Patent classifications
C03B2205/40
Methods for modifying multi-mode optical fiber manufacturing processes
Methods for modifying multi-mode optical fiber manufacturing processes are disclosed. In one embodiment, a method for modifying a process for manufacturing multi-mode optical fiber includes measuring at least one characteristic of a multi-mode optical fiber. The at least one characteristic is a modal bandwidth or a differential mode delay at one or more wavelengths. The method further includes determining a measured peak wavelength of the multi-mode optical fiber based on the measured characteristic, determining a difference between the target peak wavelength and the measured peak wavelength, and modifying the process for manufacturing multi-mode optical fiber based on the difference between the target peak wavelength and the measured peak wavelength.
OPTICAL FIBER AND METHOD FOR PRODUCING OPTICAL FIBER
An optical fiber has a central axis. The optical fiber includes a core made of silica glass and extending along the central axis, a cladding made of silica glass and surrounding the core, the cladding extending along the central axis, and a coating layer made of resin and surrounding the cladding, the coating layer extending along the central axis. An outer diameter of the cladding varies along the central axis. A residual stress in a direction along the central axis varies along the central axis, the residual stress being averaged over the core and the cladding in a cross section perpendicular to the central axis. A deviation from an average value of the outer diameter and a deviation from an average value of the residual stress have signs opposite to each other.
Method for manufacturing multimode optical fibers
A method of manufacturing a multimode optical fiber includes specifying a peak wavelength λ.sub.P for the multimode optical fiber. The peak wavelength λ.sub.P corresponds to a wavelength at which the multimode optical fiber has a maximum bandwidth. The multimode optical fiber comprises a core and a cladding surrounding and directly adjacent to the core. The core has a radius r.sub.1 and a maximum relative refractive index Δ.sub.1,MAX>0. The cladding comprises a depressed-index region having a minimum relative refractive index Δ.sub.3,MIN<0 and a volume v. A draw tension T for the multimode optical fiber is selected based on a correlation relating peak wavelength λ.sub.P to draw tension T, the correlation comprising a correlation constant. The correlation constant K is a function of at least one of Δ.sub.1,MAX, r.sub.1, v, Δ.sub.3,MIN, and λ.sub.P. The multimode optical fiber is drawn from a preform at the draw tension T.
OPTICAL FIBER MANUFACTURING METHOD AND APPARATUS
An optical fiber manufacturing method includes: a drawing step of heating one end portion of an optical fiber preform to melt and deform the one end portion and drawing an optical fiber, wherein in the drawing step, drawing is performed while applying pressure to a melted-deformed portion that is melted and deformed.
Method of manufacturing an optical fiber using axial tension control to reduce axial variations in optical properties
A method of manufacturing a tuned optical fiber includes providing a first preform from a set of like preforms each having substantially the same refractive index profile, including amount of axial variation relative to a target refractive index profile. The method includes drawing a reference optical fiber from the first preform and measuring a variation in an optical or physical property as a function of axial position. The method also includes drawing from a second preform from the set of like preforms the tuned optical fiber. The drawing includes using a time-varying tension that reduces the amount of variation of the optical or physical property of interest. The time-varying tension is defined by an amount of axial stress imparted to the tuned fiber needed to alter the refractive index profile and the at least one optical or physical property based on a stress-optic effect.
Self-learning fiber processing system and method
Provided is a system for and a method of processing an optical fiber, such as tapering an optical fiber. The method includes receiving fiber parameters defining characteristics of an optical fiber, modeling an idealized fiber based on the fiber parameters to establish modeled data, and establishing processing parameters. A processing operation is performed on the optical fiber according to the processing parameters to produce a resultant fiber. Aspects of the resultant fiber are measured to establish measured data. The measured data and the modeled data are normalized to a common axis and a difference between the two is determined. The processing parameters are adjusted based on the differences.
OPTICAL FIBER PREFORM AND METHOD OF MANUFACTURING OPTICAL FIBER
An optical fiber preform includes: a columnar portion having an approximately constant radius of r; and a taper portion located adjacent to the columnar portion in a lengthwise direction and having a radius decreasing along the lengthwise direction. The taper portion includes: a first taper portion including a portion having a radius varying between 0.9r and 0.6r; and a second taper portion including a portion having a radius varying between 0.4r and 0.15r. A diameter of the first taper portion in the portion having the radius varying between 0.9r and 0.6r decreases so as to form a maximum angle θ1 between 40 degrees and 60 degrees with respect to the columnar portion, a diameter of the second taper portion in the portion having the radius varying between 0.4r and 0.15r decreases so as to form an average angle θ2 between 5 degrees and 30 degrees with respect to a central axis in the lengthwise direction, and a volume of the taper portion is smaller than or equal to 45% of a volume of a column having a same outer diameter as a maximum outer diameter of the taper portion and having a same length as the taper portion.
High-density optical fiber ribbon with cladding-strengthened glass optical fibers in a common protective coating and fiber ribbon interconnects employing same
A high-density optical fiber ribbon is formed by two or more cladding-strengthened glass optical fibers each having an outer surface and that do not individually include a protective polymer coating. A common protective coating substantially surrounds the outer surfaces of the two or more cladding-strengthened glass optical fibers so that the common protective coating is common to the two or more cladding-strengthened glass optical fibers. A fiber ribbon cable is formed by adding a cover assembly to the fiber ribbon. A fiber ribbon interconnect is formed adding one or more optical connectors to the fiber ribbon or fiber ribbon cable. Optical data transmission systems that employ the fiber ribbon to optically connect to a photonic device are also disclosed. Methods of forming the cladding-strengthened glass optical fibers and the high-density optical fiber ribbons are also disclosed.
FIBER OPTIC MANUFACTURING IN SPACE
Aspects of the embodiments are directed to systems and methods for forming an optical fiber in a low gravity environment, and an optical fiber formed in a low gravity environment. The system can include a preform holder configured to secure a preform; a heating element secured to a heating element stage and residing adjacent the preform holder; a heating element stage motor configured to move the heating element stage; a tension sensor; a spool; a spool tension motor coupled to the spool and configured to rotate the spool; and a control system communicably coupled to the heating element stage motor and the spool tension motor and configured to control the movement of the heating element stage based on a rotational speed of the spool. The optical fiber can include a fluoride composition, such ZrF4-BaF2-LaF3-AlF3-NaF (ZBLAN), and can be characterized by an insertion loss in a range from 13 dB/1000 km to 120 dB/1000 km.
METHOD FOR CONTROLLING THE THICKNESS OF A SUBSTRATE
A method for controlling the thickness of a glass ribbon and an article produced thereby are provided. The method includes: providing a glass ribbon by drawing from a melt or redrawing from a preform; predefining a nominal thickness of the glass ribbon; determining the thickness of the glass ribbon over its entire net width; determining at least one deviation of the thickness of the glass ribbon from the predefined nominal thickness; identifying the area of the thickness deviation in the glass ribbon; and heating the area of the at least one thickness deviation in the glass ribbon using a laser, so that the glass ribbon attains the predefined thickness.