C03C2201/3447

Wavelength conversion member, and light emitting device using same

Provided is a wavelength conversion member that is less decreased in luminescence intensity with time by irradiation with light of an LED or LD and a light emitting device using the wavelength conversion member. A wavelength conversion member is formed of an inorganic phosphor dispersed in a glass matrix, wherein the glass matrix contains, in % by mole, 30 to 85% SiO.sub.2, 0 to 20% B.sub.2O.sub.3, 0 to 25% Al.sub.2O.sub.3, 0 to 3% Li.sub.2O, 0 to 3% Na.sub.2O, 0 to 3% K.sub.2O, 0 to 3% Li.sub.2O+Na.sub.2O+K.sub.2O, 0 to 35% MgO, 0 to 35% CaO, 0 to 35% SrO, 0 to 35% BaO, 0.1 to 45% MgO+CaO+SrO+BaO, and 0 to 4% ZnO, and the inorganic phosphor is at least one selected from the group consisting of an oxide phosphor, a nitride phosphor, an oxynitride phosphor, a chloride phosphor, an oxychloride phosphor, a halide phosphor, an aluminate phosphor, and a halophosphate phosphor.

WAVELENGTH CONVERSION MEMBER, AND LIGHT EMITTING DEVICE USING SAME
20230159375 · 2023-05-25 ·

Provided is a wavelength conversion member that is less decreased in luminescence intensity with time by irradiation with light of an LED or LD and a light emitting device using the wavelength conversion member. A wavelength conversion member is formed of an inorganic phosphor dispersed in a glass matrix, wherein the glass matrix contains, in % by mole, 30 to 85% SiO.sub.2, 0 to 20% B.sub.2O.sub.3, 0 to 25% Al.sub.2O.sub.3, 0 to 3% Li.sub.2O, 0 to 3% Na.sub.2O, 0 to 3% K.sub.2O, 0 to 3% Li.sub.2O+Na.sub.2O+K.sub.2O, 0 to 35% MgO, 0 to 35% CaO, 0 to 35% SrO, 0 to 35% BaO, 0.1 to 45% MgO+CaO+SrO+BaO, and 0 to 4% ZnO, and the inorganic phosphor is at least one selected from the group consisting of an oxide phosphor, a nitride phosphor, an oxynitride phosphor, a chloride phosphor, an oxychloride phosphor, a halide phosphor, an aluminate phosphor, and a halophosphate phosphor.

Solarization resistant rare earth doped glasses

Substantially alkali free glasses are disclosed which can be used to produce substrates for flat panel display devices. The glasses can have a loading of fluorine and ceria to achieve exemplary solarization and UV protection attributes when exposed to UV radiation. Methods for producing substantially alkali free glasses using a float or downdraw process (e.g., a fusion downdraw process) are also disclosed.

WAVELENGTH CONVERSION MEMBER, AND LIGHT EMITTING DEVICE USING SAME
20210230047 · 2021-07-29 ·

Provided is a wavelength conversion member that is less decreased in luminescence intensity with time by irradiation with light of an LED or LD and a light emitting device using the wavelength conversion member. A wavelength conversion member is formed of an inorganic phosphor dispersed in a glass matrix, wherein the glass matrix contains, in % by mole, 30 to 85% SiO.sub.2, 0 to 20% B.sub.2O.sub.3, 0 to 25% Al.sub.2O.sub.3, 0 to 3% Li.sub.2O, 0 to 3% Na.sub.2O, 0 to 3% K.sub.2O, 0 to 3% Li.sub.2O+Na.sub.2O+K.sub.2O, 0 to 35% MgO, 0 to 35% CaO, 0 to 35% SrO, 0 to 35% BaO, 0.1 to 45% MgO+CaO+SrO+BaO, and 0 to 4% ZnO, and the inorganic phosphor is at least one selected from the group consisting of an oxide phosphor, a nitride phosphor, an oxynitride phosphor, a chloride phosphor, an oxychloride phosphor, a halide phosphor, an aluminate phosphor, and a halophosphate phosphor.

