ANTI-CORROSIVE CONCRETE GROUTING MATERIAL FOR COASTAL STRUCTURE CONNECTION AND METHOD FOR PREPARING THE SAME

An anti-corrosive concrete grouting material for coastal structure connection and a method for preparing the same, belonging to the technical field of anti-corrosion of coastal assembled structure connectors. The grouting material includes the following components: expansible compound cement, slag sand, fly ash (FA), polyvinyl alcohol (PVA) (containing an oxidant and a catalyst), graphene oxide (GO), a water reducer, an adjusting admixture, a defoaming agent, a mineral admixture and water. A shrinkage-free effect of the grouting material is realized through internal curing of GO-PVA hydrogel, micro-expansion of the compound cement and shrinkage reduction effect of the FA; an energy storage effect of a GO-PVA hydrogel micro-capacitor is exerted to avoid formation of a reinforcement corrosion micro-battery in a grouting material sleeve, a reinforcement corrosion self-immune effect is achieved, seawater corrosion resistance of the grouting material is improved by the slag sand, and it has huge economic and environmental protection benefits.

ANTI-CORROSIVE CONCRETE GROUTING MATERIAL FOR COASTAL STRUCTURE CONNECTION AND METHOD FOR PREPARING THE SAME

An anti-corrosive concrete grouting material for coastal structure connection and a method for preparing the same, belonging to the technical field of anti-corrosion of coastal assembled structure connectors. The grouting material includes the following components: expansible compound cement, slag sand, fly ash (FA), polyvinyl alcohol (PVA) (containing an oxidant and a catalyst), graphene oxide (GO), a water reducer, an adjusting admixture, a defoaming agent, a mineral admixture and water. A shrinkage-free effect of the grouting material is realized through internal curing of GO-PVA hydrogel, micro-expansion of the compound cement and shrinkage reduction effect of the FA; an energy storage effect of a GO-PVA hydrogel micro-capacitor is exerted to avoid formation of a reinforcement corrosion micro-battery in a grouting material sleeve, a reinforcement corrosion self-immune effect is achieved, seawater corrosion resistance of the grouting material is improved by the slag sand, and it has huge economic and environmental protection benefits.

CEMENTITIOUS COMPOSITIONS COMPRISING OXIDATIVELY DEGRADED POLYSACCHARIDE AS WATER REDUCING AGENTS
20220185733 · 2022-06-16 · ·

Cementitious compositions have an oxidatively degraded polysaccharide as a water reducing agent to provide similar water reducing properties to cementitious composition formulated with lignosulfonates. The oxidatively degraded polysaccharides have the advantage over lignosulfonates of a lower price and a more consistent quality and are expected to be compatible with polycarboxylatether cement additives. Further, methods for the preparation of corresponding cementitious compositions, appropriate oxidatively degraded polysaccharides and methods for producing the same, as well as the use of oxidatively degraded polysaccharides as water reducing agents in cementitious compositions.

NON-HYDRATION STRENGTH IN CEMENTITIOUS COMPOSITIONS

Described are compositions and methods for controlled strength development in a hydratable cementitious material, and more particularly to the use of polymerizable monomer components, which are initiated and activated by a redox pair which are mixed in controlled fashion, for enhancing non-hydration strength within the matrix of the plastic hydratable cementitious material before setting of the cementitious material begins. Exemplary applications include minimizing pressures on formwork for high fluid ready-mix applications, enhancing support and bonding properties for integrated concrete slab work and other sequential applications, or facilitating speedy 3D printing applications, among other unique possibilities.

NON-HYDRATION STRENGTH IN CEMENTITIOUS COMPOSITIONS

Described are compositions and methods for controlled strength development in a hydratable cementitious material, and more particularly to the use of polymerizable monomer components, which are initiated and activated by a redox pair which are mixed in controlled fashion, for enhancing non-hydration strength within the matrix of the plastic hydratable cementitious material before setting of the cementitious material begins. Exemplary applications include minimizing pressures on formwork for high fluid ready-mix applications, enhancing support and bonding properties for integrated concrete slab work and other sequential applications, or facilitating speedy 3D printing applications, among other unique possibilities.

CEMENTITIOUS COMPOSITIONS COMPRISING OXIDATIVELY DEGRADED POLYSACCHARIDE AS WATER REDUCING AGENTS
20230322620 · 2023-10-12 · ·

Cementitious compositions and methods for the preparation of corresponding cementitious compositions, appropriate oxidatively degraded polysaccharides and methods for producing the same, as well as the use of oxidatively degraded polysaccharides as water reducing agents in cementitious compositions, wherein the compositions include an oxidatively degraded polysaccharide as a water reducing agent to provide similar water reducing properties to cementitious composition formulated with lignosulfonates. The oxidatively degraded polysaccharides have the advantage over lignosulfonates of a lower price and a more consistent quality and are expected to be compatible with polycarboxylatether cement additives.

Method for defoaming cementitious compositions using polyamine oxides
11148975 · 2021-10-19 ·

The present invention provides a composition and method for controlling air voids in aqueous systems such as paints, coatings, sealants, adhesives, mastics, cements, mortar, masonry, or concrete, which comprises the reaction product of an oxidizing agent and a compound comprising at least one polyalkoxylated polyalkylene polyamine, at least one polyalkyoxylated polyethyleneimine, or a mixture thereof.

Method for defoaming cementitious compositions using polyamine oxides
11148975 · 2021-10-19 ·

The present invention provides a composition and method for controlling air voids in aqueous systems such as paints, coatings, sealants, adhesives, mastics, cements, mortar, masonry, or concrete, which comprises the reaction product of an oxidizing agent and a compound comprising at least one polyalkoxylated polyalkylene polyamine, at least one polyalkyoxylated polyethyleneimine, or a mixture thereof.

Polyalkoxylated polyamine oxide defoaming compositions

The present invention provides a composition and method for controlling air voids in aqueous systems such as paints, coatings, sealants, adhesives, mastics, cements, mortar, masonry, or concrete, which comprises the reaction product of an oxidizing agent and a compound comprising at least one polyalkoxylated polyalkylene polyamine, at least one polyalkyoxylated polyethyleneimine, or a mixture thereof.

Polyalkoxylated polyamine oxide defoaming compositions

The present invention provides a composition and method for controlling air voids in aqueous systems such as paints, coatings, sealants, adhesives, mastics, cements, mortar, masonry, or concrete, which comprises the reaction product of an oxidizing agent and a compound comprising at least one polyalkoxylated polyalkylene polyamine, at least one polyalkyoxylated polyethyleneimine, or a mixture thereof.