RARE EARTH INTERLAYS FOR MECHANICALLY LAYERING DISSIMILAR SEMICONDUCTOR WAFERS
Structures described herein may include mechanically bonded interlayers for formation between a first Group III-V semiconductor layer and a second semiconductor layer. The mechanically bonded interlayers provide reduced lattice strain by strain balancing between the Group III-V semiconductor layer and the second semiconductor layer, which may be silicon.
Rare Earth Pnictides for Strain Management
Systems and methods described herein may include a first semiconductor layer with a first lattice constant, a rare earth pnictide buffer epitaxially grown over the first semiconductor, wherein a first region of the rare earth pnictide buffer adjacent to the first semiconductor has a net strain that is less than 1%, a second semiconductor layer epitaxially grown over the rare earth pnictide buffer, wherein a second region of the rare earth pnictide buffer adjacent to the second semiconductor has a net strain that is a desired strain, and wherein the rare earth pnictide buffer may comprise one or more rare earth elements and one or more Group V elements. In some examples, the desired strain is approximately zero.
Pnictide buffer structures and devices for GaN base applications
A structure can include a III-N layer with a first lattice constant, a first rare earth pnictide layer with a second lattice constant epitaxially grown over the III-N layer, a second rare earth pnictide layer with a third lattice constant epitaxially grown over the first rare earth pnictide layer, and a semiconductor layer with a fourth lattice constant epitaxially grown over the second rare earth pnictide layer. A first difference between the first lattice constant and the second lattice constant and a second difference between the third lattice constant and the fourth lattice constant are less than one percent.
Rare earth pnictides for strain management
Systems and methods described herein may include a first semiconductor layer with a first lattice constant, a rare earth pnictide buffer epitaxially grown over the first semiconductor, wherein a first region of the rare earth pnictide buffer adjacent to the first semiconductor has a net strain that is less than 1%, a second semiconductor layer epitaxially grown over the rare earth pnictide buffer, wherein a second region of the rare earth pnictide buffer adjacent to the second semiconductor has a net strain that is a desired strain, and wherein the rare earth pnictide buffer may comprise one or more rare earth elements and one or more Group V elements. In some examples, the desired strain is approximately zero.
Pnictide Buffer Structures and Devices for GaN Base Applications
A structure can include a III-N layer with a first lattice constant, a first rare earth pnictide layer with a second lattice constant epitaxially grown over the III-N layer, a second rare earth pnictide layer with a third lattice constant epitaxially grown over the first rare earth pnictide layer, and a semiconductor layer with a fourth lattice constant epitaxially grown over the second rare earth pnictide layer. A first difference between the first lattice constant and the second lattice constant and a second difference between the third lattice constant and the fourth lattice constant are less than one percent.