Wavelength conversion member, and light emitting device using same

Provided is a wavelength conversion member that is less decreased in luminescence intensity with time by irradiation with light of an LED or LD and a light emitting device using the wavelength conversion member. A wavelength conversion member is formed of an inorganic phosphor dispersed in a glass matrix, wherein the glass matrix contains, in % by mole, 30 to 85% SiO.sub.2, 0 to 20% B.sub.2O.sub.3, 0 to 25% Al.sub.2O.sub.3, 0 to 3% Li.sub.2O, 0 to 3% Na.sub.2O, 0 to 3% K.sub.2O, 0 to 3% Li.sub.2O+Na.sub.2O+K.sub.2O, 0 to 35% MgO, 0 to 35% CaO, 0 to 35% SrO, 0 to 35% BaO, 0.1 to 45% MgO+CaO+SrO+BaO, and 0 to 4% ZnO, and the inorganic phosphor is at least one selected from the group consisting of an oxide phosphor, a nitride phosphor, an oxynitride phosphor, a chloride phosphor, an oxychloride phosphor, a halide phosphor, an aluminate phosphor, and a halophosphate phosphor.

Wavelength conversion member, and light emitting device using same

Provided is a wavelength conversion member that is less decreased in luminescence intensity with time by irradiation with light of an LED or LD and a light emitting device using the wavelength conversion member. A wavelength conversion member is formed of an inorganic phosphor dispersed in a glass matrix, wherein the glass matrix contains, in % by mole, 30 to 85% SiO.sub.2, 0 to 20% B.sub.2O.sub.3, 0 to 25% Al.sub.2O.sub.3, 0 to 3% Li.sub.2O, 0 to 3% Na.sub.2O, 0 to 3% K.sub.2O, 0 to 3% Li.sub.2O+Na.sub.2O+K.sub.2O, 0 to 35% MgO, 0 to 35% CaO, 0 to 35% SrO, 0 to 35% BaO, 0.1 to 45% MgO+CaO+SrO+BaO, and 0 to 4% ZnO, and the inorganic phosphor is at least one selected from the group consisting of an oxide phosphor, a nitride phosphor, an oxynitride phosphor, a chloride phosphor, an oxychloride phosphor, a halide phosphor, an aluminate phosphor, and a halophosphate phosphor.

SOLARIZATION RESISTANT RARE EARTH DOPED GLASSES

Substantially alkali free glasses are disclosed which can be used to produce substrates for flat panel display devices. The glasses can have a loading of fluorine and ceria to achieve exemplary solarization and UV protection attributes when exposed to UV radiation. Methods for producing substantially alkali free glasses using a float or downdraw process (e.g., a fusion downdraw process) are also disclosed.

WAVELENGTH CONVERSION MEMBER, AND LIGHT EMITTING DEVICE USING SAME
20190119148 · 2019-04-25 ·

Provided is a wavelength conversion member that is less decreased in luminescence intensity with time by irradiation with light of an LED or LD and a light emitting device using the wavelength conversion member. A wavelength conversion member is formed of an inorganic phosphor dispersed in a glass matrix, wherein the glass matrix contains, in % by mole, 30 to 85% SiO.sub.2, 0 to 20% B.sub.2O.sub.3, 0 to 25% Al.sub.2O.sub.3, 0 to 3% Li.sub.2O, 0 to 3% Na.sub.2O, 0 to 3% K.sub.2O, 0 to 3% Li.sub.2O+Na.sub.2O+K.sub.2O, 0 to 35% MgO, 0 to 35% CaO, 0 to 35% SrO, 0 to 35% BaO, 0.1 to 45% MgO+CaO+SrO+BaO, and 0 to 4% ZnO, and the inorganic phosphor is at least one selected from the group consisting of an oxide phosphor, a nitride phosphor, an oxynitride phosphor, a chloride phosphor, an oxychloride phosphor, a halide phosphor, an aluminate phosphor, and a halophosphoric acid chloride phosphor.