METHOD OF LEACHING COPPER FROM COPPER SULFIDE ORE AND METHOD OF EVALUATING IODINE LOSS CONTENT OF COLUMN LEACHING TEST OF THE COPPER SULFIDE ORE

A method of leaching copper from a copper sulfide ore which includes adding a potential adjustment agent for lowering a potential of a leaching solution obtained after leaching copper from the copper sulfide ore by using iodide ion and iron (III) ion, the leaching solution being stored in a tank for storing the leaching solution.

EQUIPMENT AND METHOD FOR LEACHING COPPER, AND METHOD FOR PRODUCING ELECTROLYTIC COPPER USING SAID EQUIPMENT AND METHOD

Provided is a method for efficiently promoting a leaching reaction of copper. Equipment for leaching copper includes a reactor for leaching reaction and a controller for oxidation-reduction potential. The reactor is configured to be provided with a leaching solution containing iodine and iron. The reactor is configured to be capable of being tightly sealed during the leaching reaction. The controller for oxidation-reduction potential is configured so that, during the leaching reaction, the oxidation-reduction potential of the leaching solution can be maintained at 500 mV (based on Ag/AgCl reference) or higher.

EXTRACTING BASE METALS USING A WETTING AGENT AND A THIOCARBONYL FUNCTIONAL GROUP REAGENT

The present disclosure relates to the use of a wetting agent such as a non-ionic wetting agent and a reagent comprising a thiocarbonyl functional group, for example, in a method/process or use for extracting a base metal such as copper from a material comprising the base metal. Such methods/processes can comprise contacting the material under acidic conditions with the wetting agent and the reagent comprising the thiocarbonyl functional group; and optionally recovering the base metal.

Method of extracting metals from polymetallic sulphide ores or concentrates

A method of extracting metals from polymetallic sulphide ores or concentrates comprising at least Cu, Zn, Pb and Ag, comprising a first step of atmospheric leaching in sulphate medium in the presence of recycled silver for extracting Cu and Zn and a second step of atmospheric leaching in chloride medium for extracting Pb and Ag.

Method for disposal of waste printed circuit board thermal cracking slag and smelting soot

The invention discloses a method for cracking slag and smelting soot of the waste circuit board, belongs to the field of comprehensive recycling of valuable elements from typical soot of waste circuit boards, and particularly relates to a method for cracking slag and smelting soot of the waste circuit board for debromination and comprehensive recovery of copper and zinc. The method includes the following steps of: crushing and sorting, mixture roasting, reinforced leaching, replacement and silver precipitation, sulfuration and copper precipitation, and evaporation crystallization. Compared to traditional recycling technology, the purpose of treating two kinds of solid waste in a coupling mode through one recycling technology is achieved. Through mixed sulfuric acid roasting, the requirement of bromide synergistic removal of the waste circuit board cracking slag and smelting soot is met, and the purpose of selective conversion of copper and zinc is achieved.

PROCESSES FOR PRODUCING GRANULAR COPPER
20220402030 · 2022-12-22 ·

Processes for producing copper granules on a surface of a reducing metal. The process can include contacting the reducing metal with an aqueous solution comprising a copper(II) salt and a halide. The molar ratio of the halide to the copper(II) in the copper (II) salt can be at least about 3:1. The granular copper can be produced on a surface of the reducing metal, and is optionally removed from the surface of the reducing metal by shaking, washing, and/or brushing, and/or optionally with stirring and/or circulating of the aqeuous solution.

System and method for adjusting leaching operations based on leach analytic data

The method may comprise receiving historical data (e.g., mineralogy data, irrigation data, raffinate data, heat data, lift height data, geographic data on ore placement and/or blower data); training a predictive model using the historical data to create a trained predictive model; adding future assumption data to the trained predictive model; running the forecast engine for a plurality of parameters to obtain forecast data for a mining production target; comparing the forecast data for the mining production target to the actual data for the mining production target; determining deviations between the forecast data and the actual data, based on the comparing; and changing each of the plurality of parameters from the forecast data to the actual data to determine a contribution to the deviations for each of the plurality of parameters.

Integrated pressure oxidative leach of copper sulphidic feed with copper heap leach

An integrated pressure leaching, heap leaching process for recovering copper from sulphidic feed containing iron, arsenic, and copper. Aqueous feed slurry of the sulphidic feed is pressure oxidized to form a liquid phase containing free sulphuric acid and aqueous copper sulphate, and to precipitate arsenic as solid iron arsenic compounds. Treated slurry is withdrawn from the pressure vessel and the liquid phase is separated from the solids. Copper is recovered from the separated liquid phase and generates a solution enriched in acid and depleted in copper. At least a portion of this solution is neutralized in a copper heap leach to produce a PLS containing copper and reduced in acid. At least a portion of the heap leach PLS is neutralized to produce a solution further reduced in acid, and solids containing copper precipitates, followed by a liquid solid separation.

Process for leaching a mineral particulate material

A process for leaching a mineral particulate material comprising the steps of feeding the mineral particulate material to a leaching step (10) in which at least one valuable metal in the mineral particulate material is leached into a leach solution to form a pregnant leach liquor and a solid residue containing undissolved mineral matter, the leaching step being conducted under conditions such that elemental sulphur is formed in the leaching step, wherein beads or particles that take up elemental sulphur are added to the leaching step such that elemental sulphur is taken up by or collects on the beads or particles, and separating the beads or particles from the pregnant leach liquor and the solid residue. The beads or particles may be treated to remove sulphur and the beads or particles are returned to the leaching step. Alternatively the mineral doesn't need to comprise a soluble component and can be a refractory sulphide of iron and/or arsenic containing precious metals that require oxidation before downstream conventional processes such as cyanidation.

Method For Cooperative Disposal Of Waste Printed Circuit Board Thermal Cracking Slag And Smelting Ash
20230037130 · 2023-02-02 ·

The invention discloses a method for co-processing cracking slag and smelting soot of the waste circuit board, belongs to the field of comprehensive recycling of valuable elements from typical soot of waste circuit boards, and particularly relates to a method for co-processing cracking slag and smelting soot of the waste circuit board for debromination and comprehensive recovery of copper and zinc. The method mainly comprises the following steps of: crushing and sorting, mixture roasting, reinforced leaching, replacement and silver precipitation, sulfuration and copper precipitation, and evaporation crystallization. Compared with a traditional recycling technology, the purpose that two kinds of solid waste are treated in a coupling mode through one recycling technology is achieved. Through mixed sulfuric acid roasting, the requirement of bromide synergistic removal of the waste circuit board cracking slag and smelting soot is met, and the purpose of selective conversion of copper and zinc is achieved.