C10G25/03

PROCESS FOR PREPARING A MOLDING COMPRISING A ZEOLITE CATALYST AND METHOD FOR CONVERTING OXYGENATES TO OLEFINS USING THE CATALYTIC MOLDING

The present invention relates to a process for preparing a molding comprising a zeolitic material and one or more oxidic binders, the process particularly comprising preparing a mixture of a zeolitic material, such as Mg-ZSM-5, a source of an oxidic binder, and a first plasticizer; admixing an acid to said mixture; and shaping of the mixture, to obtain a precursor of a molding; wherein in said mixture a specific weight ratio of the source of the oxidic binder to the sum of the zeolitic material and the source of the oxidic binder is applied. Further, the present invention relates to a molding obtainable or obtained by the inventive process, and to a molding itself displaying in particular a comparatively improved crush strength. Yet further, the present invention relates to a method for the conversion of oxygenates to olefins and to a use of the inventive molding.

DLM-1 Molecular Sieve, Process for Preparing the Same, and Use Thereof
20230025198 · 2023-01-26 ·

A DLM-1 molecular sieve, a process for preparing the molecular sieve, and use thereof in treating an organic substance are provided. The DLM-1 molecular sieve is an Al-SBA-15 molecular sieve, and has a schematic chemical composition as represented by the formula “first oxide*second oxide”. The first oxide is silica, the second oxide is alumina, and the content by mass percent of alumina in the schematic chemical composition is 2% to 85%. The DLM-1 molecular sieve is suitable for the hydrodenitrogenation reaction of heavy distillate oil, and is favorable for improving the hydrodenitrogenation activity.

ADSORPTIVE PROCESS FOR SEPARATION OF ISOPARAFFINIC LUBE BASE STOCK FROM LOWER QUALITY OILS

Provided herein are methods and systems of making a high quality isoparaffinic base stock which include contacting an adsorbent material with a hydrocarbon feedstock and a solvent and separating at least some of the one or more high VI components from the hydrocarbon feedstock to produce a first fraction base stock having a first fraction base stock viscosity index. The adsorbent material is desorbed with a second solvent to produce a second fraction base stock having a second fraction base stock viscosity index. In these methods, the first fraction base stock viscosity index is less than the hydrocarbon feedstock viscosity index and the second fraction base stock viscosity index is greater than the hydrocarbon feedstock viscosity index.

ADSORPTIVE PROCESS FOR SEPARATION OF ISOPARAFFINIC LUBE BASE STOCK FROM LOWER QUALITY OILS

Provided herein are methods and systems of making a high quality isoparaffinic base stock which include contacting an adsorbent material with a hydrocarbon feedstock and a solvent and separating at least some of the one or more high VI components from the hydrocarbon feedstock to produce a first fraction base stock having a first fraction base stock viscosity index. The adsorbent material is desorbed with a second solvent to produce a second fraction base stock having a second fraction base stock viscosity index. In these methods, the first fraction base stock viscosity index is less than the hydrocarbon feedstock viscosity index and the second fraction base stock viscosity index is greater than the hydrocarbon feedstock viscosity index.

Form of copper sulfide

Copper sulfide of the formula Cu.sub.xS.sub.y, wherein x and y are integer or non-integer values, wherein (i) the copper sulfide has a sulfur 2p XPS spectrum with peaks at 162.3 eV (±1 ev), 163.8 eV (±1 ev) and 68.5 eV (±1 ev), characterised in that the peak at 168.5 eV has a lower value of counts per second (CPS) than both the peak at 162.3 eV and the peak at 163.8 eV; and (ii) the copper sulfide has a copper 2p XPS spectrum with peaks at 932.0 eV (±2 ev) and 933.6 eV (±3 eV) and characterised in that the XPS spectrum does not comprise identifiable satellite peaks at 939.8 eV and 943.1 eV (±3 eV).

Form of copper sulfide

Copper sulfide of the formula Cu.sub.xS.sub.y, wherein x and y are integer or non-integer values, wherein (i) the copper sulfide has a sulfur 2p XPS spectrum with peaks at 162.3 eV (±1 ev), 163.8 eV (±1 ev) and 68.5 eV (±1 ev), characterised in that the peak at 168.5 eV has a lower value of counts per second (CPS) than both the peak at 162.3 eV and the peak at 163.8 eV; and (ii) the copper sulfide has a copper 2p XPS spectrum with peaks at 932.0 eV (±2 ev) and 933.6 eV (±3 eV) and characterised in that the XPS spectrum does not comprise identifiable satellite peaks at 939.8 eV and 943.1 eV (±3 eV).

PROCESS FOR INCREASING THE CONCENTRATION OF NORMAL PARAFFINS IN A LIGHT NAPHTHA STREAM

A process increases the concentration of normal paraffins in a feed stream comprising separating a naphtha feed stream into a normal paraffin rich stream and a non-normal paraffin rich stream. A naphtha feed stream may be separated into a normal paraffin stream and a non-normal paraffin stream. An isomerization feed stream is taken from the non-normal paraffin stream and isomerized over an isomerization catalyst to convert non-normal paraffins to normal paraffins and produce an isomerization effluent stream. The isomerization effluent stream may be separated into a propane stream and a C4+ hydrocarbon stream optionally in a single column. The C4+ hydrocarbon stream may be recycled to the step of separating a naphtha feed stream.

Conversion of aromatic complex bottoms to useful products in an integrated refinery process

Systems and integrated methods are disclosed for processing aromatic complex bottoms into high value products. The system includes an adsorption column, the adsorption column in fluid communication with an aromatics complex and operable to receive and remove polyaromatics from an aromatic bottoms stream. The adsorption column producing a cleaned aromatic bottoms stream with reduced polyaromatic content and a reject stream including the removed polyaromatics. In some embodiments, the reject stream is recycled for further processing, passed to a coke production unit to produce high quality coke, or both.

Method of Producing Lubricating Base Oil from Atmospheric Residue in Pyrolysis Oil Derived from Waste Plastic

Provided are a method of producing a lubricating base oil composition including a) reacting at least a part of waste plastic pyrolysis oil having a boiling point in a range higher than 340° C. to remove impurities and structurally isomerizing the oil; and b) hydroisomerizing at least a part of the product of step a), and a lubricating base oil composition produced therefrom. A lubricating base oil, which has more methyl branches than petroleum-based lubricating base oil, to have improved low-temperature properties may be provided.

Method of Producing Lube Base Oil from Middle Distillate in Pyrolysis Oil Derived from Waste Plastic

Provided are a method of producing a Lube base oil composition including a) reacting at least a part of waste plastic pyrolysis oil having a boiling point in a range of 180 to 340° C. to remove impurities and oligomerize the oil; and b) hydroisomerizing at least a part of the product of step a). A lube base oil composition is also produced therefrom.