B29K2023/06

Pouch forming apparatus and method

To solve the above problem, a pouch forming apparatus according to an embodiment of the present invention includes: a die in which a forming space is recessed inward from a top surface thereof; a partition wall partitioning the forming space into first and second forming spaces; a stripper disposed above the die and configured to descend to contact the die with the pouch film therebetween to fix the pouch film to be seated on a top surface of the die; and an electromagnetic force generation part disposed above the forming space and configured to generate electromagnetic force and configured to apply the electromagnetic force to the forming space.

Injection stretch blow-molding (ISBM) enhancement for semi-crystalline polyolefin containers utilizing alicyclic polyolefins

An injection stretch blow-molded (ISBM) container prepared by way of injection molding a tubular preform followed by reheating and concurrently stretching and blow-molding the heated preform into the container. The container and preform comprise from 70 wt. % to 97.5 wt. % of a semi-crystalline polyolefin composition comprising one or polymers selected from polyethylene polymers and polypropylene polymers and from 2.5 wt. % to 30 wt. % of an alicyclic polyolefin composition, wherein the alicyclic polyolefin composition has a glass transition temperature, Tg, of from 80° to 145° C.

Heat sealer provided with interfacial temperature sensor
11577474 · 2023-02-14 ·

The embodiment provides a heat-sealing apparatus and a method of accurately controlling heat sealing temperature by measuring the temperature using a heat-sealing apparatus which heat-seals a pair of heat seal materials by nipping them between a pair of heating bodies. The method of heat-sealing includes mounting a cover material on the surface of at least one of the heating bodies to be in contact with the heat seal material, attaching a minute temperature sensor to the surface of the cover material on the side to be in contact with the heat seal material, and controlling temperature of welding face by the temperature detected by the minute temperature sensor, and an apparatus therefor.

Heat sealer provided with interfacial temperature sensor
11577474 · 2023-02-14 ·

The embodiment provides a heat-sealing apparatus and a method of accurately controlling heat sealing temperature by measuring the temperature using a heat-sealing apparatus which heat-seals a pair of heat seal materials by nipping them between a pair of heating bodies. The method of heat-sealing includes mounting a cover material on the surface of at least one of the heating bodies to be in contact with the heat seal material, attaching a minute temperature sensor to the surface of the cover material on the side to be in contact with the heat seal material, and controlling temperature of welding face by the temperature detected by the minute temperature sensor, and an apparatus therefor.

FILMS AND SHEETS HAVING MICROLAYERS AND NANOLAYERS INCLUDING RECYCLED CONTENT

A polymeric film, sheet, or extrusion coating is formed as a multilayered structure having at least one A layer and at least one B layer. The polymeric film, sheet, or extrusion coating is able to include at least 30% recycled content resin while also exhibiting improved stiffness and strength relative to films with purely virgin polymers. One embodiment of the present invention further presents improved oxygen barrier properties relative to existing films, sheets, or extrusion coatings. Due to the strong structural properties, the polymeric film, sheet, or extrusion coating allows for the inclusion of recycled content into applications where recycled content has previously not been able to be included, such as flexible food, pharmaceutical, or cosmetics packaging.

FILMS AND SHEETS HAVING MICROLAYERS AND NANOLAYERS INCLUDING RECYCLED CONTENT

A polymeric film, sheet, or extrusion coating is formed as a multilayered structure having at least one A layer and at least one B layer. The polymeric film, sheet, or extrusion coating is able to include at least 30% recycled content resin while also exhibiting improved stiffness and strength relative to films with purely virgin polymers. One embodiment of the present invention further presents improved oxygen barrier properties relative to existing films, sheets, or extrusion coatings. Due to the strong structural properties, the polymeric film, sheet, or extrusion coating allows for the inclusion of recycled content into applications where recycled content has previously not been able to be included, such as flexible food, pharmaceutical, or cosmetics packaging.

POROUS POLYMER COMPOSITE FOR DAYTIME RADIATIVE COOLING AND METHOD OF MAKING A POROUS POLYMER COMPOSITE
20230012311 · 2023-01-12 ·

A porous polymer composite for daytime radiative cooling includes a porous polymer matrix comprising a thermoplastic polymer and including a plurality of pores, and selectively emitting particles dispersed in the porous polymer matrix. When exposed to solar radiation, the porous polymer composite comprises an infrared emissivity of at least about 80% in a wavelength range of 8-13 μm and/or a solar reflectivity of at least about 80% in a wavelength range of 0.3-2 μm.

Coextruded Polyethylene Pipe and Methods of Making and Using Same
20230039633 · 2023-02-09 ·

A pipe having an inner layer and an outer layer. The inner layer includes a first material having a first hydrostatic design basis (HDB), and the outer layer is coextruded with the inner layer and includes a second material having a second HDB. The second HDB is greater than or equal to the first HDB, and the first HDB and the second HDB are as specified in ASTM Test Method D2387. Also provided re methods of making and using the pipe.

Method of making coextruded, crosslinked polyolefin foam with KEE cap layers

The present disclosure is directed to a physically crosslinked, closed cell continuous multilayer foam structure comprising at least one foam polypropylene/polyethylene layer with a KEE cap layer. The multilayer foam structure can be obtained by coextruding a multilayer structure comprising at least one foam layer composition layer with at least one cap layer composition layer, irradiating the coextruded structure with ionizing radiation, and continuously foaming the irradiated structure.

FIBER OPTIC CABLES WITH ACCESS FEATURES AND METHODS OF MAKING FIBER OPTIC CABLES
20180003914 · 2018-01-04 ·

Cables are constructed with extruded discontinuities in the cable jacket that allow the jacket to be torn to provide access to the cable core. The discontinuities can be longitudinally extending strips of material in the cable jacket.