D21H23/50

A PACKAGING MATERIAL FOR PACKAGING OF LIQUID AND FOOD
20230212825 · 2023-07-06 · ·

The invention discloses a paperboard for packaging of a heat-sealable packaging material comprising: —a paperboard substrate comprising a first and a second side, —a first and an optional second dispersion coating layer on the first side, which first and optional second dispersion coating layer provides a barrier against at least one of liquid, moisture, grease and gas, —an extrusion coated barrier layer comprising a polyolefin, wherein the first and optional second dispersion coating layer is applied between the paperboard substrate and the extrusion coated barrier layer, and wherein the coat weight of the extrusion coated barrier layer is less than 15 gsm. The packaging material according of the invention minimizes the amount of plastic coating, but still provides the needed barrier properties for the packaging of food and/or liquid. The packaging material has especially been shown to provide a longer shelf life for food items packed in a packaging made from the material. Especially, the packaging material provides gas-, liquid and/or grease barrier properties. Although the packaging material comprises such low amount of extruded thermoplastic polymers, the material is readily heat-sealable.

A PACKAGING MATERIAL FOR PACKAGING OF LIQUID AND FOOD
20230212825 · 2023-07-06 · ·

The invention discloses a paperboard for packaging of a heat-sealable packaging material comprising: —a paperboard substrate comprising a first and a second side, —a first and an optional second dispersion coating layer on the first side, which first and optional second dispersion coating layer provides a barrier against at least one of liquid, moisture, grease and gas, —an extrusion coated barrier layer comprising a polyolefin, wherein the first and optional second dispersion coating layer is applied between the paperboard substrate and the extrusion coated barrier layer, and wherein the coat weight of the extrusion coated barrier layer is less than 15 gsm. The packaging material according of the invention minimizes the amount of plastic coating, but still provides the needed barrier properties for the packaging of food and/or liquid. The packaging material has especially been shown to provide a longer shelf life for food items packed in a packaging made from the material. Especially, the packaging material provides gas-, liquid and/or grease barrier properties. Although the packaging material comprises such low amount of extruded thermoplastic polymers, the material is readily heat-sealable.

Method of manufacturing of a foam-formed cellulosic fibre-material, a bulk sheet and a laminated packaging material comprising the cellulosic fibre-material

The invention relates to a method for manufacturing a foam-formed cellulosic fibre-material comprising coarse cellulosic fibres a cellulose reinforcement fraction. Furthermore, the invention relates to a foam-formed cellulosic fibre-material, a cellulose bulk sheet for a packaging material and a laminated packaging material comprising the foam-formed cellulosic fibre-material.

Method of manufacturing of a foam-formed cellulosic fibre-material, a bulk sheet and a laminated packaging material comprising the cellulosic fibre-material

The invention relates to a method for manufacturing a foam-formed cellulosic fibre-material comprising coarse cellulosic fibres a cellulose reinforcement fraction. Furthermore, the invention relates to a foam-formed cellulosic fibre-material, a cellulose bulk sheet for a packaging material and a laminated packaging material comprising the foam-formed cellulosic fibre-material.

FIBER BODY MANUFACTURING METHOD
20220412012 · 2022-12-29 ·

There is provided a fiber body manufacturing method including an accumulating step of forming the web by accumulating a material containing fibers and starch or dextrin on the first transport belt by a dry method; a transport step of transporting the web by peeling off a first surface of the web from the first transport belt, and by bringing a second surface of the web, which is a surface opposite to the first surface peeled off from the first transport belt, into contact with the second transport belt; a water-applying step of applying the water to the web which is in contact with the first transport belt or the second transport belt; and a heating step of heating the web by bringing the heating section into contact with the web peeled off from the second transport belt, and forming a fiber body by binding the fibers with the starch or dextrin, in which the web peeled off from the second transport belt is directly supplied to the heating section.

FIBER BODY MANUFACTURING METHOD
20220412012 · 2022-12-29 ·

There is provided a fiber body manufacturing method including an accumulating step of forming the web by accumulating a material containing fibers and starch or dextrin on the first transport belt by a dry method; a transport step of transporting the web by peeling off a first surface of the web from the first transport belt, and by bringing a second surface of the web, which is a surface opposite to the first surface peeled off from the first transport belt, into contact with the second transport belt; a water-applying step of applying the water to the web which is in contact with the first transport belt or the second transport belt; and a heating step of heating the web by bringing the heating section into contact with the web peeled off from the second transport belt, and forming a fiber body by binding the fibers with the starch or dextrin, in which the web peeled off from the second transport belt is directly supplied to the heating section.

Bio-based polyelectrolyte complex compositions comprising non-water soluble particles
11525211 · 2022-12-13 · ·

The present invention relates to a bio-based polyelectrolyte complex (PEC) composition suitable as a binder for fiber based materials, textiles, woven and nonwoven materials, said PEC composition comprising cationic biopolymer, anionic biopolymer, acid and preservative, and wherein the net charge of the PEC is cationic, the charge ratio of the anionic polymer and the cationic polymer is ≤1, the cationic biopolymer is chitosan, the anionic biopolymer is a polyanion derived from nature, the acid is a Brønsted acid and/or a Lewis acid, wherein the Brønsted acid is selected from any organic and/or inorganic acids, and wherein the Lewis acid is selected from any cationic mono- or multivalent atom, the weight ratio between cation and anion is 1:0.1 to 1:20, the weight ratio between the cation and acid is 1:0.01 to 1:30, chitosan has a degree of deacetylation being 66-100%, the pH is less than 7, and wherein said composition further comprises one or more non-water soluble particles. The present invention further relates to a method for preparing the PEC composition, uses of the PEC composition, as well as method of treating materials with the PEC composition.

COATED PAPERBOARD CONTAINERS AND METHODS
20220355979 · 2022-11-10 ·

A coated paperboard container includes a precursor paperboard substrate that includes a paperboard substrate and a barrier coating on the paperboard substrate. The coated paperboard container also includes an aqueous barrier coating on at least a portion of the barrier coating after the precursor paperboard container is formed with the barrier coating.

Fiber body forming method and sheet
11492759 · 2022-11-08 · ·

A fiber body forming method includes a step of defibrating a raw material containing fibers to form a defibrated material; a step of depositing the defibrated material to form a web; a step of applying a liquid containing a thermoplastic resin which binds the fibers to the web; and a step of heating the web to which the liquid is applied to form a fiber body, and in the method described above, the fiber body has a storage elastic modulus of 600 MPa or more at 100° C. and a storage elastic modulus of 400 MPa or more at 150° C.

Fiber body forming method and sheet
11492759 · 2022-11-08 · ·

A fiber body forming method includes a step of defibrating a raw material containing fibers to form a defibrated material; a step of depositing the defibrated material to form a web; a step of applying a liquid containing a thermoplastic resin which binds the fibers to the web; and a step of heating the web to which the liquid is applied to form a fiber body, and in the method described above, the fiber body has a storage elastic modulus of 600 MPa or more at 100° C. and a storage elastic modulus of 400 MPa or more at 150° C.