C10G73/16

Method and apparatus for purifying a mixture comprising oil and wax
10138433 · 2018-11-27 · ·

The present invention relates to a method for fractionating a crude mixture comprising at least one oil and at least one wax, which comprises the following steps: (a) mixing the crude mixture with a solvent to obtain a crude solvent-mixture, (b) carrying out at least one crystallization stage with the solvent-mixture obtained in step (a) to prepare a first fraction containing dewaxed oil and a second fraction containing slack wax, (c) carrying out at least one crystallization stage with the second fraction obtained in step (b) in a layer crystallizer, wherein to the second fraction prior to the crystallization in step (c) no solvent or at most 100% by weight of solvent relative to the weight of the second fraction are added, to prepare a third fraction containing hard wax having an oil content of at most 1.5% by weight and a fourth fraction containing soft wax having an oil content of more than 1.5% by weight and (d) circulating at least a part of the fourth fraction into at least one of the at least one crystallization stage of step (b).

Method and apparatus for purifying a mixture comprising oil and wax
10138433 · 2018-11-27 · ·

The present invention relates to a method for fractionating a crude mixture comprising at least one oil and at least one wax, which comprises the following steps: (a) mixing the crude mixture with a solvent to obtain a crude solvent-mixture, (b) carrying out at least one crystallization stage with the solvent-mixture obtained in step (a) to prepare a first fraction containing dewaxed oil and a second fraction containing slack wax, (c) carrying out at least one crystallization stage with the second fraction obtained in step (b) in a layer crystallizer, wherein to the second fraction prior to the crystallization in step (c) no solvent or at most 100% by weight of solvent relative to the weight of the second fraction are added, to prepare a third fraction containing hard wax having an oil content of at most 1.5% by weight and a fourth fraction containing soft wax having an oil content of more than 1.5% by weight and (d) circulating at least a part of the fourth fraction into at least one of the at least one crystallization stage of step (b).

Method and Apparatus for Purifying a Mixture Comprising Oil and Wax
20180142169 · 2018-05-24 · ·

The present invention relates to a method for fractionating a crude mixture comprising at least one oil and at least one wax, which comprises the following steps: (a) mixing the crude mixture with a solvent to obtain a crude solvent-mixture, (b) carrying out at least one crystallization stage with the solvent-mixture obtained in step (a) to prepare a first fraction containing dewaxed oil and a second fraction containing slack wax, (c) carrying out at least one crystallization stage with the second fraction obtained in step (b) in a layer crystallizer, wherein to the second fraction prior to the crystallization in step (c) no solvent or at most 100% by weight of solvent relative to the weight of the second fraction are added, to prepare a third fraction containing hard wax having an oil content of at most 1.5% by weight and a fourth fraction containing soft wax having an oil content of more than 1.5% by weight and (d) circulating at least a part of the fourth fraction into at least one of the at least one crystallization stage of step (b).

Method and Apparatus for Purifying a Mixture Comprising Oil and Wax
20180142169 · 2018-05-24 · ·

The present invention relates to a method for fractionating a crude mixture comprising at least one oil and at least one wax, which comprises the following steps: (a) mixing the crude mixture with a solvent to obtain a crude solvent-mixture, (b) carrying out at least one crystallization stage with the solvent-mixture obtained in step (a) to prepare a first fraction containing dewaxed oil and a second fraction containing slack wax, (c) carrying out at least one crystallization stage with the second fraction obtained in step (b) in a layer crystallizer, wherein to the second fraction prior to the crystallization in step (c) no solvent or at most 100% by weight of solvent relative to the weight of the second fraction are added, to prepare a third fraction containing hard wax having an oil content of at most 1.5% by weight and a fourth fraction containing soft wax having an oil content of more than 1.5% by weight and (d) circulating at least a part of the fourth fraction into at least one of the at least one crystallization stage of step (b).

METHOD FOR PREPARING LOW-POUR POINT, HIGH-AROMATIC, AND ENVIRONMENTAL-FRIENDLY RUBBER OIL BY COMBINING EXTRACTION AND DEWAXING

A method for preparing an environmental-friendly rubber oil, including: conducting extraction in an extraction tower, where a primary extraction solvent is introduced into an upper section of the extraction tower, a raw oil is introduced into a middle-lower section of the extraction tower, and a secondary extraction solvent is introduced into a lower section of the extraction tower; subjecting a material at a bottom of the extraction tower to solvent recovery to obtain a secondary extract oil; mixing a substance flowing out from a top of the extraction tower, a solubilizer and a part of the primary extraction solvent, cooling to 15 C. to 10 C., and filtering to obtain a wax paste and a filtrate; subjecting the wax paste to heating evaporation and solvent recovery to obtain a wax; and subjecting the filtrate to heating evaporation and solvent recovery, obtaining the environmental-friendly rubber oil.

METHOD FOR PREPARING LOW-POUR POINT, HIGH-AROMATIC, AND ENVIRONMENTAL-FRIENDLY RUBBER OIL BY COMBINING EXTRACTION AND DEWAXING

A method for preparing an environmental-friendly rubber oil, including: conducting extraction in an extraction tower, where a primary extraction solvent is introduced into an upper section of the extraction tower, a raw oil is introduced into a middle-lower section of the extraction tower, and a secondary extraction solvent is introduced into a lower section of the extraction tower; subjecting a material at a bottom of the extraction tower to solvent recovery to obtain a secondary extract oil; mixing a substance flowing out from a top of the extraction tower, a solubilizer and a part of the primary extraction solvent, cooling to 15 C. to 10 C., and filtering to obtain a wax paste and a filtrate; subjecting the wax paste to heating evaporation and solvent recovery to obtain a wax; and subjecting the filtrate to heating evaporation and solvent recovery, obtaining the environmental-friendly rubber oil.