Patent classifications
C08F4/603
Method of making an olefin polymerization catalyst activator
A method for preparing ammonium tetrakis(pentafluorophenyl)borate salt comprising reacting a secondary amine with an aldehyde to form an iminium ion; hydrogenating the iminium ion by reaction with a reducing agent to form a tertiary amine; reacting the tertiary amine with a mineral acid to form an amine salt; and reacting the amine salt with K[B(C.sub.6F.sub.5).sub.4], Li[B(C.sub.6F.sub.5).sub.4], or combinations thereof to form an ammonium tetrakis(pentafluorophenyl)borate salt, wherein the secondary amine is derived from a non-animal source and the aldehyde has seven or more carbon atoms; wherein the ammonium tetrakis(pentafluorophenyl)borate salt is characterized by a solubility at 25 C. in hexane, cyclohexane or methylcyclohexane of at least 10 weight percent; and wherein the tertiary amine has a molecular weight of at least 450 g/mole is provided.
Method of making an olefin polymerization catalyst activator
A method for preparing ammonium tetrakis(pentafluorophenyl)borate salt comprising reacting a secondary amine with an aldehyde to form an iminium ion; hydrogenating the iminium ion by reaction with a reducing agent to form a tertiary amine; reacting the tertiary amine with a mineral acid to form an amine salt; and reacting the amine salt with K[B(C.sub.6F.sub.5).sub.4], Li[B(C.sub.6F.sub.5).sub.4], or combinations thereof to form an ammonium tetrakis(pentafluorophenyl)borate salt, wherein the secondary amine is derived from a non-animal source and the aldehyde has seven or more carbon atoms; wherein the ammonium tetrakis(pentafluorophenyl)borate salt is characterized by a solubility at 25 C. in hexane, cyclohexane or methylcyclohexane of at least 10 weight percent; and wherein the tertiary amine has a molecular weight of at least 450 g/mole is provided.
Reinforcement of a chromium/silica catalyst with silicate oligomers
Methods for reinforcing chromium catalysts by the deposition of additional silica are disclosed herein. The resultant silica-reinforced chromium supported catalysts can be used to polymerize olefins to produce, for example, ethylene based homopolymers and copolymers with higher molecular weights and additional long chain branching.
METHOD OF MAKING AN OLEFIN POLYMERIZATION CATALYST ACTIVATOR
A method for preparing ammonium tetrakis(pentafluorophenyl)borate salt comprising reacting a secondary amine with an aldehyde to form an iminium ion; hydrogenating the iminium ion by reaction with a reducing agent to form a tertiary amine; reacting the tertiary amine with a mineral acid to form an amine salt; and reacting the amine salt with K[B(C.sub.6F.sub.5).sub.4], Li[B(C.sub.6F.sub.5).sub.4], or combinations thereof to form an ammonium tetrakis(pentafluorophenyl)borate salt, wherein the secondary amine is derived from a non-animal source and the aldehyde has seven or more carbon atoms; wherein the ammonium tetrakis(pentafluorophenyl)borate salt is characterized by a solubility at 25 C. in hexane, cyclohexane or methylcyclohexane of at least 10 weight percent; and wherein the tertiary amine has a molecular weight of at least 450 g/mole is provided.
METHOD OF MAKING AN OLEFIN POLYMERIZATION CATALYST ACTIVATOR
A method for preparing ammonium tetrakis(pentafluorophenyl)borate salt comprising reacting a secondary amine with an aldehyde to form an iminium ion; hydrogenating the iminium ion by reaction with a reducing agent to form a tertiary amine; reacting the tertiary amine with a mineral acid to form an amine salt; and reacting the amine salt with K[B(C.sub.6F.sub.5).sub.4], Li[B(C.sub.6F.sub.5).sub.4], or combinations thereof to form an ammonium tetrakis(pentafluorophenyl)borate salt, wherein the secondary amine is derived from a non-animal source and the aldehyde has seven or more carbon atoms; wherein the ammonium tetrakis(pentafluorophenyl)borate salt is characterized by a solubility at 25 C. in hexane, cyclohexane or methylcyclohexane of at least 10 weight percent; and wherein the tertiary amine has a molecular weight of at least 450 g/mole is provided.
Method of making an olefin polymerization catalyst activator
A method for preparing ammonium tetrakis(pentafluorophenyl)borate salt comprising reacting a secondary amine with an aldehyde to form an iminium ion; hydrogenating the iminium ion by reaction with a reducing agent to form a tertiary amine; reacting the tertiary amine with a mineral acid to form an amine salt; and reacting the amine salt with K[B(C.sub.6F.sub.5).sub.4], Li[B(C.sub.6F.sub.5).sub.4], or combinations thereof to form an ammonium tetrakis(pentafluorophenyl)borate salt, wherein the secondary amine is derived from a non-animal source and the aldehyde has seven or more carbon atoms; wherein the ammonium tetrakis(pentafluorophenyl)borate salt is characterized by a solubility at 25 C. in hexane, cyclohexane or methylcyclohexane of at least 10 weight percent; and wherein the tertiary amine has a molecular weight of at least 450 g/mole is provided.
Method of making an olefin polymerization catalyst activator
A method for preparing ammonium tetrakis(pentafluorophenyl)borate salt comprising reacting a secondary amine with an aldehyde to form an iminium ion; hydrogenating the iminium ion by reaction with a reducing agent to form a tertiary amine; reacting the tertiary amine with a mineral acid to form an amine salt; and reacting the amine salt with K[B(C.sub.6F.sub.5).sub.4], Li[B(C.sub.6F.sub.5).sub.4], or combinations thereof to form an ammonium tetrakis(pentafluorophenyl)borate salt, wherein the secondary amine is derived from a non-animal source and the aldehyde has seven or more carbon atoms; wherein the ammonium tetrakis(pentafluorophenyl)borate salt is characterized by a solubility at 25 C. in hexane, cyclohexane or methylcyclohexane of at least 10 weight percent; and wherein the tertiary amine has a molecular weight of at least 450 g/mole is provided.