Patent classifications
C03C25/1062
STRUCTURES IN OPTICAL DEVICES HAVING GRAPHENE AND MANUFACTURING METHOD FOR THE SAME
The present disclosure discloses an optical device structure including an optical fiber including a core part, a clad part, and a three-dimensional micro hole structure in the clad part, wherein a surface of the three-dimensional micro hole structure is provided with at least a non-flat surface, and a conformal graphene layer is formed on the surface of the three-dimensional micro hole structure, and a method of manufacturing the same.
PHOTONIC CRYSTAL FIBER, A METHOD OF PRODUCTION THEREOF AND A SUPERCONTINUUM LIGHT SOURCE
The invention concerns a Photonic Crystal Fiber (PCF) a method of its production and a supercontinuum light source comprising such PCF. The PCF has a longitudinal axis and comprises a core extending along the length of said longitudinal axis and a cladding region surrounding the core. At least the cladding region comprises a plurality of microstructures in the form of inclusions extending along the longitudinal axis of the PCF in at least a microstructured length section. In at least a degradation resistant length section of the microstructured length section the PCF comprises hydrogen and/or deuterium. In at least the degradation resistant length section the PCF further comprises a main coating surrounding the cladding region, which main coating is hermetic for the hydrogen and/or deuterium at a temperature below Th, wherein Th is at least about 50° C., preferably 50° C.<Th<250° C.
Fiber Bragg gratings in carbon-coated optical fibers and techniques for making same
A technique is described for fabricating one or more optical devices in a carbon-coated optical fiber. A photosensitive optical fiber is provided having a hermetic carbon coating. Further provided is a laser having a beam output that is configured to inscribe one or more refractive index modulations into the optical fiber through the hermetic carbon layer while leaving the hermetic carbon layer intact. The laser is used to inscribe one or more optical devices into the optical fiber through the hermetic carbon layer.
High-density optical fiber ribbon with cladding-strengthened glass optical fibers in a common protective coating and fiber ribbon interconnects employing same
A high-density optical fiber ribbon is formed by two or more cladding-strengthened glass optical fibers each having an outer surface and that do not individually include a protective polymer coating. A common protective coating substantially surrounds the outer surfaces of the two or more cladding-strengthened glass optical fibers so that the common protective coating is common to the two or more cladding-strengthened glass optical fibers. A fiber ribbon cable is formed by adding a cover assembly to the fiber ribbon. A fiber ribbon interconnect is formed adding one or more optical connectors to the fiber ribbon or fiber ribbon cable. Optical data transmission systems that employ the fiber ribbon to optically connect to a photonic device are also disclosed. Methods of forming the cladding-strengthened glass optical fibers and the high-density optical fiber ribbons are also disclosed.
Photonic crystal fiber, a method of production thereof and a supercontinuum light source
A Photonic Crystal Fiber (PCF) a method of its production and a supercontinuum light source comprising such PCF. The PCF has a longitudinal axis and includes a core extending along the length of said longitudinal axis and a cladding region surrounding the core. At least the cladding region includes a plurality of microstructures in the form of inclusions extending along the longitudinal axis of the PCF in at least a microstructured length section. In at least a degradation resistant length section of the microstructured length section the PCF includes hydrogen and/or deuterium. In at least the degradation resistant length section the PCF further includes a main coating surrounding the cladding region, which main coating is hermetic for the hydrogen and/or deuterium at a temperature below T.sub.h, wherein T.sub.h is at least about 50° C., preferably 50° C.<T.sub.h<250° C.
Structures in optical devices having graphene and manufacturing method for the same
The present disclosure discloses an optical device structure including an optical fiber including a core part, a clad part, and a three-dimensional micro hole structure in the clad part, wherein a surface of the three-dimensional micro hole structure is provided with at least a non-flat surface, and a conformal graphene layer is formed on the surface of the three-dimensional micro hole structure, and a method of manufacturing the same.
PHOTONIC CRYSTAL FIBER, A METHOD OF PRODUCTION THEREOF AND A SUPERCONTINUUM LIGHT SOURCE
A Photonic Crystal Fiber (PCF) a method of its production and a supercontinuum light source comprising such PCF. The PCF has a longitudinal axis and includes a core extending along the length of said longitudinal axis and a cladding region surrounding the core. At least the cladding region includes a plurality of microstructures in the form of inclusions extending along the longitudinal axis of the PCF in at least a microstructured length section. In at least a degradation resistant length section of the microstructured length section the PCF includes hydrogen and/or deuterium. In at least the degradation resistant length section the PCF further includes a main coating surrounding the cladding region, which main coating is hermetic for the hydrogen and/or deuterium at a temperature below T.sub.h, wherein Th is at least about 50° C., preferably 50° C.<Th.sub.h<250° C.
Photonic crystal fiber, a method of production thereof and a supercontinuum light source
A Photonic Crystal Fiber (PCF) a method of its production and a supercontinuum light source comprising such PCF. The PCF has a longitudinal axis and includes a core extending along the length of said longitudinal axis and a cladding region surrounding the core. At least the cladding region includes a plurality of microstructures in the form of inclusions extending along the longitudinal axis of the PCF in at least a microstructured length section. In at least a degradation resistant length section of the microstructured length section the PCF includes hydrogen and/or deuterium. In at least the degradation resistant length section the PCF further includes a main coating surrounding the cladding region, which main coating is hermetic for the hydrogen and/or deuterium at a temperature below T.sub.h, wherein T.sub.h is at least about 50° C., preferably 50° C.<T.sub.h<250° C.
PHOTONIC CRYSTAL FIBER, A METHOD OF PRODUCTION THEREOF AND A SUPERCONTINUUM LIGHT SOURCE
A Photonic Crystal Fiber (PCF) a method of its production and a supercontinuum light source comprising such PCF. The PCF has a longitudinal axis and includes a core extending along the length of said longitudinal axis and a cladding region surrounding the core. At least the cladding region includes a plurality of microstructures in the form of inclusions extending along the longitudinal axis of the PCF in at least a microstructured length section. In at least a degradation resistant length section of the microstructured length section the PCF includes hydrogen and/or deuterium. In at least the degradation resistant length section the PCF further includes a main coating surrounding the cladding region, which main coating is hermetic for the hydrogen and/or deuterium at a temperature below T.sub.h, wherein T.sub.h is at least about 50° C., preferably 50° C.<T.sub.h<250° C.
Photonic crystal fiber, a method of production thereof and a supercontinuum light source
A Photonic Crystal Fiber (PCF) a method of its production and a supercontinuum light source comprising such PCF. The PCF has a longitudinal axis and includes a core extending along the length of said longitudinal axis and a cladding region surrounding the core. At least the cladding region includes a plurality of microstructures in the form of inclusions extending along the longitudinal axis of the PCF in at least a microstructured length section. In at least a degradation resistant length section of the microstructured length section the PCF includes hydrogen and/or deuterium. In at least the degradation resistant length section the PCF further includes a main coating surrounding the cladding region, which main coating is hermetic for the hydrogen and/or deuterium at a temperature below T.sub.h, wherein T.sub.h is at least about 50 C., preferably 50 C.<T.sub.h<250 C.