CHROME-FREE TANNING PROCESS OF ECOLOGICAL LEATHER
A chrome-free tanning process of an ecological leather is characterized by a TWS+sodium lignosulfonate+TWLZ ternary tanning process system. The sodium lignosulfonate added can not only have a fixation effect on a TWS tanning agent to make the TWS tanning not undergo detanning at a low pH, but also significantly improve the uniformity of distribution of a TWLZ tanning agent in a hide/skin and promote the formation of a stable cross-linked network structure by the TWLZ tanning agent in a collagen fiber, which effectively overcomes the defects of tanning performance of the existing tanning systems to obtain a leather with uniform and sufficient tanning, a high isoelectric point, a strong electropositivity, excellent absorption for post-tanning chemicals, and a prominent softness, and gives a leather a wide use range and a high quality.
CHROME-FREE TANNING PROCESS OF ECOLOGICAL LEATHER
A chrome-free tanning process of an ecological leather is characterized by a TWS+sodium lignosulfonate+TWLZ ternary tanning process system. The sodium lignosulfonate added can not only have a fixation effect on a TWS tanning agent to make the TWS tanning not undergo detanning at a low pH, but also significantly improve the uniformity of distribution of a TWLZ tanning agent in a hide/skin and promote the formation of a stable cross-linked network structure by the TWLZ tanning agent in a collagen fiber, which effectively overcomes the defects of tanning performance of the existing tanning systems to obtain a leather with uniform and sufficient tanning, a high isoelectric point, a strong electropositivity, excellent absorption for post-tanning chemicals, and a prominent softness, and gives a leather a wide use range and a high quality.
Chrome-free tanning process of ecological leather
A chrome-free tanning process of an ecological leather is characterized by a TWS+sodium lignosulfonate+TWLZ ternary tanning process system. The sodium lignosulfonate added can not only have a fixation effect on a TWS tanning agent to make the TWS tanning not undergo detanning at a low pH, but also significantly improve the uniformity of distribution of a TWLZ tanning agent in a hide/skin and promote the formation of a stable cross-linked network structure by the TWLZ tanning agent in a collagen fiber, which effectively overcomes the defects of tanning performance of the existing tanning systems to obtain a leather with uniform and sufficient tanning, a high isoelectric point, a strong electropositivity, excellent absorption for post-tanning chemicals, and a prominent softness, and gives a leather a wide use range and a high quality.
Chrome-free tanning process of ecological leather
A chrome-free tanning process of an ecological leather is characterized by a TWS+sodium lignosulfonate+TWLZ ternary tanning process system. The sodium lignosulfonate added can not only have a fixation effect on a TWS tanning agent to make the TWS tanning not undergo detanning at a low pH, but also significantly improve the uniformity of distribution of a TWLZ tanning agent in a hide/skin and promote the formation of a stable cross-linked network structure by the TWLZ tanning agent in a collagen fiber, which effectively overcomes the defects of tanning performance of the existing tanning systems to obtain a leather with uniform and sufficient tanning, a high isoelectric point, a strong electropositivity, excellent absorption for post-tanning chemicals, and a prominent softness, and gives a leather a wide use range and a high quality.
Chrome-free leather retanning
A method for forming chrome-free retanned leather including: (a) contacting wet white with from 1% to 8%, by solids weight, based on the wet weight of wet white, retanning agent selected from the group consisting of: i) an aqueous emulsion polymer including, as copolymerized units, from 2% to 35%, by weight, based on the weight of the emulsion polymer, ethylenically-unsaturated monomer bearing at least one epoxy group, the emulsion polymer having a weight average molecular weight of from 2,000 to 100,000; ii) a compound selected from the group comprising piperazine, piperazine hydrates, salts of piperazine, and combinations thereof; and iii) combinations of i) and ii); (b) heating the contacted wet white; and (c) drying the contacted, heated wet white is provided. The present application also relates to chrome-free retanned leather formed by the method of the invention.