Patent classifications
C01F7/46
Pseudo-boehmite, manufacturing process and application thereof
A pseudo-boehmite has a dry basis content of 55-85 wt % and contains a phosphoric acid ester group. The sodium oxide content is not greater than 0.5 wt %, and the phosphorus content (in terms of phosphorus pentoxide) is 1.2-5.7 wt %, relative to 100 wt % of the total weight of the pseudo-boehmite. The pseudo-boehmite has a low sodium content.
Pseudo-boehmite, manufacturing process and application thereof
A pseudo-boehmite has a dry basis content of 55-85 wt % and contains a phosphoric acid ester group. The sodium oxide content is not greater than 0.5 wt %, and the phosphorus content (in terms of phosphorus pentoxide) is 1.2-5.7 wt %, relative to 100 wt % of the total weight of the pseudo-boehmite. The pseudo-boehmite has a low sodium content.
SYSTEMS AND METHODS FOR RECOVERING SALTS, ALUMINUM, ALUMINA AND AMMONIA FROM SALT SLAG WASTE GENERATED IN ALUMINUM RECYCLING
The disclosed technology includes a method for producing ultrafine alumina from salt slag waste generated in aluminum recycling useful in the manufacture of durable ceramic products; a system for recovering alumina from salt slag waste; a method and systems for recovering salts, aluminum and alumina from salt slag waste; and a method and systems of capturing ammonia in a process recovering salts, aluminum and alumina from salt slag waste. The methods and systems provided crush the dry particles of the salt slag waste, scrub the slag with water, and with steam and by means of a vented alumina press, dewater the scrubbed slag particles. In some methods and systems of the disclosed technology, the particles of the pressed alumina cake are further reduced. In some methods and systems, the salt in the salt effluent is crystalized. In some methods and systems of the disclosed technology, the ammonia is contained and captured.
SYSTEMS AND METHODS FOR RECOVERING SALTS, ALUMINUM, ALUMINA AND AMMONIA FROM SALT SLAG WASTE GENERATED IN ALUMINUM RECYCLING
The disclosed technology includes a method for producing ultrafine alumina from salt slag waste generated in aluminum recycling useful in the manufacture of durable ceramic products; a system for recovering alumina from salt slag waste; a method and systems for recovering salts, aluminum and alumina from salt slag waste; and a method and systems of capturing ammonia in a process recovering salts, aluminum and alumina from salt slag waste. The methods and systems provided crush the dry particles of the salt slag waste, scrub the slag with water, and with steam and by means of a vented alumina press, dewater the scrubbed slag particles. In some methods and systems of the disclosed technology, the particles of the pressed alumina cake are further reduced. In some methods and systems, the salt in the salt effluent is crystalized. In some methods and systems of the disclosed technology, the ammonia is contained and captured.
METHODS FOR PURIFYING ALUMINIUM IONS
There is provided a process for purifying aluminum ions comprising: reacting an aluminum-containing material with an acid so as to obtain a composition comprising aluminum ions; precipitating said aluminum ions in the form of AlCl.sub.3; optionally converting AlCl.sub.3 into Al(OH).sub.3; and heating said AlCl.sub.3 or said Al(OH).sub.3 under conditions effective for converting AlCl.sub.3 or Al(OH).sub.3 into Al.sub.2O.sub.3 and optionally recovering gaseous HCl so-produced. Aluminum ions so purified are thus useful for preparing various types of alumina.
METHODS FOR PURIFYING ALUMINIUM IONS
There is provided a process for purifying aluminum ions comprising: reacting an aluminum-containing material with an acid so as to obtain a composition comprising aluminum ions; precipitating said aluminum ions in the form of AlCl.sub.3; optionally converting AlCl.sub.3 into Al(OH).sub.3; and heating said AlCl.sub.3 or said Al(OH).sub.3 under conditions effective for converting AlCl.sub.3 or Al(OH).sub.3 into Al.sub.2O.sub.3 and optionally recovering gaseous HCl so-produced. Aluminum ions so purified are thus useful for preparing various types of alumina.
A Method for the Manufacture of Hydraulic Binders from Water Treatment Residuals
A method for the manufacture of a high alumina hydraulic binder comprising hydrating a source of aluminium ions with a source of calcium ions in the presence of water to form mineral hydrates and subsequently heating said mineral hydrates to form said high alumina hydraulic binder.
Recovery of mining processing product using boronic acid-containing polymers
Methods and compositions for improving performance of flocculants in an industrial production process. Methods include pH triggered cross-linking reaction between a flocculating agent, such as dextran, and a composition comprising a boronic acid-containing polymer. The pH trigger can be provided by a fluid having a pH of 8 or more. The production process can be a Bayer Process and the fluid is caustic liquor or slurry in the fluid circuit of the Bayer, wherein the reaction time is reduced over conventional methods and the cross-linked dextran composition effectuates improved flocculation of the trihydrate particles.
Recovery of mining processing product using boronic acid-containing polymers
Methods and compositions for improving performance of flocculants in an industrial production process. Methods include pH triggered cross-linking reaction between a flocculating agent, such as dextran, and a composition comprising a boronic acid-containing polymer. The pH trigger can be provided by a fluid having a pH of 8 or more. The production process can be a Bayer Process and the fluid is caustic liquor or slurry in the fluid circuit of the Bayer, wherein the reaction time is reduced over conventional methods and the cross-linked dextran composition effectuates improved flocculation of the trihydrate particles.
PROCESS FOR THE PREPARATION OF HIGH PURITY ALUMINA
A method for preparing high purity alumina (HPA) is provided. The method includes subjecting an aluminum feedstock to acid leaching, thereby yielding an aluminum bearing leachate; subjecting the aluminum bearing leachate to solvent extraction, thereby yielding an organic phase which is loaded with aluminum; stripping the aluminum from the loaded organic phase with a stripping solution containing an acid, thereby yielding an aluminum bearing extract; crystallizing an aluminum salt from the aluminum bearing extract; dissolving the aluminum salt in an ammoniacal solution, thereby generating a boehmite precursor compound and an ammonium salt; calcining the boehmite precursor compound to yield HPA; subjecting the ammonium salt to electro-dialysis, thereby yielding ammonia and the acid; and performing at least one step of (a) utilizing the ammonia in preparing the ammoniacal solution used in a subsequent iteration of the method, or (b) utilizing the acid in preparing the stripping solution used in a subsequent iteration of the method.