C04B41/63

METHOD OF PREPARING SUPERHYDROPHOBIC ASPHALT

A superhydrophobic asphalt and a method of its preparation. The superhydrophobic asphalt contains an asphalt layer containing a polymer modified asphalt, preferably a radial SBS modified asphalt, and a polypropylene layer. The polypropylene layer comprises granules of polypropylene thermally fused to the asphalt layer. The superhydrophobic asphalt has a water contact angle of 145 to 170°, above the classification threshold for superhydrophobicity. The method of preparing the superhydrophobic asphalt involves distributing polypropylene granules over the surface of a polymer modified asphalt and curing below the melting temperature of the polypropylene. The asphalt may find use in waterproofing applications such as roofing.

METHOD OF PREPARING SUPERHYDROPHOBIC ASPHALT

A superhydrophobic asphalt and a method of its preparation. The superhydrophobic asphalt contains an asphalt layer containing a polymer modified asphalt, preferably a radial SBS modified asphalt, and a polypropylene layer. The polypropylene layer comprises granules of polypropylene thermally fused to the asphalt layer. The superhydrophobic asphalt has a water contact angle of 145 to 170°, above the classification threshold for superhydrophobicity. The method of preparing the superhydrophobic asphalt involves distributing polypropylene granules over the surface of a polymer modified asphalt and curing below the melting temperature of the polypropylene. The asphalt may find use in waterproofing applications such as roofing.

Chemically reactive surface-applied waterproofing for post-construction materials

Post-construction materials, including concrete, containing water insoluble polymers are disclosed herein. The water insoluble polymers are formed beneath the surface of the post-construction material using a first composition comprising a blend of fatty acid salts and a second composition comprising alkaline earth metal halides or alkaline earth metal carbonates.

Chemically reactive surface-applied waterproofing for post-construction materials

Post-construction materials, including concrete, containing water insoluble polymers are disclosed herein. The water insoluble polymers are formed beneath the surface of the post-construction material using a first composition comprising a blend of fatty acid salts and a second composition comprising alkaline earth metal halides or alkaline earth metal carbonates.

Coloured fiber cement products and methods for the production thereof

The present invention relates to coloured fiber cement products as well as to methods for manufacturing such products. In particular, the present invention provides coloured fiber cement products, which fiber cement products are coloured in the mass, and at least comprise on at least part of their outer surface one or more cured layers of a coating composition, which composition at least comprises a binder and a pigment and/or a filler and is characterized by a pigment volume concentration (PVC) of between about 1% and about 20%. The present invention further provides processes for producing these coloured fiber cement products. Finally, the present invention provides uses of the coloured fiber cement products as building materials. In particular embodiments, the fiber cement products produced by the processes of the present invention can be used to provide an outer surface to walls, both internal as well as external, a building or construction, e.g. as fagade plate, siding, etc.

Coloured fiber cement products and methods for the production thereof

The present invention relates to coloured fiber cement products as well as to methods for manufacturing such products. In particular, the present invention provides coloured fiber cement products, which fiber cement products are coloured in the mass, and at least comprise on at least part of their outer surface one or more cured layers of a coating composition, which composition at least comprises a binder and a pigment and/or a filler and is characterized by a pigment volume concentration (PVC) of between about 1% and about 20%. The present invention further provides processes for producing these coloured fiber cement products. Finally, the present invention provides uses of the coloured fiber cement products as building materials. In particular embodiments, the fiber cement products produced by the processes of the present invention can be used to provide an outer surface to walls, both internal as well as external, a building or construction, e.g. as fagade plate, siding, etc.

WATERBORNE WET LOOK COATING COMPOSITION

A water-based coating composition is described herein. The composition includes an aqueous dispersion derived from an ethylenically unsaturated monomer and one or more organic solvents. The composition when applied to a substrate and allowed to dry provides a wet look to the substrate.

MOLD AND MILDEW RESISTANT WALLBOARD

A wallboard product and a method of making a wallboard product are provided. The method may include providing a wallboard core. And exterior surface may be provided to the wallboard core. The exterior surface may include a magnesium compound.

MOLD AND MILDEW RESISTANT WALLBOARD

A wallboard product and a method of making a wallboard product are provided. The method may include providing a wallboard core. And exterior surface may be provided to the wallboard core. The exterior surface may include a magnesium compound.

METHOD FOR PRODUCING A CEMENTITIOUS BOARD, APPARATUS FOR PRODUCING A CEMENTITIOUS BOARD, AND CEMENTITIOUS BOARD

Method for producing a cementitious board (1), wherein a first liner (2) with first overlap sections (5) is provided and furnished with at least one layer of at least one slurry comprising a cementitious material (3); a second liner (4) with second overlap sections (8) is provided and arranged such that it contacts the first overlap sections (5) of the first liner (2), wherein the at least one layer of the at least one slurry (3) is arranged between the first liner (2) and the second liner (4); an adhesive foam (6) is provided at least partly on at least one of the first or second overlap sections (5, 8); and the first liner (2) and the second liner (4) are bonded via the adhesive foam (6) in the overlap sections (5, 8).