B27K5/0055

TREATMENT OF WOOD
20180009126 · 2018-01-11 ·

The present invention relates methods for heat treatment of wood. The invention further relates to wood obtainable by the methods of the invention as well as the use of the method for preparing treated wood. The method comprises the step of pressurising said airtight tank (4) to a predefined pressure (P.sub.1) in order to establish a pressurised environment for said wood (6). The method comprises the step of placing said wood (6) in an airtight tank (4) and heating said wood (6) to a predefined temperature (T.sub.2, T.sub.3). The predefined pressure (P.sub.1) is kept so high that the water in the wood (6) cannot evaporate at the predefined temperature (T.sub.2, T.sub.3).

RADIOFREQUENCY HEATING OF WOOD USING A THREE-ELECTRODE SYSTEM HAVING A WINGED CENTRAL ELECTRODE

Wood kilns, electrode systems for wood kilns, and methods of using the systems for the radiofrequency (RF) drying and phytosanitizing of wood are provided. The electrode systems are based on a three-electrode design in which a central plate electrode having winged edges is disposed between a pair of ground plate electrodes. The winged edges of the central electrode improve the uniformity of heating during the phytosanitizing process, relative to a five-electrode parallel plate system, or a three-electrode parallel plate system having a conventional planar central plate electrode.

Method and system for a continuous wood modification heat process
11679526 · 2023-06-20 ·

A continuous wood modification by heat process, that comprises: stacking wooden boards on a trolley at intervals; exerting pressure on said wooden boards; transferring said wooden boards to a heating kiln, pre-heated by microwave and hot air circulation, that has a water vapor flow of 2-5 meter3/hour, a temperature range of 60-100° C., and a humidity range of 50%-100%; transferring said wooden boards to a shallow drying kiln, pre-heated by microwave and hot air circulation, that has a drying temperature of 100-120° C.; transferring said wooden boards to a deep drying kiln, pre-heated by microwave and hot air circulation, that has a drying temperature of 120-120° C., an oxygen content range of 1-10%, and a water vapor flow rate of 1-10 m3/hour; transferring said wooden boards to a carbonization kiln, pre-heated by microwave and hot air circulation, that has a temperature range of 120-180° C., an oxygen content range of 1%-5%; transferring said wooden boards to a slow cooling kiln, that has a temperature range of 120-130° C., and an oxygen content range of 1%-10%; transferring said wooden boards to a fast cooling kiln, that has a temperature range of 90-100° C.; transferring said wooden boards to a rewetting kiln, that has a humidity range of 50%-100%; providing water vapor to said rewetting kiln; while being in said rewetting kiln, and when a temperature range of said wooden boards is 40-60° C., and a moisture content of said wooden boards is 6%-10%, transferring said wooden boards out of said rewetting kiln; wherein each of said heating kiln, said shallow drying kiln, said deep drying kiln, said carbonization kiln, said slow cooling kiln, said fast cooling kiln, and said rewetting kiln comprises a fan, a partition board, a shunt hood, and an exhaust port; wherein said partition board divides an interior of each of said heating kiln, said shallow drying kiln, said deep drying kiln, said carbonization kiln, said slow cooling kiln, said fast cooling kiln, and said rewetting kiln into an upper chamber and a lower chamber; wherein said shunt hood is disposed in said upper chamber; wherein said fan, said shunt hood, and said lower chamber are connected and form a air channel; wherein said lower chamber comprises a shunt plate, disposed along left and right walls of a kiln; wherein said shunting plate comprises a plurality of sieve holes that are disposed gradually dense from top to bottom; wherein one end of said shunt plate is connected with said partition board and the other end is connected with the bottom of a kiln.

WOOD PRESERVATIVE AND METHOD FOR PRODUCING SAME
20220000115 · 2022-01-06 ·

A synergistic aqueous wood preservative composition comprising a copper compound and penflufen. The copper compounds of the compositions of the invention may be soluble, partially solubilized or micronized particles. The penflufen of the compositions of the invention may be solubilized, emulsified or particulate. The wood preservative compositions of the present invention are surprisingly provided as stable dispersions and confer surprising and unexpected resistance to treated wood and wood products.

RADIO FREQUENCY TREATMENT TO PHYTOSANITIZE WOOD PACKAGING MATERIALS USED IN INTERNATIONAL SHIPPING

A method for treating wood packaging materials using Radio Frequency heating includes the steps of heating wood packaging materials using RF heating and applying a pressure before the heating or incrementally applying a pressure during the heating. The wood packaging materials are heated in a RF operating unit that has a sealed chamber with an inner surface and a liner cover a majority of the inner surface, the liner having a heat-reflective inner face and an insulation layer between the inner face and the inner surface.

