A method for finishing a glass or ceramic article includes applying a force to the glass or ceramic article. The force is applied to the glass or ceramic article at least when the glass or ceramic article is at a temperature that is greater than or equal to a creep temperature of the glass or ceramic article. Holding the force to the glass or ceramic article as the glass or ceramic article is cooled to a temperature that is less than the creep temperature of the glass or ceramic article.

HIGH TOUGHNESS INORGANIC COMPOSITE ARTIFICIAL STONE PANEL AND PREPARATION METHOD THEREOF

A high toughness inorganic composite artificial stone panel and preparation method are disclosed. The panel includes a surface layer, an intermediate metal fiber toughening layer and a substrate toughening layer. The surface layer includes the following components: 40-70 parts of quartz sand, 10-30 parts of quartz powder, 20-45 parts of inorganic active powder, 0.5-4 parts of pigment, 0.3-1 part of water reducer and 3-10 parts of water. The intermediate metal fiber toughening layer includes the following components: 40-60 parts of inorganic active powder, 45-65 parts of sand, 0.8-1.5 parts of water reducer, 6-14 parts of water and 4-8 parts of metal fiber. The substrate toughening layer includes the following components: 30-50 parts of inorganic active powder, 30-55 parts of quartz sand, 15-20 parts of quartz powder, 0.5-1.2 parts of water reducer, 4-8 parts of water and 0.8-2.5 parts of toughening agent.

Inorganic fiber toughened inorganic composite artificial stone panel and preparation method thereof
20210017080 · 2021-01-21 ·

An inorganic fiber toughened inorganic composite artificial stone panel and a preparation method thereof are disclosed. The panel includes a surface layer and a toughened base layer. The surface layer includes the the following components in parts by weight: 40-70 parts of quartz sand, 10-30 parts of quartz powder, 20-45 parts of inorganic active powder, 0.5-4 parts of pigment, 0.3-1 parts of water reducing agent and 3-10 parts of water. The toughened base layer includes the following components in parts by weight: 40-60 parts of inorganic active powder, 45-65 parts of sand, 0.8-1.5 parts of water reducing agent, 6-14 parts of water, 0.4-2 parts of inorganic fiber and 0.8-2.5 parts of toughener.

METHOD FOR PRODUCING A COMPOSITE PART CONTAINING A CERAMIC MATRIX
20200377417 · 2020-12-03 ·

A process for manufacturing a composite material part including a particulate reinforcement densified by a ceramic matrix, the process including: formation of a blank of the part to be manufactured by shaping a mixture including a binder, first ceramic or carbon particles intended to form the particulate reinforcement of the part and second ceramic or carbon particles distinct from the first particles, removal or pyrolysis of the binder present in the blank to obtain a porous preform of the part to be manufactured, and infiltration of the porosity of the preform by a molten composition including a metal in order to obtain the part.

INJECTION MOLDING APPARATUS AND INJECTION MOLDING METHOD

An injection molding apparatus including a mold, an injection device and a gas supply device is provided. The injection device is adapted to inject a ceramic powder material into the mold. The gas supply device is adapted to provide a gas into the mold to form a cavity in the ceramic powder material by the gas. In addition, an injection molding method is also provided.

INJECTION MOLDING APPARATUS AND INJECTION MOLDING METHOD

An injection molding apparatus including a ceramic powder material injection device, a mold, and a gas providing device is provided. The ceramic powder material injection device is adapted to contain a ceramic powder material. The mold has a molding concavity, wherein the ceramic powder material injection device is adapted to inject at least the ceramic powder material into the molding concavity. The gas providing device is adapted to provide a gas into the molding concavity to increase a pressure in the molding concavity to increase a density of the ceramic powder material in the molding concavity. In addition, an injection molding method is also provided.

Ceramic wafer and the manufacturing method thereof

A method of producing ceramic wafer includes a forming step and processing step. The processing step includes forming positioning notch or positioning, flat edge and edge profile, which avoids the ceramic wafers to have processing defect during cutting, grinding, and polishing, for increasing yield. The ceramic particles for producing ceramic wafer include nitride ceramic powder, oxide ceramic powder, and nitride ceramic powder. The ceramic wafer has low dielectric constant, insulation, and excellent heat dissipation, which can be applied for the need of semiconductor process, producing electric product and semiconductor equipment.

Systems and methods for infusion mixing a slurry-based electrode

Embodiments described in this application relate generally to a system, an apparatus and/or methods for manufacturing electrodes by infusion electrolyte into compacted electrode materials. In some embodiments, a working electrode materials can be produced using an infusion mixing and manufacturing process. In some embodiments, a single-sided finished electrode can be produced directly from a dry powder mixture using an infusion mixing and manufacturing process. In some embodiments, a double-sided finished electrode can be produced directly from a dry powder mixture using an infusion mixing and manufacturing process. The electrodes produced by an infusion mixing and manufacturing process generally perform better than those produced by non-infusion processes.

Method for manufacturing part made of composite material

A method of fabricating a part out of composite material, includes forming a fiber texture from refractory fibers; impregnating the fiber texture for a first time with a first slip containing first refractory particles; eliminating the liquid phase from the first slip so as to leave within the texture only the first refractory particles; impregnating the fiber texture for a second time with a second slip containing second refractory particles; eliminating the liquid phase from the second slip so as to leave within the texture only the second refractory particles and obtain a fiber preform filled with the first and second refractory particles; and sintering the first and second refractory particles present in the fiber preform in order to form a refractory matrix in the preform.

METHOD OF USING PERMEABLE MEMBRANE IN THE DEBULKING OF CMC PREPREG MATERIAL
20240158306 · 2024-05-16 ·

A method used for forming ceramic matrix composite components includes several steps. The method comprises arranging a layup of a predetermined number of pre-impregnated ceramic plies on a layup too and a plurality of different stages to debulk and consolidate the layup.