F05D2300/134

System and method for manufacture of abrasive coating

A component for a gas turbine engine includes an airfoil section including a free end and an abrasive coating sprayed onto the free end, the abrasive coating including a polymer matrix and an abrasive filler, the abrasive filler between about 50%-75% by volume of the abrasive coating.

Reduced radial clearance seal system

A seal system for a gas turbine engine includes a seal runner manufactured of a Molybdenum alloy material that provides a first coefficient of thermal expansion and a seal ring manufactured of a graphitic material that provides a second coefficient of thermal expansion greater than the first coefficient of thermal expansion.

VANE ARC SEGMENT WITH THERMAL INSULATION ELEMENT
20230106689 · 2023-04-06 ·

Disclosed is a method of reducing play in a vane arc segment. The vane arc segment includes an airfoil piece that defines first and second platforms and a hollow airfoil section that has an internal cavity and that extends between the first and second platforms. The first platform defines a gaspath side, a non-gaspath side, and a radial flange that projects from the non-gaspath side. Support hardware supports the airfoil piece via the radial flange, and a thermal insulation element is located adjacent the radial flange. The method includes performing a light scan of the radial flange to produce a digital three-dimensional model of the radial flange, and then machining the thermal insulation element in accordance with the digital three-dimensional model to provide a low-tolerance fit between the radial flange and the thermal insulation element that limits play between the airfoil piece and the thermal insulation element.

Self-modulated cooling on turbine components

Systems and methods are disclosed herein for passively managing cooling air in a gas turbine engine. A cooling air supply line may supply cooling air to a component in the gas turbine engine. A metering coupon may have a negative coefficient of thermal expansion. The metering coupon may allow more airflow through the metering coupon and through the component in response to an increase in temperature.

CRACK HEALING ADDITIVE MANUFACTURING OF A SUPERALLOY COMPONENT
20220234101 · 2022-07-28 ·

A method of additively manufacturing is provided. The method may include successively depositing and fusing together layers of a superalloy powder mixture comprised of a base material powder and a eutectic powder, to build up an additive portion, which eutectic powder has a solidus temperature lower than the solidus temperature of the base material powder. The method may also include heat treating the additive portion at a temperature greater than 1200° C. to heal cracks and/or fill pores and to homogenize the alloy of which the additive portion is comprised. The additive portion alloy has a chemistry defined by the superalloy powder mixture. The base material powder may be formed of a nickel-base superalloy with an aluminum content by weight of at least 1.5%. The eutectic powder may be a nickel-base alloy including by weight about 6% to about 11% chromium, about 5% to about 9% titanium, and about 9% to about 13% zirconium, with balance nickel as its primary components.

Wear resistant turbine blade tip

A gas turbine engine includes: a turbine section including a casing extending circumferentially about a plurality of turbine blades and having at least one seal member coated with an abradable coating. At least one turbine blade has sides and a tip and at least one seal member is located adjacent to the tip of the at least one turbine blade. The tip of the at least one turbine blade has a wear resistant layer and an abrasive coating disposed on the wear resistant layer. The wear resistant layer has a thickness less than or equal to 10 mils (254 micrometers) and includes metal boride compounds.

Wear resistant airfoil tip

A gas turbine engine includes an engine static structure extending circumferentially about an engine centerline axis; a compressor section, a combustor section, and a turbine section within the engine static structure. At least one of the compressor section and the turbine section includes at least one airfoil and at least one seal member adjacent to the at least one airfoil. A tip of the at least one airfoil is metal having a wear resistant coating and the at least one seal member is coated with an abradable coating. The wear resistant coating is formed as a layer in a base metal surface of the airfoil, has a thickness less than or equal to 10 mils (254 micrometers) and includes metal boride compounds.

VANE ARC SEGMENT WITH THERMAL INSULATION ELEMENT
20220162945 · 2022-05-26 ·

A vane arc segment includes an airfoil piece that defines first and second platforms and an airfoil section that extends between the first and second platforms. The first platform defines a gaspath side, a non-gaspath side, and a first platform radial flange that projects from the non-gaspath side. Support hardware supports the airfoil piece via the first platform radial flange. A thermal insulation element is situated adjacent the first platform radial flange. The support hardware supports the airfoil piece through the thermal insulation element.

System and Method for Manufacture of Abrasive Coating

A component for a gas turbine engine includes an airfoil section including a free end and an abrasive coating sprayed onto the free end, the abrasive coating including a polymer matrix and an abrasive filler, the abraisive filler between about 50%-75% by volume of the abrasive coating.

Control system and method

A control system includes one or more processors configured to determine when to extend a life span of an engine by applying an additional restorative coating to the engine based on one or more monitored parameters of the engine. The monitored parameters include a condition of a previously applied restorative coating. The one or more processors are configured to determine the condition of the previously applied restorative coating based on an optical response of the previously applied restorative coating. The one or more processors also are configured to direct application of the additional restorative coating based on the one or more monitored parameters of the engine.