Patent classifications
C03B2203/22
Method for manufacturing optical fiber preform, optical fiber preform, method for manufacturing optical fiber, and optical fiber
A method for manufacturing an optical fiber preform includes: producing a core preform including a core portion made of transparent glass and a first cladding layer obtained by adding fluorine to the core portion; and forming, on an outer periphery of the first cladding layer, a second cladding layer made of glass having a refractive index higher than that of the first cladding layer. Further, a refractive index profile is formed in the first cladding layer due to a fluorine concentration profile, the refractive index profile being provided at least near a boundary surface with the second cladding layer and having a profile such that a refractive index difference between a refractive index of the first cladding layer and a refractive index of the second cladding layer decreases in accordance with a reduction in a distance from the boundary surface with the second cladding layer.
Method to prevent cracks in optical fiber preforms
The present disclosure provides optical fiber preforms formed from core canes having large core-clad ratio, intermediate core-cladding assemblies, and methods for making the preforms and core cladding assemblies. The preforms are made with capped core canes. The capping material has a coefficient of thermal expansion less than the coefficient of thermal expansion of the core cane and more closely matched to or lower than the coefficient of thermal expansion of the surrounding cladding monolith in a cane-in-soot process. Presence of the cap reduces stresses that arise from differential thermal expansion of the core cane and cladding materials and leads to preforms having low defect concentration and low probability of failure during subsequent thermal processing steps.
Low cross-talk multicore optical fiber for single mode operation
A multicore optical fiber comprises a common cladding and a plurality of core portions disposed in the common cladding. Each of the core portions includes a central axis, a core region extending from the central axis to a radius r.sub.1, the core region comprising a relative refractive index Δ.sub.1, an inner cladding region extending from the radius r.sub.1 to a radius r.sub.2, the inner cladding region comprising a relative refractive index Δ.sub.2, and a depressed cladding extending from the radius r.sub.2 to a radius r.sub.3, the depressed cladding region comprising a relative refractive index Δ.sub.3 and a minimum relative refractive index Δ.sub.3 min. The relative refractive indexes may satisfy Δ.sub.1>Δ.sub.2>Δ.sub.3 min. The mode field diameter of each core portion may greater than or equal to 8.2 μm and less than or equal to 9.5 μm.
Optical fiber and method of manufacturing optical fiber
An optical fiber includes: a central core portion; an intermediate layer; a trench layer; and a cladding portion. Further, Δ1>Δ2>Δ3 and 0>Δ3 are satisfied, where Δ1 is a relative refractive-index difference of the central core portion, Δ2 is a relative refractive-index difference of the intermediate layer, and Δ3 is a relative refractive-index difference of the trench layer with respect to the cladding portion, respectively, and (c−b) is smaller than 4.5 μm when Δ1 is equal to or larger than 0.36% and equal to or smaller than 0.40%, Δ2 is equal to or larger than −0.05% and equal to or smaller than 0.05%, |Δ3| is equal to or smaller than 0.25%, Δ1×|Δ3| is equal to or smaller than 0.08%.sup.2, an inner diameter of the trench layer is 2b, and an outer diameter of the trench layer is 2c.
Optical fiber and method of manufacturing optical fiber
An optical fiber includes: a central core portion; an intermediate layer; a trench layer; and a cladding portion. Further, relationships Δ1>Δ2>Δ3 and 0>Δ3 are satisfied, where Δ1, Δ2, and Δ3 are a relative refractive-index difference of the central core portion, the intermediate layer, and the trench layer, respectively, with respect to the cladding portion, Δ1 is equal to or larger than 0.34% and equal to or smaller than 0.37%, |Δ3| is equal to or larger than 0.1% and equal to or smaller than 0.25%, Δ1×|Δ3| is equal to or smaller than 0.08%.sup.2, a mode field diameter at a wavelength of 1310 nm is equal to or larger than 8.8 μm, and a transmission loss at a wavelength of 1550 nm is equal to or smaller than 0.195 dB/km.
SPECIAL OPTICAL FIBER FOR MEASURING 3D CURVED SHAPE, MANUFACTURING METHOD THEREOF, AND SYSTEM FOR MEASURING 3D CURVED SHAPE BY USING SPECIAL OPTICAL FIBER
Provided is a special optical fiber for measuring a 3D curved shape, and a system for measuring the 3D curved shape by using a special optical fiber. The special optical fiber comprises: an optical fiber core for transmitting an optical signal; an inner cladding covering the optical fiber core; and an outer cladding covering the inner cladding. In particular, the refractive index (n1) of the optical fiber core, the refractive index (n2) of the inner cladding, and the refractive index (n3) of the outer cladding are set in a relationship of n1≥n3>n2. The inner cladding covering the optical fiber core has a cut portion in the longitudinal direction. The optical fiber core is exposed through the cut portion. In addition, the cut portion is filled with a material having the same refractive index as the optical fiber core or the outer cladding.
Optical fiber and method for manufacturing optical fiber
An optical fiber includes: a central core portion; an intermediate layer formed around an outer circumference of the central core portion; a trench layer formed around an outer circumference of the intermediate layer; and a cladding portion formed around an outer circumference of the trench layer. Further, when, relative to the cladding portion, a relative refractive-index difference of the central core portion is Δ1, a relative refractive-index difference of the intermediate layer is Δ2, and a relative refractive-index difference of the trench layer is Δ3, relationships Δ1>Δ2>Δ3 and 0>Δ3 are satisfied and Δ1 is equal to or greater than 0.34% and equal to or less than 0.40%, |Δ3| is equal to or less than 0.25%, and Δ1×|Δ3| is less than 0.08%.sup.2.
Multi-core fibers and method of manufacturing the same, and optical transmission system and optical transmission method
A multi-core fiber includes: a plurality of cores; and a cladding portion formed around outer peripheries of the cores. Further, the cores each have a propagation characteristic conforming to any one of a plurality of standards for optical propagation characteristics, and of the cores, cores that are closest to each other conform to standards different from each other.
METHOD FOR DRAWING AN OPTICAL FIBER USING ROD-IN CYLINDER TECHNIQUE
A method for drawing an optical fibre from an optical fibre preform with a core section, a cladding section, a first gap and a second gap. The optical fibre preform is attached to an optical fibre draw tower through a handle. In addition, the optical fibre preform is connected to a vacuum system to supply and remove gas from the first gap and the second gap. Moreover, the gas is supplied to create a thermal barrier between the core section and the cladding section during heating of the optical fibre preform. Further, the optical fibre preform is heated inside a heating furnace to draw the optical fibre from the optical fibre preform.
OPTICAL FIBRE PREFORM AND METHOD OF MANUFACTURING THEREOF
A reduced diameter optical fibre preform positioned along a longitudinal axis includes a core section defined around the longitudinal axis and a cladding section circumferentially surrounding the core section. The reduced diameter optical fibre preform is manufactured by utilizing a calcium aluminum silicate rod and a fluorine doped glass cylinder.