Patent classifications
B29K101/10
Rotor
A rotor, in particular of an electrical machine, has a base body and at least one metallic end plate which is mounted on the base body. The base body and the at least one end plate have a continuous layer which is injection molded.
Three-dimensional printed composites using sodium silicate binder
A three-dimensional object comprises stacked substrate layers infiltrated by a hardened material. Each substrate layer is a sheet-like structure that comprises fibers held together by a sodium silicate binder. The substrate layer material may be non-woven or woven. The substrate layer may be a non-woven fiber veil bound by a sodium silicate binder. The fibers may optionally include carbon fibers, ceramic fibers, polymer fibers, glass fibers, metal fibers, or a combination thereof.
Methods for manufacturing wind turbine rotor blade components
A method for manufacturing a rotor blade component of a rotor blade includes feeding a flat sheet of material into a thermoforming system, wherein the material comprises at least one of a thermoplastic or thermoset material. The method also includes heating the flat sheet of material via the thermoforming system. Further, the method includes shaping the heated flat sheet of material via at least one roller of the thermoforming system into a desired curved shape. Moreover, the method includes dispensing the shaped sheet of material from the thermoforming system. In addition, the method includes cooling the shaped sheet of material to form the rotor blade component.
Panel with paint ready surface
In a preferred embodiment, a composite panel with a smooth outer surface, ready for painting with or without addition of primer, may be created by constructing a panel layup assembly upon a mold, the panel layup assembly including a composite panel having a core and a resin formulation, and a release film between the mold and the composite panel, where a smooth release surface of the release film is in contact with the composite panel upon construction; initiating curing of the composite panel at a first temperature within a lowermost ten percent of a curing temperature range of the resin formulation; continuing curing of the composite panel at a second temperature above the lowermost ten percent of the curing temperature range; and completing curing of the composite panel at a third temperature below the second temperature.
System and method for curing thermoset composites
A system for curing a thermoset composite may include a tooling die configured to receive and support an uncured thermoset composite part and to heat the uncured thermoset composite part; a pressure media bag configured to be placed over the uncured thermoset composite part disposed on the tooling die and including a pressure media; and a mechanical press configured to apply a consolidation pressure to the uncured thermoset composite part disposed on the tooling die, the pressure media bag may be configured to distribute the consolidation pressure applied by the mechanical press to the uncured thermoset composite part disposed on the tooling die.
Panel with paint ready surface
In a preferred embodiment, a composite panel with a smooth outer surface, ready for painting with or without addition of primer, may be created by constructing a panel layup assembly upon a mold, the panel layup assembly including a composite panel having a core and a resin formulation, and a release film between the mold and the composite panel, where a smooth release surface of the release film is in contact with the composite panel upon construction; initiating curing of the composite panel at a first temperature within a lowermost ten percent of a curing temperature range of the resin formulation; continuing curing of the composite panel at a second temperature above the lowermost ten percent of the curing temperature range; and completing curing of the composite panel at a third temperature below the second temperature.
Manufacturing method of mounting structure, and sheet therefor
A manufacturing method of a mounting structure, the method including: a step of preparing a mounting member including a first circuit member and a plurality of second circuit members placed on the first circuit member; a step of preparing a sheet having thermosetting property; a disposing step of disposing the sheet on the mounting member so as to face the second circuit members; and a sealing step of pressing the sheet against the first circuit member and heating the sheet, to seal the second circuit members and to cure the sheet, wherein the second circuit members include a reference member, and a first adjacent member and a second adjacent member each adjacent to the reference member, a separation distance D1 between the reference member and the first adjacent member is different from a separation distance D2 between the reference member and the second adjacent member, at least one of the plurality of the second circuit members is a hollow member to be provided with a space from the first circuit member, and in the sealing step, the plurality of the second circuit members are sealed so as to maintain the space.
Low density syntactic foams via material extrusion additive manufacturing
An ink formulation for additive manufacturing of low density syntactic foams is described. The ink formulation can include a thermoset resin, a curing agent suitable for use with the thermoset resin, a plurality of hollow spheres, such as glass microballoons, one or more solvents, and one or more non-hollow, viscosity modifying filler. Also described are a method of preparing the ink formulation, a method of preparing three-dimensional objects comprising low density syntactic foams, and the three-dimensional objects prepared thereby.
Molded article and method for making the same
A composite article includes a first segment and a second segment spaced apart form the first segment. The composite article includes continuous fibers that extend from the first segment to the second segment. The composite article also includes discontinuous fiber distributed throughout the composite article.
Method of shaping a cured thermosetting resin
The present invention relates to a method of shaping a cured thermosetting resin substrate, and more particularly to a method of shaping a cured thermosetting resin using electromagnetic radiation, said method comprises providing a cured thermosetting resin substrate; providing a confined temperature controlling environment; placing the cured thermosetting resin substrate in the confined temperature controlling environment; providing a source of electromagnetic radiation; irradiating the cured thermosetting resin substrate in the confined temperature controlling environment; and shaping the irradiated thermosetting resin substrate.