B27K3/0242

PARAFFIN-REINFORCED WOOD AND METHOD FOR MANUFACTURING THE SAME
20210260788 · 2021-08-26 ·

The present invention provides a paraffin-reinforced wood and a method for manufacturing the same, and more specifically, a paraffin-reinforced wood in which a natural wood is vacuum impregnated with dissolved paraffin and processed, thereby preventing a penetration of moisture into the wood and increasing durability and corrosion resistance of the wood, such that the reinforced wood is very useful as various deck-wood, agricultural wood posts, water wood posts, etc., and a method and apparatus for manufacturing the same.

Method for impregnation of wood component with solid paraffin wax, apparatus therefor and wood component so impregnated
10926285 · 2021-02-23 · ·

A method for treating a piece of wood impregnates the piece of wood with a water repellent, wherein the water repellent is solid at ambient temperatures. The method includes the steps of providing a piece of wood to be treated; heating the piece of wood for a predetermined period of time, the piece of wood being heated at a temperature A; subsequently immersing at least a portion of the piece of wood in a bath of liquefied water repellent, the bath being at a temperature B, for a predetermined period of time. Thereafter the piece of wood is removed from the bath and allowed to cool. The temperature A is above 100 C. and the temperature B is below 100 C. but above a liquefying point for the water repellent, and a differential between temperatures A and B is at least 60 C.

WOOD TREATMENT COMPOSITIONS HAVING ANTIMICROBIAL PROPERTIES
20240033966 · 2024-02-01 ·

The present application relates to wood treatment. More specifically, the present application relates to wood treatment compositions having antimicrobial properties, methods using the same and wood products treated therewith. The present application includes a wood treatment composition comprising: an antimicrobial additive comprising at least one tannin; and a water-based solvent. The present application also includes a method for treating a wood product to stop or prevent microbial growth applying a wood treatment composition on the wood product, and optionally applying a wax; wherein applying the wood treatment composition comprises heating at least one surface of the wood product and impregnating the composition.

METHOD FOR IMPREGNATION OF WOOD COMPONENT WITH SOLID PARAFFIN WAX, APPARATUS THEREFOR AND WOOD COMPONENT SO IMPREGNATED
20170246653 · 2017-08-31 · ·

A method for treating a piece of wood impregnates the piece of wood with a water repellent, wherein the water repellent is solid at ambient temperatures. The method includes the steps of providing a piece of wood to be treated; heating the piece of wood for a predetermined period of time, the piece of wood being heated at a temperature A; subsequently immersing at least a portion of the piece of wood in a bath of liquefied water repellent, the bath being at a temperature B, for a predetermined period of time. Thereafter the piece of wood is removed from the bath and allowed to cool. The temperature A is above 100 C. and the temperature B is below 100 C. but above a liquefying point for the water repellent, and a differential between temperatures A and B is at least 60 C.

Method for impregnation of wood component with solid paraffin wax, apparatus therefor and wood component so impregnated
09682493 · 2017-06-20 · ·

A method for treating a piece of wood impregnates the piece of wood with a water repellent, wherein the water repellent is solid at ambient temperatures. The method includes the steps of providing a piece of wood to be treated; heating the piece of wood for a predetermined period of time, the piece of wood being heated at a temperature A; subsequently immersing at least a portion of the piece of wood in a bath of liquefied water repellent, the bath being at a temperature B, for a predetermined period of time. Thereafter the piece of wood is removed from the bath and allowed to cool. The temperature A is above 100 C. and the temperature B is below 100 C. but above a liquefying point for the water repellent, and a differential between temperatures A and B is at least 60 C.