C03C3/12

Sealed devices comprising transparent laser weld regions

Disclosed herein are sealed devices comprising a first substrate, a second substrate, an inorganic film between the first and second substrates, and at least one weld region comprising a bond between the first and second substrates. The weld region can comprise a chemical composition different from that of the inorganic film and the first or second substrates. The sealed devices may further comprise a stress region encompassing at least the weld region, in which a portion of the device is under a greater stress than the remaining portion of the device. Also disclosed herein are display and electronic components comprising such sealed devices.

Sealed devices comprising transparent laser weld regions

Disclosed herein are sealed devices comprising a first substrate, a second substrate, an inorganic film between the first and second substrates, and at least one weld region comprising a bond between the first and second substrates. The weld region can comprise a chemical composition different from that of the inorganic film and the first or second substrates. The sealed devices may further comprise a stress region encompassing at least the weld region, in which a portion of the device is under a greater stress than the remaining portion of the device. Also disclosed herein are display and electronic components comprising such sealed devices.

Low LOI tellurium-lithium-silicon-zirconium frit system and conductive paste and application thereof

The present disclosure discloses a low LOI tellurium-lithium-silicon-zirconium frit system and a conductive paste and application thereof, and belongs to the field of conductive paste. In the low LOI tellurium-lithium-silicon-zirconium frit system, components of the frit are 24%-40% TeO.sub.2, 18%-24% Li.sub.2O, 4%-13% SiO.sub.2, 0-2% ZrO.sub.2, and a balance MO.sub.x, and M is one or a mixture of Na, K, Mg, Ca, Sr, Ti, V, Cr, Mo, W, Mn, Cu, Ag, Zn, Cd, B, Al, Ga, Tl, Ge, Pb, P, and Bi. There is no need to add additional surfactants, a viscosity change of the conductive paste prepared after standing for 30 days is less than 20%, the conductive paste has good stability, the water related weight loss of inorganic oxide of the conductive paste is less than 1.6%, and the application performance of the conductive paste is not affected after standing for 30 days.

Method for preparing all-solid-state photonic crystal fiber preforms by extrusion

A method for preparing all-solid-state photonic crystal fiber preform by extrusion by aligning the center of the first jacking end of the first jacking rod with the center of the core outlet mold. The adverse effect on this part of extruded core glass by oxygen or other impurities in air during the extrusion out of the core outlets can be avoided. The defects on the core glass surface and the cladding glass surface can be effectively removed, and the purity and quality of the core component in the obtained fiber preform can be improved.

Method for preparing all-solid-state photonic crystal fiber preforms by extrusion

A method for preparing all-solid-state photonic crystal fiber preform by extrusion by aligning the center of the first jacking end of the first jacking rod with the center of the core outlet mold. The adverse effect on this part of extruded core glass by oxygen or other impurities in air during the extrusion out of the core outlets can be avoided. The defects on the core glass surface and the cladding glass surface can be effectively removed, and the purity and quality of the core component in the obtained fiber preform can be improved.

GLASS COMPOSITION AND SEALING MATERIAL
20230059274 · 2023-02-23 ·

Provided are a glass composition capable of sealing through low-temperature firing without containing environmentally harmful lead, and a sealing material using the same. The glass composition includes, in terms of mol %, 1%, to 30% of MgO+CaO+SrO+BaO+ZnO, 30% to 80% of TeO.sub.2, and 5% to 30% of MoO.sub.3.

FLEXIBLE AND TUNABLE INFRARED EMISSIVITY MATERIAL PLATFORM

A material platform with controllable emissivity and fabrication methods are provided that permit the manipulation of thermal radiation detection and IR signal modulation and can be adapted to a variety of uses including infrared camouflage, thermal IR decoys, thermo-reflectance imaging and IR signal modulation. The platform is a multilayer W.sub.xV.sub.1-xO.sub.2 film with different W doping levels (x values) and layer thicknesses, forming a graded W-doped construct. In WVO.sub.2 films with a total thickness <100 nm, the graded doping of W spreads the originally sharp metal-insulator phase transition (MIT) to a broad temperature range, greatly expanding the temperature window for emissivity modulation.

Scratch resistant glass and method of making

Glass-based articles comprise stress profiles providing improved scratch resistance. A glass-based article comprises a lithium aluminosilicate composition and a molar ratio of potassium oxide (K.sub.2O) to sodium oxide (Na.sub.2O) averaged over a distance from the surface to a depth of 0.4 micrometers that is greater than or equal to 0 and less than or equal to 1.8. The article comprises sodium having a non-zero varying concentration extending from a surface of the glass-based article to a depth of the glass-based article and a spike depth of layer that is greater than or equal to 4 micrometers and less than or equal to 8 micrometers. The article may comprise an average compressive stress of greater than or equal to 150 MPa over a depth from 15 micrometers to 40 micrometers.

Transparent, near infrared-shielding glass ceramic

Optically transparent glass ceramic materials comprising a glass phase containing and a crystalline tungsten bronze phase comprising nanoparticles and having the formula M.sub.xWO.sub.3, where M includes at least one H, Li, Na, K, Rb, Cs, Ca, Sr, Ba, Zn, Cu, Ag, Sn, Cd, In, Tl, Pb, Bi, Th, La, Pr, Nd, Sm, Eu, Gd, Dy, Ho, Er, Tm, Yb, Lu, and U, and where 0<x<1. Aluminosilicate and zinc-bismuth-borate glasses comprising at least one of Sm.sub.2O.sub.3, Pr.sub.2O.sub.3, and Er.sub.2O.sub.3 are also provided.

TRANSPARENT ANTIVIRAL/ANTIMICROBIAL COATING
20230112638 · 2023-04-13 ·

The present disclosure concerns copper coatings on glass with a thickness of about 8 to 10 nm to maintain high levels of transparency. In some aspects, the coatings are of copper, copper (I) oxide, and/or copper (II) oxide. In some aspects, the copper coatings as set forth herein provide an antiviral and/or antimicrobial surface for safer touch-screen devices.