20230001626 · 2023-01-05 ·

The invention is characterized by a semifinished composite structure product with the at least two layers, of which the at least one layer, in which the continuous fibers are contained, is heated such that the matrix of thermoplastic material is heated within at least one first surface region to or above a melting temperature that can be assigned to the thermoplastic material, and the matrix of thermoplastic material is kept to a temperature below the melting temperature within a second surface region directly adjoining the first surface region. The semifinished composite structure product is heated in this way so that the moldable thermoplastic, continuous fiber-reinforced composite structure in which the continuous fibers within the first surface region are movable relative to each other and those within the second surface region are spatially fixed relative to each other.

Article and methods of making the same

Article (9,19) comprising a substrate (10, 20) comprising a polymer and having first (11,21) and second (12, 22) opposed major surfaces. The first major surface (11, 21) has first surface regions (13, 23) with first nanoparticles (14a, 14b, 14c, 14d, 24a, 24b, 24c, 24d) partially embedded into the first major surface (11, 21), and one of •(a) second surface regions (15) free of nanoparticles; or •(b) second surface regions (25) with at least second nanoparticles (28) on the first major surface (11, 21) or partially embedded into the first major surface (11, 21). The first surface regions (13, 23) have a first average surface roughness, R.sub.a1, of at least 20 nm, wherein the second surface regions (15, 25) have a second average surface roughness, R.sub.a2, of less than 100 nm, wherein the first average surface roughness, R.sub.a1, is greater than the second average surface roughness, R.sub.a2, and wherein there is an absolute difference between the first and second average surface roughness of at least 10 nm.

Electrophoretic device, electrophoretic display apparatus, electronic apparatus, and method of manufacturing electrophoretic device
09851614 · 2017-12-26 · ·

An electrophoretic device includes a fiber layer, an electrophoretic particle configured to migrate through a gap in the fiber layer, and a partition wall extended in a thickness direction of the fiber layer to separate the fiber layer into a plurality of migration cells. The partition wall includes a cured body of a curable resin, and the cured body includes a constriction part between both end portions of the fiber layer in the thickness direction.

UV CURABLE LATTICE MICROSTRUCTURE FOR FOOTWEAR
20170360156 · 2017-12-21 ·

An upper for a sports shoe may include a component such as a vamp or a rear portion. The shoe component may include a UV curable microlattice structure with a plurality of regions such that each region has a different density. In some cases, the microlattice structure may include a high density microlattice structure, a mid-level density microlattice structure, and a non-structural region with a low density microlattice structure.

Method and apparatus for generating a superficial structure
11673364 · 2023-06-13 ·

A method and related apparatus for producing an embossing on a substrate using a digital printing technology includes the application of an embossing liquid, for example a water-based liquid, on a non-polymerized resin layer and the subsequent polymerization of the resin with UV curing.

Rigid mask for protecting selective portions of a chip, and use of the rigid mask

A rigid mask protects selective portions of a chip including a plurality of wells for biochemical reactions. The rigid mask includes a supporting portion and a plurality of legs, where each leg is provided with a rigid stem and a plate. The plurality of legs are arranged and fixed with respect to the supporting portion in a way aligned to the spatial arrangement of the wells, and are configured in such a way that, when each leg is inserted into the corresponding well, the respective plate covers at least in part the bottom of the well, protecting it during a chemical/physical treatment of side walls of the wells.

Method for producing patterned materials

A large area patterned film includes a first patterned area; a second patterned area; and a seam joining the first patterned area and the second patterned area, wherein the seam has a width less than about 20 micrometers. A method for tiling patterned areas includes depositing a predetermined thickness of a curable material; contacting a first portion of the curable material with a mold; curing the first portion of the curable material; removing the mold from the cured first portion of the curable material; contacting a second portion of the curable material with the mold, such that the mold contacts a portion of the cured first portion of the curable material; curing the second portion of the curable material; and removing the mold to yield a seam between the cured first portion of the curable material and the cured second portion of the curable material, wherein the seam has a dimension less than about 20 micrometers.

Multi-chemistry microlattice structures and methods of manufacturing the same

A multi-chemistry structure includes: a plurality of interconnected polymer struts arranged in a lattice; a first layer of the lattice including a first array of first unit cells; a second layer of the lattice including a second array of second unit cells; at least one region of the lattice being formed of a first polymer; and at least one region of the lattice being formed of a second polymer different from the first polymer.

Method of manufacturing an artificial elastic implant for restorative an reconstructive surgery

A method for manufacturing an artificial elastic implant for restorative and reconstructive surgery includes two casting steps performed in a casting mold. The mold has at least a cover that is optically and UV transparent. In a first step, a first layer of a first photo-curable material or of a second photo-curable material is cast while forming a meniscus. Using one of two photo masks, the mold is irradiated with UV light to cure the first layer. In a second step, a second layer of either the first or the second photo-curable material is cast onto the cured first layer while forming a meniscus. After irradiating the mold again with ultraviolet light, unhardened photo-curable material is removed from the product by dissolving in a suitable solvent. After additionally irradiating the product with UV light, the product is soaked, separated from the mold, placed in isopropyl alcohol and then vacuum dried.

METHOD FOR PRODUCING SHOE MEMBER, AND MOLDING DIE
20210387433 · 2021-12-16 · ·

Provided is a method for producing a shoe member that includes a plurality of portions including a first portion and a second portion, each of which is constituted by one or more of members, the method including: a step of preparing a collective body including a first member that constitutes the first portion and a second member that constitutes the second portion and formed of a material different from that of the first member; and a step of irradiating electromagnetic wave toward the collective body, wherein the electromagnetic wave irradiation step including partly shielding the electromagnetic wave irradiated toward the second member by a shielding member capable of shielding electromagnetic wave, thereby reducing the electromagnetic wave irradiated onto the second member. Also provided is a molding die having a molding space corresponding to a shoe member and capable of being used for producing the shoe member by performing the method.