C03C2201/3429

Doped bismuth silicate crystals via devitrification of glass forming liquids

This technology is directed to the preparation of doped-bismuth-silicate seed crystals through controlled crystallization (e.g. dimensionality of growth and nucleation mechanism) and the method of forming high purity single seed (particle size ranges from micrometers to millimeters) for various uses. These seed crystals have a nominal stoichiometry of Bi.sub.2-xA.sub.xSiO.sub.5, Bi.sub.2-xA.sub.xSi.sub.3O.sub.9, Bi.sub.4-xA.sub.xSi.sub.3O.sub.9, and Bi.sub.12-xA.sub.xSiO.sub.20, where A is a rare earth dopant selected from La, Ce, Nd, Pr, and/or Sm.

DOPED BISMUTH SILICATE CRYSTALS VIA DEVITRIFICATION OF GLASS FORMING LIQUIDS
20190284090 · 2019-09-19 ·

This technology is directed to the preparation of doped-bismuth-silicate seed crystals through controlled crystallization (e.g. dimensionality of growth and nucleation mechanism) and the method of forming high purity single seed (particle size ranges from micrometers to millimeters) for various uses. These seed crystals have a nominal stoichiometry of Bi.sub.2-xA.sub.xSiO.sub.5, Bi.sub.2-xA.sub.xSi.sub.3O.sub.9, Bi.sub.4-xA.sub.xSi.sub.3O.sub.9, and Bi.sub.12-xA.sub.xSiO.sub.20, where A is a rare earth dopant selected from La, Ce, Nd, Pr, and/or Sm.