Patent classifications
C03B2205/62
Method and apparatus for suppressing flow instabilities in an optical fiber draw system
A furnace system includes a muffle defining a furnace cavity. A lower heater is coupled to the muffle and is configured to create a hot zone within the furnace cavity having a temperature of about 1900° C. or greater. An upper muffle extension is positioned above the muffle and defines a handle cavity. A downfeed handle is positioned within the handle cavity such that a gap is defined between an outer surface of the downfeed handle and an inner surface of the upper muffle extension. An upper heater is thermally coupled to the upper muffle extension and configured to heat the gap. A gas screen is positioned in the upper muffle extension and is configured to inject a process gas into the handle cavity.
Optical fiber draw furnace system and method
An optical fiber draw system and method of operating thereof. The method includes positioning a downfeed handle for supporting an optical fiber preform within a furnace such that the downfeed handle is movable within the furnace. The method further includes operating one or more heating elements to thermally heat at least a portion of an upper muffle extension disposed within the furnace, the one or more heating elements being moveable with the downfeed handle.
Optical fiber forming apparatus
An optical fiber forming apparatus comprises: a draw furnace comprising: (i) a muffle with an inner surface, (ii) an axial opening below the muffle, the inner surface of the muffle defining a passageway extending through the axial opening, and (iii) an upper inlet into the passageway; and a tube that extends into the passageway of the draw furnace above the axial opening, the tube having (i) an outer surface and the inner surface of the muffle surrounds the outer surface of the tube with a space separating the outer surface of the tube from the inner surface of the muffle, (ii) an inner surface that defines a second passageway extending through the tube, (iii) an inlet into the second passageway of the tube, (iii) an outlet out of the second passageway of the tube.
ELONGATING METHOD AND ELONGATING APPARATUS FOR GLASS BASE MATERIAL
Provided is an elongating method for elongating a glass base material by heating the same while moving the same downward within an elongating apparatus, the glass base material including a transparent tapered section, wherein the transparent tapered section is located at an upper end of the glass base material and has an end face to which a suspension dummy formed from a glass pole is welded, the elongating method comprising steps for: starting to elongate the glass base material by heating the same, starting from a lower-end side thereof, by causing the glass base material to pass through a range within the elongating apparatus in which a preset elongating process temperature or higher is maintained; and after the tapered section enters the range, ending the elongating of the glass base material before the end face enters the range.
OPTICAL FIBER DRAW FURNACE SYSTEM AND METHOD
An optical fiber draw system and method of operating thereof. The method includes positioning a downfeed handle for supporting an optical fiber preform within a furnace such that the downfeed handle is movable within the furnace. The method further includes operating one or more heating elements to thermally heat at least a portion of an upper muffle extension disposed within the furnace, the one or more heating elements being moveable with the downfeed handle.
MANUFACTURING METHOD FOR OPTICAL FIBER AND MANUFACTURING APPARATUS FOR OPTICAL FIBER
A manufacturing method for an optical fiber, includes: drawing, while heating in a heating furnace, a lower end of an optical fiber preform that is to be an optical fiber having a core consisting of silica glass containing a rare earth element compound. The heating furnace has a temperature profile in which a temperature of the heating furnace increases to a maximum temperature T.sub.max and then decreases from an upstream side of the heating furnace toward a downstream side of the heating furnace. The temperature profile has a changing point at which the temperature decreases more steeply on the downstream side from a position where the maximum temperature T.sub.max is reached. At the maximum temperature, a temperature of the silica glass is higher than or equal to a glass transition temperature and the silica glass is in a single phase.
Fiber optic manufacturing in space
Aspects of the embodiments include an optical fiber formed in a low gravity environment. The optical fiber can be used in airframe applications for missile defense, oil-field applications for down-well laser applications, optical communications, and other applications. The optical fiber can include a fluoride composition, such ZrF4-BaF2-LaF3-AlF3-NaF (ZBLAN), and can be characterized by an insertion loss in a range from 13 dB/1000 km to 120 dB/1000 km. The optical fiber can deliver optical energy with low insertion loss at the desired power and wavelength for the various applications.
METHOD AND APPARATUS FOR SUPPRESSING FLOW INSTABILITIES IN AN OPTICAL FIBER DRAW SYSTEM
A furnace system includes a muffle defining a furnace cavity. A lower heater is coupled to the muffle and is configured to create a hot zone within the furnace cavity having a temperature of about 1900? C. or greater. An upper muffle extension is positioned above the muffle and defines a handle cavity. A downfeed handle is positioned within the handle cavity such that a gap is defined between an outer surface of the downfeed handle and an inner surface of the upper muffle extension. An upper heater is thermally coupled to the upper muffle extension and configured to heat the gap. A gas screen is positioned in the upper muffle extension and is configured to inject a process gas into the handle cavity.
FIBER OPTIC MANUFACTURING IN SPACE
Aspects of the embodiments include an optical fiber formed in a low gravity environment. The optical fiber can be used in airframe applications for missile defense, oil-field applications for down-well laser applications, optical communications, and other applications. The optical fiber can include a fluoride composition, such ZrF4-BaF2-LaF3-AlF3-NaF (ZBLAN), and can be characterized by an insertion loss in a range from 13 dB/1000 km to 120 dB/1000 km. The optical fiber can deliver optical energy with low insertion loss at the desired power and wavelength for the various applications.
Fiber optic manufacturing in space
Aspects of the embodiments are directed to systems and methods for forming an optical fiber in a low gravity environment, and an optical fiber formed in a low gravity environment. The system can include a preform holder configured to secure a preform; a heating element secured to a heating element stage and residing adjacent the preform holder; a heating element stage motor configured to move the heating element stage; a tension sensor; a spool; a spool tension motor coupled to the spool and configured to rotate the spool; and a control system communicably coupled to the heating element stage motor and the spool tension motor and configured to control the movement of the heating element stage based on a rotational speed of the spool. The optical fiber can include a fluoride composition, such ZrF4-BaF2-LaF3-AlF3-NaF (ZBLAN), and can be characterized by an insertion loss in a range from 13 dB/1000 km to 120 dB/1000 km.