative composition comprises at least 10% by weight of 4.5-dichloro-2-octylisothiazol-3-one (DCOI) based on the total weight of the composition, at least 10% by weight of a non-polar organic solvent based on the total weight of the composition, and at least 1% by weight of a polar organic solvent based on the total weight of the composition. A weight ratio of the non-polar organic solvent to the polar organic solvent is in a range of 80:1 to 1:8.

METHOD FOR THE MODIFICATION OF WOOD

Disclosed is a method for the continuous impregnation of wood elements, such as wood chips. The method comprises the subsequent steps of subjecting the wood elements to vacuum, to contact with acetylation fluid, and to impregnation pressure. Preferably, the process is conducted in a plant having conveyors, such as transportation screws, in suitable positions between the zones in which the subsequent process steps are conducted. The impregnation method is used in connection with the acetylation of the wood elements, and preferably is followed by a continuous acetylation process conducted in an acetylation reaction zone downstream of the zone where the impregnation is conducted.

WOOD PRESERVATIVE COMPOSITION COMPRISING 4,5-DICHLORO-2-OCTYLISOTHIAZOL-3(2H)-ONE, A METHOD TREATING A WOOD SUBSTRATE THEREWITH, AND A WOOD PRODUCT PRODUCED THEREFROM
20250196393 · 2025-06-19 ·

A wood preservative composition comprising 4,5-dichloro-2-octylisothiazol-3(2H)-one, a method of treating a wood substrate therewith, and a wood product produced therefrom are provided. The wood preservative composition comprises at least 0.5% by weight of DCOI based on the total weight of the composition and a retaining additive comprising a solvent-borne polymeric resin, a wax, or a combination thereof. A weight ratio of the DCOI to the retaining additive in the composition is in a range of 1:5 to 5:1.

Wood preservative composition comprising 4,5-dichloro-2-octylisothiazol-3(2H)-one, a method treating a wood substrate therewith, and a wood product produced therefrom

A wood preservative composition comprising 4,5-dichloro-2-octylisothiazol-3(2H)-one, a method of treating a wood substrate therewith, and a wood product produced therefrom are provided. The wood preservative composition comprises at least 0.5% by weight of DCOI based on the total weight of the composition and a retaining additive comprising a solvent-borne polymeric resin, a wax, or a combination thereof. A weight ratio of the DCOI to the retaining additive in the composition is in a range of 1:5 to 5:1.

Wood preservative composition comprising 4,5-dichloro-2-octylisothiazol-3(2H)-one, a method treating a wood substrate therewith, and a wood product produced therefrom

A wood preservative composition comprising 4,5-dichloro-2-octylisothiazol-3(2H)-one, a method of treating a wood substrate therewith, and a wood product produced therefrom are provided. The wood preservative composition comprises at least 0.5% by weight of DCOI based on the total weight of the composition and a retaining additive comprising a solvent-borne polymeric resin, N a wax, or a combination thereof. A weight ratio of the DCOI to the retaining additive in the composition is in a range of 1:5 to 5:1.

WOOD PRESERVATIVE COMPOSITION COMPRISING 4,5-DICHLORO-2-OCTYLISOTHIAZOL-3(2H)-ONE, A METHOD TREATING A WOOD SUBSTRATE THEREWITH, AND A WOOD PRODUCT PRODUCED THEREFROM
20250375917 · 2025-12-11 ·

A wood preservative composition comprising 4,5-dichloro-2-octylisothiazol-3 (2H)-one, a method of treating a wood substrate therewith, and a wood product produced therefrom are provided. The wood preservative composition comprises at least 0.5% by weight of DCOI based on the total weight of the composition and a retaining additive comprising a solvent-borne polymeric resin, a wax, or a combination thereof. A weight ratio of the DCOI to the retaining additive in the composition is in a range of 1:5 to 5:1.

WOOD PRESERVATIVE COMPOSITION COMPRISING 4,5-DICHLORO-2-OCTYLISOTHIAZOL-3(2H)-ONE, A METHOD TREATING A WOOD SUBSTRATE THEREWITH, AND A WOOD PRODUCT PRODUCED THEREFROM
20260070256 · 2026-03-12 ·

A wood preservative composition comprising 4,5-dichloro-2-octylisothiazol-3(2H)-one, a method of treating a wood substrate therewith, and a wood product produced therefrom are provided. The wood preservative composition comprises at least 0.5% by weight of DCOI based on the total weight of the composition and a retaining additive comprising a solvent-borne polymeric resin, a wax, or a combination thereof. A weight ratio of the DCOI to the retaining additive in the composition is in a range of 1:5 to 5:1.

SELF-FLOWING TREATMENT OF WOOD, BAMBOO, AND OTHER POROUS MATERIALS
20260070255 · 2026-03-12 · ·

Methods and systems for self-flowing treatment of wood, bamboo or other porous materials do not require external pressure or complicated equipment. Treatment liquid flows through these porous materials through use of capillary action, the use of absorbent sheets, and differences in pressure. The treatment solution is more evenly dispersed throughout the materials.