Injection stretch blow-molding (ISBM) enhancement for semi-crystalline polyolefin containers utilizing alicyclic polyolefins
An injection stretch blow-molded (ISBM) container prepared by way of injection molding a tubular preform followed by reheating and concurrently stretching and blow-molding the heated preform into the container. The container and preform comprise from 70 wt. % to 97.5 wt. % of a semi-crystalline polyolefin composition comprising one or polymers selected from polyethylene polymers and polypropylene polymers and from 2.5 wt. % to 30 wt. % of an alicyclic polyolefin composition, wherein the alicyclic polyolefin composition has a glass transition temperature, Tg, of from 80° to 145° C.
Injection stretch blow-molding (ISBM) enhancement for semi-crystalline polyolefin containers utilizing alicyclic polyolefins
An injection stretch blow-molded (ISBM) container prepared by way of injection molding a tubular preform followed by reheating and concurrently stretching and blow-molding the heated preform into the container. The container and preform comprise from 70 wt. % to 97.5 wt. % of a semi-crystalline polyolefin composition comprising one or polymers selected from polyethylene polymers and polypropylene polymers and from 2.5 wt. % to 30 wt. % of an alicyclic polyolefin composition, wherein the alicyclic polyolefin composition has a glass transition temperature, Tg, of from 80° to 145° C.
METHOD FOR MANUFACTURING A CONTAINER PREFORM USING ADDITIVE MANUFACTURING
The method for manufacturing a preform intended for creating a container comprises: - a step 34 of transferring a digital model of the preform that is to be manufactured to an additive manufacturing machine, - a step 36 of producing the preform using the additive manufacturing machine from the transferred digital model, and - a step 38 of cooling the manufactured preform at ambient temperature.
METHOD FOR MANUFACTURING A CONTAINER PREFORM USING ADDITIVE MANUFACTURING
The method for manufacturing a preform intended for creating a container comprises: - a step 34 of transferring a digital model of the preform that is to be manufactured to an additive manufacturing machine, - a step 36 of producing the preform using the additive manufacturing machine from the transferred digital model, and - a step 38 of cooling the manufactured preform at ambient temperature.
Method for renovating the interior of a hollow structure
A method for renovating the interior of a hollow structure such as a sewerage pit (1) is described. The method provides an access opening (16) to the hollow structure (1); provides a plurality of material sheets (3) comprising reinforcing fibers and a curable resin composition through the access opening (16) and against a wall (11a, 11b) of the hollow structure (1); and provides an inflatable pressure means (4a, 4b) within the hollow structure (1). The pressure means (4a, 4b) are inflated against the wall (11a, 11b). A curing means (6) is then provided within the hollow structure (1) for curing the resin composition; and the resin composition is cured to harden the material sheets and provide a renovated interior of the hollow structure (1).
Injection Stretch Blow-Molding (ISBM) Enhancement for Semi-Crystalline Polyolefin Containers Utilizing Alicyclic Polyolefins
An injection stretch blow-molded (ISBM) container prepared by way of injection molding a tubular preform followed by reheating and concurrently stretching and blow-molding the heated preform into the container. The container and preform comprise from 70 wt. % to 97.5 wt. % of a semi-crystalline polyolefin composition comprising one or polymers selected from polyethylene polymers and polypropylene polymers and from 2.5 wt. % to 30 wt. % of an alicyclic polyolefin composition, wherein the alicyclic polyolefin composition has a glass transition temperature, Tg, of from 60° to 145° C.
Injection Stretch Blow-Molding (ISBM) Enhancement for Semi-Crystalline Polyolefin Containers Utilizing Alicyclic Polyolefins
An injection stretch blow-molded (ISBM) container prepared by way of injection molding a tubular preform followed by reheating and concurrently stretching and blow-molding the heated preform into the container. The container and preform comprise from 70 wt. % to 97.5 wt. % of a semi-crystalline polyolefin composition comprising one or polymers selected from polyethylene polymers and polypropylene polymers and from 2.5 wt. % to 30 wt. % of an alicyclic polyolefin composition, wherein the alicyclic polyolefin composition has a glass transition temperature, Tg, of from 60° to 145° C.
Method of manufacturing a bladder element with an etched feature and article having a bladder element with an etched feature
A method of manufacturing an article comprises etching an etched feature on a surface of a first polymeric sheet, and forming a fluid-filled bladder element from the first polymeric sheet, with the fluid-filled bladder element having a sealable internal cavity that retains fluid. The method includes assembling the bladder element in the article so that a first portion of the bladder element having the etched feature is exposed to view, and a second portion of the bladder element is blocked from view by the article. An article includes the bladder element with the etched feature.
HIGH STRENGTH BLOW-MOLDED STRUCTURE
A blow-molded plastic frame of a portable collapsible sign includes a first outer portion, a second outer portion spaced apart from the first outer portion, and a pattern of structural stiffening features formed in the first and second outer portions. The pattern comprises rows and columns of first depressions extending from the first outer portion into a hollow interior portion between the first and second outer portions, and rows and columns of second depressions extending from the second outer portion into the hollow interior portion. Each first depression has a first floor comprising three first arms having rotational symmetry. Each first arm is rotated from another first arm by 120 degrees. Each second depression has a second floor comprising three second arms having rotational symmetry. Each second arm is rotated from another second arm by 120 degrees. The first floor of each first depression is aligned with the second floor of an adjacent second depression.
HIGH STRENGTH BLOW-MOLDED STRUCTURE
A blow-molded plastic frame of a portable collapsible sign includes a first outer portion, a second outer portion spaced apart from the first outer portion, and a pattern of structural stiffening features formed in the first and second outer portions. The pattern comprises rows and columns of first depressions extending from the first outer portion into a hollow interior portion between the first and second outer portions, and rows and columns of second depressions extending from the second outer portion into the hollow interior portion. Each first depression has a first floor comprising three first arms having rotational symmetry. Each first arm is rotated from another first arm by 120 degrees. Each second depression has a second floor comprising three second arms having rotational symmetry. Each second arm is rotated from another second arm by 120 degrees. The first floor of each first depression is aligned with the second floor of an adjacent second depression.