Method for producing bleached wood fibre material
In a process for producing bleached mechanical woodpulp, said process comprising the steps of a) delaminating comparatively large particles of wood, which have optionally been pretreated with chemicals and/or water, into modified particles of wood, b) grinding the modified particles of wood from a) in one or more refiners, c) optionally treating the stalk obtained in step b) with oxidative or reductive bleaching agents, a composition Z is present during step a) and/or step b), said composition Z comprising one or more of the following components (Z1) to (Z3): a salt of dithionous acid H.sub.2S.sub.2O.sub.4 (Z1), a dithionous acid or dithionous acid derivative generator compound (Z2), a salt of sulfurous acid (sulfite) plus sodium tetraborohydride (Z3) and also optionally additives (Z4).
METHOD FOR PRODUCING BLEACHED WOOD FIBRE MATERIAL
In a process for producing bleached mechanical woodpulp, said process comprising the steps of
a) delaminating comparatively large particles of wood, which have optionally been pretreated with chemicals and/or water, into modified particles of wood,
b) grinding the modified particles of wood from a) in one or more refiners,
c) optionally treating the stalk obtained in step b) with oxidative or reductive bleaching agents, a composition Z is present during step a) and/or step b), said composition Z comprising one or more of the following components (Z1) to (Z3): a salt of dithionous acid H.sub.2S.sub.2O.sub.4(Z1), a dithionous acid or dithionous acid derivative generator compound (Z2), a salt of sulfurous acid (sulfite) plus sodium tetraborohydride (Z3) and also optionally additives (Z4).
Method for producing bleached wood fibre material
In a process for producing bleached mechanical woodpulp, said process comprising the steps of a) delaminating comparatively large particles of wood, which have optionally been pretreated with chemicals and/or water, into modified particles of wood, b) grinding the modified particles of wood from a) in one or more refiners, c) optionally treating the stalk obtained in step b) with oxidative or reductive bleaching agents, a composition Z is present during step a) and/or step b), said composition Z comprising one or more of the following components (Z1) to (Z3): a salt of dithionous acid H.sub.2S.sub.2O.sub.4 (Z1), a dithionous acid or dithionous acid derivative generator compound (Z2), a salt of sulfurous acid (sulfite) plus sodium tetraborohydride (Z3) and also optionally additives (Z4).
Stabilization of sodium dithionite by means of various additives
The present invention relates to a method for reducing or preventing the decomposition of a composition Z comprising Z1 a salt of dithionous acid in an amount ranging from 50 to 100 wt % and optionally Z2 an additive selected from the group consisting of alkali metal carbonate, alkaline earth metal carbonate, alkali metal or alkaline earth metal tripolyphosphate (Na.sub.5P.sub.3O.sub.10), alkali metal or alkaline earth metal sulfite, disulfite or sulfate, dextrose and complexing agents in a combined amount ranging from 0.0001 to 40 wt %, which comprises contacting the components Z1 and optionally Z2 in the solid and/or dry or solvent-dissolved or -suspended state with at least one of the following compounds V in the solid and/or dry or solvent-dissolved or -suspended state, wherein the compounds V are selected from the group consisting of: (a) oxides of the alkali metals lithium, sodium, potassium, rubidium, cesium, or of magnesium, (b) sodium tetrahydroborate (NaBH.sub.4), (c) anhydrous copper(II) sulfate (Cu(SO.sub.4)), phosphorus pentoxide and (d) basic amino acids arginine, lysine, histidine, wherein the solvent for Z1, optionally Z2 and V is practically water-free.
METHOD FOR PRODUCING BLEACHED WOOD FIBRE MATERIAL
In a process for producing bleached mechanical woodpulp, said process comprising the steps of a) delaminating comparatively large particles of wood, which have optionally been pretreated with chemicals and/or water, into modified particles of wood, b) grinding the modified particles of wood from a) in one or more refiners, c) optionally treating the stalk obtained in step b) with oxidative or reductive bleaching agents, a composition Z is present during step a) and/or step b), said composition Z comprising one or more of the following components (Z1) to (Z3): a salt of dithionous acid H.sub.2S.sub.2O.sub.4 (Z1), a dithionous acid or dithionous acid derivative generator compound (Z2), a salt of sulfurous acid (sulfite) plus sodium tetraborohydride (Z3) and also optionally additives (Z4).
STABILIZATION OF SODIUM DITHIONITE BY MEANS OF VARIOUS ADDITIVES
The present invention relates to a method for reducing or preventing the decomposition of a composition Z comprising Z1 a salt of dithionous acid in an amount ranging from 50 to 100 wt % and optionally Z2 an additive selected from the group consisting of alkali metal carbonate, alkaline earth metal carbonate, alkali metal or alkaline earth metal tripolyphosphate (Na.sub.5P.sub.3O.sub.10), alkali metal or alkaline earth metal sulfite, disulfite or sulfate, dextrose and complexing agents in a combined amount ranging from 0.0001 to 40 wt %, which comprises contacting the components Z1 and optionally Z2 in the solid and/or dry or solvent-dissolved or -suspended state with at least one of the following compounds V in the solid and/or dry or solvent-dissolved or -suspended state, wherein the compounds V are selected from the group consisting of: (a) oxides of the alkali metals lithium, sodium, potassium, rubidium, cesium, or of magnesium, (b) sodium tetrahydroborate (NaBH.sub.4), (c) anhydrous copper(II) sulfate (Cu(SO.sub.4)), phosphorus pentoxide and (d) basic amino acids arginine, lysine, histidine, wherein the solvent for Z1, optionally Z2 and V is practically water-free.