C22C33/0264

ALLOYED STEEL POWDER FOR POWDER METALLURGY, IRON-BASED MIXED POWDER FOR POWDER METALLURGY, AND SINTERED BODY

Provided is an alloyed steel powder for powder metallurgy that has excellent compressibility and enables obtaining a sintered body having improved strength as sintered. An alloyed steel powder for powder metallurgy comprises: Cu: 2.0 mass % or more and 8.0 mass % or less; Mo: more than 0.50 mass % and 2.00 mass % or less; one or both of Mn: 0.1 mass % or more and 1.0 mass % or less and Cr: 0.3 mass % or more and 3.5 mass % or less; and a balance consisting of Fe and inevitable impurities, wherein the alloyed steel powder contains particulate oxide, and a total amount of Mn and Cr in the particulate oxide is 0.15 mass % or less with respect to 100 mass % of the alloyed steel powder, and a number ratio of particulate oxide in contact with Cu of FCC structure to the particulate oxide is 50% or more.

Method for producing a sintered component

The invention relates to a method for producing a sintered component comprising the steps: providing a metallic powder; filling the powder into a powder press; pressing the powder to form a green compact; removing the green compact from the powder press; sintering the green compact into a sintered component with pores; optional redensification of the sintered component; hardening of the sintered component, wherein the pores of the sintered component, prior to hardening at least in that region of the surface of the sintered component which is subjected to a hardening, are at least partially filled with a filling agent.

Yttrium-added rare-earth permanent magnetic material and preparation method thereof

The present disclosure discloses an yttrium (Y)-added rare-earth permanent magnetic material and a preparation method thereof. A chemical formula of the material expressed in atomic percentage is (YxRE1-x)aFebalMbNc, wherein 0.05≤x≤0.4, 7≤a≤13, 0≤b≤3, 5≤c≤20, and the balance is Fe, namely, bal=100-a-b-c; RE represents a rare-earth element Sm, or a combination of the rare-earth element Sm and any one or more elements of Zr, Nd and Pr; M represents Co and/or Nb; and N represents nitrogen. In the preparation method, the rare-earth element Y is utilized to replace the element Sm of a samarium-iron-nitrogen material. By regulating a ratio of the element Sm to the element Y, viscosity of an alloy liquid can be reduced, and an amorphous forming ability of the material is enhanced.

Yttrium-added rare-earth permanent magnetic material and preparation method thereof

The present disclosure discloses an yttrium (Y)-added rare-earth permanent magnetic material and a preparation method thereof. A chemical formula of the material expressed in atomic percentage is (YxRE1-x)aFebalMbNc, wherein 0.05≤x≤0.4, 7≤a≤13, 0≤b≤3, 5≤c≤20, and the balance is Fe, namely, bal=100-a-b-c; RE represents a rare-earth element Sm, or a combination of the rare-earth element Sm and any one or more elements of Zr, Nd and Pr; M represents Co and/or Nb; and N represents nitrogen. In the preparation method, the rare-earth element Y is utilized to replace the element Sm of a samarium-iron-nitrogen material. By regulating a ratio of the element Sm to the element Y, viscosity of an alloy liquid can be reduced, and an amorphous forming ability of the material is enhanced.

TOOL MAIN BODY AND METHOD FOR PRODUCING TOOL MAIN BODY

A tool main body to which an insert is attachable, in which the tool main body is made of sintered metal material, and the sintered metal material includes a parent phase made of a metal and a plurality of pores present in the parent phase.

Alloy powder, fe-based nanocrystalline alloy powder and magnetic core

An alloy powder having an alloy composition represented by Fe.sub.100-a-b-c-d-e-fCu.sub.aSi.sub.bB.sub.cCr.sub.dSn.sub.eC.sub.f, wherein a, b, c, d, e and f are atomic % meeting 0.80≤a≤1.80, 2.00≤b≤10.00, 11.00≤c≤17.00, 0.10≤d≤2.00, 0.01≤e≤1.50, and 0.10≤f≤0.40.

LIGHTWEIGHT HIGH LOAD-BEARING REDUCER AND METHOD FOR GENERATING BIONIC BONE STRUCTURE OF GEAR THEREOF

The present disclosure provides a reducer gear for robot, and a method for generating the gear and a reducer therewith. The reducer gear comprises: an outer contour layer and a reticulated porous base layer cladded by the outer contour layer; the outer contour layer comprises a mounting surface layer, a tooth surface layer, and a connecting surface layer connected between the mounting surface layer and the tooth surface layer and forming a complete gear outer contour together with the mounting surface layer and the tooth surface layer; the mounting surface layer, the tooth surface layer and the connecting surface layer are compact structures; the reticular porous base layer is located in a cavity formed by the outer contour layer, and fiber trabeculae in a porous grid structure are provided in the reticular porous base layer.

METHOD OF FORMING ARTICLE, COATED POWDER AND ARTICLE
20230131097 · 2023-04-27 · ·

A method of forming an article includes producing a base powder including a plurality of base particles. Each base particle includes an external surface and a first material. The method further includes removing one or more oxides from the external surface of each base particle to form a cleaned powder including a plurality of cleaned particles. Each cleaned particle includes a cleaned external surface made of the first material. The method further includes coating the cleaned external surface of each cleaned particle with a second material having a greater oxidation resistance than the first material to form a coated powder including a plurality of coated particles. Each coated particle includes an external layer including the second material that fully covers the cleaned external surface made of the first material. The method further includes forming the article using the coated powder.

ALLOY COMPOSITIONS
20230125609 · 2023-04-27 ·

The present disclosure provides compositions comprising iron, about 0.01 to about 0.4% w/w of manganese; about 1.3 to about 1.9% w/w of chromium; about 0.10% w/w or less of nickel; about 1.2 to about 1.7% w/w of molybdenum; about 0.01 to about 0.4% w/w of niobium; about 0.01 to about 0.4% w/w of vanadium; about 1.5 to about 2% w/w of silicon; and about 0.01 to about 0.20% w/w of carbon. The present disclosure also provides methods of preparing a metal powder, comprising atomizing a composition described herein and methods of preparing a metal object, comprising subjecting metal powder described herein to metal binder jetting.

Iron-Based Mixed Powder and Method for Manufacturing the Same
20230128986 · 2023-04-27 ·

The present disclosure relates to an iron-based mixed powder having excellent uniformity, fluidity and moldability by applying polyamide as a binder, and a method for manufacturing the same. The iron-based mixed powder according to an embodiment of the present disclosure is composed of a mixture of a raw material of mixed powder in which iron-based powder and additive powder are mixed, and polyamide as a binder, wherein 0.03 to 1.50 parts by weight of the binder is mixed based on 100 parts by weight of the raw material of the mixed powder.