C01P2002/52

A POWDEROUS LITHIUM COBALT-BASED OXIDE CATHODE ACTIVE MATERIAL POWDER FOR RECHARGEABLE LITHIUM ION BATTERIES AND A METHOD FOR MAKING THEREOF
20230040464 · 2023-02-09 ·

A lithium cobalt-based oxide cathode active material powder having: —a primary phase comprising Li, Co, and O, and —a secondary phase comprising LiNaSO.sub.4, wherein the content of said LiNaSO.sub.4 secondary phase in said powder is of at least 0.4 wt. % and inferior or equal to 1.1 wt. % with respect to a total weight of the cathode active material powder, said cathode active material powder being characterized in that it has a S/Na atomic ratio superior or equal to 0.80 and inferior or equal to 1.20.

DOPED PHOSPHORUS-SULFUR IODIDE SOLID ELECTROLYTE, PREPARATION METHOD THEREFOR, AND USE THEREOF

A doped phosphorus-sulfur iodide solid electrolyte, a preparation method therefor, and use thereof. The chemical formula of said solid electrolyte is Li.sub.6-xM.sub.xP.sub.1-xS.sub.5I, in which 0<x<0.8, and M is tungsten and/or molybdenum. Said method comprises: 1) mixing a lithium source, a phosphorus source, an iodine source, a sulfur source, and an M source in an inert atmosphere, and then ball-milling same to obtain a solid electrolyte precursor; and 2) sintering the solid electrolyte precursor obtained in step 1) in an inert atmosphere or in vacuum to obtain the doped phosphorus-sulfur iodide solid electrolyte.

POSITIVE ELECTRODE ACTIVE MATERIAL, METHOD OF PREPARING THE SAME, AND LITHIUM SECONDARY BATTERY INCLUDING THE SAME

Provided are a positive electrode active material for a lithium secondary battery, a method of preparing the same, and a lithium secondary battery including the same.

According to an exemplary embodiment, a positive electrode active material for a lithium secondary battery which includes lithium metal oxide particles and a coating layer placed on at least a part of a surface of the lithium metal oxide particles may be provided, wherein the coating layer includes B, LiOH, Li.sub.2CO.sub.3, and Li.sub.2SO.sub.4.

CATHODE ACTIVE MATERIAL AND LITHIUM SECONDARY BATTERY COMPRISING SAME

The present exemplary embodiments relate to a positive electrode active material and a lithium secondary battery including the same. The positive active material for a lithium secondary battery according to an exemplary embodiment includes lithium metal oxide particles including lithium, nickel, cobalt, manganese and doping elements, and includes a first domain and a second domain inside the lithium metal oxide particles.

POSITIVE ELECTRODE ACTIVE MATERIAL, METHOD FOR PRODUCING SAME, AND LITHIUM SECONDARY BATTERY INCLUDING SAME

The present exemplary embodiments relate to a positive electrode active material, a manufacturing method thereof, and a lithium secondary battery including the same. A positive active material for a lithium secondary battery according to an exemplary embodiment is a lithium metal oxide particle in the form of secondary particles including a plurality of primary particles: a first coating layer positioned on at least a part of the surface of the primary particle, and a second coating layer positioned over at least a portion of the secondary particle surface, the first coating layer comprising a first niobium compound, the second coating layer comprising the first niobium compound and a second niobium compound having a composition different from the first niobium compound.

POSITIVE ELECTRODE ACTIVE MATERIAL FOR NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY, AND NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY

This positive electrode active material for a non-aqueous electrolyte secondary battery contains a lithium-transition metal composite compound. The lithium-transition metal composite compound is represented by general formula Li.sub.xMn.sub.yNi.sub.zMe.sub.αO.sub.aF.sub.b (in the formula, 1≤x≤1.2, 0.4≤y≤0.8; 0≤z≤0.4, x+y+z=2, 0<α<0.05, 1.8≤a≤2, and 1.8≤a±b≤2.2 are satisfied, and Me represents at least two kinds of elements selected from metal elements other than Li, Mn, and Ni) and Me includes at least one kind of element having an ion radius of 0.6 Å or more.

POSITIVE ELECTRODE ACTIVE MATERIAL FOR ALL-SOLID-STATE LITHIUM ION SECONDARY BATTERY, METHOD FOR PRODUCING THE SAME, AND ALL-SOLID-STATE LITHIUM ION SECONDARY BATTERY

A positive electrode active material for an all-solid-state lithium ion secondary battery, containing: a lithium-metal composite oxide particle having a niobium solid solution layer and a center other than the niobium solid solution layer; and a coating layer coating at least a part of a surface of the lithium-metal composite oxide particle and formed of a compound containing lithium and niobium, an average thickness of the coating layer is 2 nm or more and 1 μm or less, and an average thickness of the niobium solid solution layer is 0.5 nm or more and 20 nm or less.

Ferrite sintered magnet and rotating electric machine comprising the same

A ferrite sintered magnet comprising an M type Sr ferrite having a hexagonal structure as a main phase, wherein the ferrite sintered magnet comprises La and Co, a content of B is 0.005 to 0.9% by mass in terms of B.sub.2O.sub.3, a content of Zn is 0.01 to 1.2% by mass in terms of ZnO, and the ferrite sintered magnet satisfies [La]/[Zn]≤0.79 and [Co]/[Zn]≤0.67 when an atomic concentration of La is represented by [La], an atomic concentration of Co is represented by [Co], and an atomic concentration of Zn is represented by [Zn].

CATHODE MATERIAL AND METHOD FOR PREPARING CATHODE MATERIAL, CATHODE, LITHIUM ION BATTERY AND VEHICLE
20230009617 · 2023-01-12 ·

The present disclosure provides a cathode material and a method for preparing the cathode material, a cathode, a lithium ion battery and a vehicle. The cathode material comprises a matrix particle, wherein the matrix particle is a monocrystal particle comprising nickel lithium manganate and nickel cobalt lithium manganate. A position in the matrix particle close to a surface layer is provided with a buffer layer. A content of at least one of elements Ni, Co and Mn in the buffer layer is lower than contents thereof in other positions of the matrix particle. The cathode material has at least one of advantages of relatively high specific capacity, cycling stability, better safety performance and the like, and the buffer layer can alleviate erosion by an electrolyte and inhibit separation of active oxygen.

MIXED METAL OXIDE

In an aspect, a mixed metal oxide comprises or consists essentially of: a mixture comprises or consisting essentially of 0.30 to 0.69 parts by mole Mg, 0.20 to 0.69 parts by mole Zn, 0.01 to 0.30 parts by mole of a third element selected from Al and Ga, and, either, when the third element is Al, 0.00 to 0.31 parts by mole of other elements selected from metals and metalloids, or, when the third element is Ga, 0.00 to 0.15 parts by mole of other elements selected from metals and metalloids, wherein the sum of all parts by mole of Mg, Zn, the third element, and the other elements amounts to 1.00, wherein the amount in parts by mole of the other elements is lower than the amount in parts by mole of Mg and is lower than the amount in parts by mole of Zn; oxygen; and less than 0.01 parts by mole of non-metallic and non-metalloid impurities.