Wood preservative and method for producing same

A synergistic aqueous wood preservative composition comprising a copper compound and penflufen. The copper compounds of the compositions of the invention may be soluble, partially solubilized or micronized particles. The penflufen of the compositions of the invention may be solubilized, emulsified or particulate. The wood preservative compositions of the present invention are surprisingly provided as stable dispersions and confer surprising and unexpected resistance to treated wood and wood products.

Ethanol-Based Extraction of Soluble Wood Components
20210245392 · 2021-08-12 · ·

A method (10) for ethanol-based extraction of soluble wood components. Wood is prepared (12), and chipped (18) to provide wood chips. The wood chips and a liquid are mixed (20) in a container to provide a mixture. After waiting (22) for a specified time, RF energy is applied (26) to the mixture while controlling (28) at least one an RF power level, a temperature of the mixture, a time of application of the RF energy, or a speed of a pump which is circulating the liquid in the mixture. The mixture is then cooled (30), the liquid and the components are removed (32) from the container, and are filtered (36) to provide a filtered extract. The wood may be heated (14) such as by charring and/or toasting before being chipped. Oxygen may be added (34) to the liquid and the components removed from the container before being filtered.

Method and System for a Continuous Wood Modification Heat Process
20210154884 · 2021-05-27 ·

A continuous wood modification by heat process, that comprises: stacking wooden boards on a trolley at intervals; exerting pressure on said wooden boards; transferring said wooden boards to a heating kiln, pre-heated by microwave and hot air circulation, that has a water vapor flow of 2-5 meter3/hour, a temperature range of 60-100° C., and a humidity range of 50%-100%; transferring said wooden boards to a shallow drying kiln, pre-heated by microwave and hot air circulation, that has a drying temperature of 100-120° C.; transferring said wooden boards to a deep drying kiln, pre-heated by microwave and hot air circulation, that has a drying temperature of 120-120° C., an oxygen content range of 1-10%, and a water vapor flow rate of 1-10 m3/hour; transferring said wooden boards to a carbonization kiln, pre-heated by microwave and hot air circulation, that has a temperature range of 120-180° C., an oxygen content range of 1%-5%; transferring said wooden boards to a slow cooling kiln, that has a temperature range of 120-130° C., and an oxygen content range of 1%-10%; transferring said wooden boards to a fast cooling kiln, that has a temperature range of 90-100° C.; transferring said wooden boards to a rewetting kiln, that has a humidity range of 50%-100%; providing water vapor to said rewetting kiln; while being in said rewetting kiln, and when a temperature range of said wooden boards is 40-60° C., and a moisture content of said wooden boards is 6%-10%, transferring said wooden boards out of said rewetting kiln; wherein each of said heating kiln, said shallow drying kiln, said deep drying kiln, said carbonization kiln, said slow cooling kiln, said fast cooling kiln, and said rewetting kiln comprises a fan, a partition board, a shunt hood, and an exhaust port; wherein said partition board divides an interior of each of said heating kiln, said shallow drying kiln, said deep drying kiln, said carbonization kiln, said slow cooling kiln, said fast cooling kiln, and said rewetting kiln into an upper chamber and a lower chamber; wherein said shunt hood is disposed in said upper chamber; wherein said fan, said shunt hood, and said lower chamber are connected and form a air channel; wherein said lower chamber comprises a shunt plate, disposed along left and right walls of a kiln; wherein said shunting plate comprises a plurality of sieve holes that are disposed gradually dense from top to bottom; wherein one end of said shunt plate is connected with said partition board and the other end is connected with the bottom of a kiln.

DISINFECTION SYSTEM FOR WOOD BARRELS
20210121589 · 2021-04-29 ·

Different aspects of the invention refer to a disinfection apparatus, and corresponding method, for wood barrel disinfection using microwave shock pulse, MwSP, technology for the complete elimination of microbial populations. This is accomplished by a system which ensures deep and complete disinfection, however such that the temperature is maintained below material degradation level. Complete disinfection is achieved due to effectiveness up to the deepest layers. The wooden barrel material is however preserved, due to the non-harmful nature of the dosage regime programmed into the radio frequency emission.

METHOD FOR DRYING WOOD USING MICROWAVE
20210080178 · 2021-03-18 · ·

The present invention relates to a method for drying wood by using microwaves. The method for drying wood by using microwaves, according to an embodiment of the present invention, comprises the steps of: preparing wood; wrapping at least a portion of the wood by using a wrapping member; applying microwaves to the wood wrapped with the wrapping member to raise the temperature inside the wrapping member; removing the wrapping member from the wood wrapped with the wrapping member; and drying moisture of an outer layer of the wood from which the wrapping member has been removed.